实验性开窗腔内修复中Advanta V12/iCast与Viabahn球扩覆膜支架的抗疲劳性能比较

Fatigue Resistance of the Advanta V12/iCast and Viabahn Balloon-Expandable Stent-Graft as Bridging Stents in Experimental Fenestrated Endografting.
PubMed 文献 · J Endovasc Ther · 2021-02-25

本研究在模拟开窗腔内修复的体外疲劳测试中,比较Viabahn球扩覆膜支架(VBX)与Advanta V12/iCast在5千万次循环后的抗疲劳性能。结果显示两组均无支架断裂,VBX全程无聚四氟乙烯(PTFE)全层缺陷,而Advanta组出现全层缺陷且PTFE破损失效循环数显著更低。

要点

  • 5千万次循环后VBX与Advanta均无支架断裂。
  • VBX全程无PTFE全层缺陷,Advanta出现全层缺陷。
  • Advanta组2/5例见镍钛环早期穿透导致PTFE缺陷。

核心结论

  • 在模拟呼吸运动的疲劳测试中,VBX与Advanta V12在抗断裂和免于PTFE初始改变方面表现相当。
  • VBX在全部5千万次循环中保持免于PTFE破损失效。
  • 全层缺陷仅见于Advanta组,主要由镍钛环穿透PTFE所致。

研究设计与样本

  • 体外实验研究,使用带10个开窗的聚酯测试片模拟开窗腔内移植物。
  • 植入5枚6×59 mm VBX和5枚6×58 mm Advanta支架至6×6 mm开窗。
  • 支架用10×20 mm PTA导管扩口后连接疲劳应力机,定期显微和射线评估至5千万次循环(模拟约75个月)。

主要发现

  • 数字射线图像显示两组在5千万次循环后均无支架断裂。
  • VBX在5千万次循环结束时无任何全层缺陷,免于PTFE破损失效(FBP)显著高于Advanta(50,000,000 vs 33,400,000;p<0.01)。
  • 全层缺陷仅见于Advanta组,5枚中2枚出现镍钛环早期穿透导致PTFE缺陷。
  • 免于PTFE初始改变(FIC)两组无显著差异(VBX 3,400,000 vs Advanta 3,200,000)。

关键数值与推荐

  • FBP:VBX 50,000,000次循环 vs Advanta 33,400,000次循环,p<0.01。
  • FIC:VBX 3,400,000次循环 vs Advanta 3,200,000次循环,无显著差异。
  • 全层缺陷仅见于Advanta组,5枚中2枚见镍钛环穿透PTFE。

临床怎么用

  • 在需要桥接支架的开窗腔内修复中,VBX可能提供更持久的PTFE抗破损性能。
  • Advanta V12需关注镍钛环穿透导致PTFE全层缺陷的风险。
  • 体外疲劳测试结果可为支架选择提供参考,但需结合体内环境综合判断。

局限性

  • 研究为体外实验,不能完全模拟体内生物力学环境。
  • 样本量较小(每组5枚支架)。
  • 模拟寿命约75个月,长期性能未验证。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

PURPOSE: Bridging stents undergo millions of cycles during respiratory movements of the kidneys throughout the patient's life. Thus, understanding the response of fabric and endoskeleton of the stent to cyclic loading over the time is crucial. In this study, we compare the fatigue resistance of the Viabahn Balloon-Expandable stent-graft (VBX) with the widely used Advanta V12/iCast under prolonged stress induction. MATERIALS AND METHODS: A polyester test sheet with 10 fenestrations was used simulating a fenestrated endograft. Five 6×59 mm VBX stent-grafts and five 6×58 mm Advanta stent-grafts were implanted into 6×6 mm fenestrations. The stents were flared with a 10×20 mm PTA (percutaneous transluminal angioplasty) catheter and connected with a fatigue stress machine. All stent-grafts were evaluated by microscopy and radiography at baseline and after regular intervals until 50,000,000 cycles were applied, simulating a life span of approximately 75 months. Freedom from fracture (FF), freedom from initial polytertafluoroethylene (PTFE) changes (FIC), and from PTFE breakpoint (FBP, all-layer defect) were calculated. RESULTS: Digital radiographic images did not show any stent fracture in both groups after 50,000,000 cycles. The VBX stent-graft was free from any all-layer defects at the conclusion of 50,000,00 cycles resulting in a significant higher FBP compared with Advanta V12 (50,000,000 vs 33,400,000; p<0.01). All-layer defects were observed only in the Advanta group. Two of 5 Advanta stents showed early penetration of the nitinol ring causing a defect of PTFE. Regarding FIC, there was no significant difference between the stents (3,400,000 in VBX vs 3,200,000 in Advanta). CONCLUSIONS: In fatigue tests simulating respiration movements, VBX and Advanta V12 performed equally well in terms of fracture resistance and freedom from initial PTFE changes. VBX maintained freedom from PTFE breakpoint throughout the full 50,000,000 cycles. All-layers defects were detected only in Advanta and were mainly caused by penetration of the nitinol ring through the PTFE.

来源:J Endovasc Ther,查看原文。版权归原作者所有。