文献速递烧伤创面修复

猪烧伤模型中银基抗菌敷料疗效比较

Comparison of the efficacy of silver-based antimicrobial burn dressings in a porcine model of burn wounds.
PubMed 文献 · Burns · 2020-04-27

该研究在猪烧伤模型中比较了四种敷料对金黄色葡萄球菌和铜绿假单胞菌的抗菌效果。结果显示纳米晶银敷料使细菌log10减少4-5(P=0.02),优于镀银尼龙和高氧化银盐敷料;所有敷料第3天抗菌效果较第1天下降。

要点

  • 纳米晶银敷料抗菌效果最佳,log10减少4-5且具统计学显著性(P=0.02)
  • 所有银基敷料均减少烧伤组织细菌回收,但仅纳米晶银达显著差异
  • 所有敷料第3天抗菌效果较第1天下降,感染创面或需更频繁更换

核心结论

  • 纳米晶银敷料在猪烧伤模型中抗菌表现总体优于镀银尼龙和高氧化银盐敷料。
  • 治疗感染创面时或应比预防性使用更频繁地更换敷料。

研究设计与样本

  • 采用家养约克夏杂交猪构建烧伤模型,用加热黄铜棒造成深达真皮深层的烧伤。
  • 创面人工接种金黄色葡萄球菌和铜绿假单胞菌混合菌液,缝合固定四种敷料。
  • 在第1天和第3天评估红斑、肿胀和再上皮化,活检组织定量细菌回收并做组织学检查。
  • 同时检测敷料自身保留的微生物数量。

主要发现

  • 组织学显示30秒即可造成深达真皮深层的烧伤。
  • 第3天纳米晶银和镀银尼龙较单纯纱布轻度减轻肿胀,但所有敷料对红斑和再上皮化无显著影响。
  • 所有敷料均减少烧伤组织细菌回收,纳米晶银减少幅度最大(log10减少4-5),且仅其达统计学显著(P=0.02)。
  • 所有敷料第3天抗菌效果较第1天下降,敷料自身微生物保留呈相似趋势。

关键数值与推荐

  • 纳米晶银敷料细菌log10减少4-5,P=0.02。
  • 烧伤模型加热黄铜棒接触30秒可造成深真皮烧伤。

临床怎么用

  • 预防性使用银基敷料时可选纳米晶银以获得更强抗菌效果。
  • 治疗已感染创面时考虑增加敷料更换频率以应对抗菌效果随时间下降。

局限性

  • 研究为猪烧伤模型,结果外推至临床需谨慎。
  • 仅评估至第3天,未观察更长期效果。
  • 仅测试两种病原体混合接种,未涵盖其他常见烧伤感染病原体。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

PURPOSE: A variety of silver-based antimicrobial dressings are available on the market and are commonly used to prevent infection. Such prophylaxis is particularly important in treating burns, yet there is a paucity of evidence confirming the efficacy of commercially available dressingsin vivo. We describe here an in vivo porcine model of burns, which we use to test the antimicrobial efficacy of three common wound dressings and a control. PROCEDURES: Domestic Yorkshire-cross pigs were medicated for pain management before inflicting burns with a heated brass rod. The wounds were artificially challenged with a mixture of two pathogens commonly associated with burn wound infection:Staphylococcus aureus and Pseudomonas aeruginosa. The following dressing materials were sutured in place: gauze, nanocrystalline silver, silver-plated nylon, and polyethylene/polyester coated with high-oxidation silver salts. After 1 and 3 days, the wounds were assessed for erythema, swelling, and re-epithelialization, tissue was biopsied to determine the recovery of the challenge microorganisms, and histology was performed. We also examined the number of microorganisms present on the dressings themselves. RESULTS: Histology indicated that 30 s was sufficient to produce burns extending into the deep dermal layer. After 3 days, nanocrystalline silver and silver-plated nylon led to slightly reduced swelling relative to simple gauze, although none of the dressings significantly affected erythema or wound re-epithelialization. All the dressings led to decreased recovery of the challenge organisms from the burn tissue, relative to simple gauze. However, the magnitude of the reduction was greatest for nanocrystalline silver (log10 reduction = 4-5); additionally, only nanocrystalline silver gave a statistically significant decrease (P = 0.02). Notably, the antimicrobial effect for all dressings was reduced by Day 3 relative to Day 1. Similar trends were observed for microbial retention on the dressings themselves. CONCLUSION: Nanocrystalline silver-based wound dressings generally outperformed silver-plated nylon and high-oxidation silver salts in thisin vivo model of burn wounds. Relative to prophylactic use, it may be advisable to change the dressings more frequently when treating an infected wound.

来源:Burns,查看原文。版权归原作者所有。

引用

  1. Ross JA, Allan N, Olson M, et al. Comparison of the efficacy of silver-based antimicrobial burn dressings in a porcine model of burn wounds. Burns. 2020. PMID: 32381448. doi:10.1016/j.burns.2020.04.004

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。