含银纳米颗粒的聚乳酸-姜黄素纳米纤维伤口敷料的制备与评估用于烧伤创面治疗

Preparation and assessment of polylactic acid-curcumin nanofibrous wound dressing containing silver nanoparticles for burn wound treatment.
PubMed 文献 · Burns · 2025-02-27

本研究通过静电纺丝法制备含聚乳酸、姜黄素和银纳米颗粒的纳米纤维伤口敷料,共五种配方。结果显示加入姜黄素提高拉伸强度,高含量银纳米颗粒降低拉伸强度;PLA+Cur+3%AgNPs敷料抗菌性达99.12%,PLA+Cur敷料为84.06%;细胞培养显示姜黄素和银纳米颗粒促进细胞生长、增殖和黏附。作者认为PLA+Cur+1%AgNPs纳米纤维支架作为多功能敷料在伤口愈合和烧伤治疗中具有可观前景。

要点

  • 五种静电纺丝敷料均成功制备,纤维直径达纳米级。
  • PLA+Cur+3%AgNPs敷料抗菌性99.12%,PLA+Cur敷料84.06%。
  • 加入姜黄素提高拉伸强度,高含量银纳米颗粒降低拉伸强度。

核心结论

  • PLA+Cur+1%AgNPs纳米纤维支架作为多功能敷料在伤口愈合和烧伤治疗中展现出可观前景。

研究设计与样本

  • 采用静电纺丝法制备五种敷料:PLA、PLA+Cur、PLA+Cur+1%AgNPs、PLA+Cur+2%AgNPs和PLA+Cur+3%AgNPs。

主要发现

  • 傅里叶变换红外光谱和扫描电镜观察表明所有静电纺丝样品均成功制备并达到纳米级直径。
  • 在40小时以上,静电纺丝样品的吸水率在0%至0.25%之间变化。
  • 一周内姜黄素释放试验显示PLA+Cur+2%AgNPs纳米纤维释放率最低,PLA+Cur+3%AgNPs释放率最高。
  • 拉伸强度随姜黄素加入聚乳酸而增加,高含量AgNPs导致拉伸强度下降。
  • PLA+Cur敷料抗菌性为84.06%,PLA+Cur+3%AgNPs敷料抗菌性为99.12%。

关键数值与推荐

  • PLA+Cur+3%AgNPs敷料抗菌性为99.12%,PLA+Cur敷料为84.06%。
  • 静电纺丝样品在40小时以上的吸水率在0%至0.25%之间。
  • 一周内姜黄素释放率PLA+Cur+2%AgNPs最低,PLA+Cur+3%AgNPs最高。

临床怎么用

  • 作者认为PLA+Cur+1%AgNPs纳米纤维支架作为多功能敷料在伤口愈合和烧伤治疗中具有可观前景。

局限性

  • 原文未报告局限性

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

This study aims to produce and evaluate nanofibrous wound dressings through the electrospinning method, utilizing polylactic acid (PLA), curcumin (Cur), and silver nanoparticles (AgNPs). For this purpose, five types of wound dressings with PLA, PLA+Cur, PLA+Cur+ 1 %AgNPs, PLA+Cur+ 2 %AgNPs and PLA+Cur+ 3 %AgNPs were produced using the electrospinning method. Analysis of the Fourier transform infrared spectroscopy and scanning electron microscopic observations indicated successful fabrication, with nanometer diameters achieved in all electrospun samples. Examination of water absorption of wound dressings revealed that over 40 h the electrospun samples had variable water absorption between 0 % and 0.25 %. The results of the curcumin release test over one week showed that the nanofibers with PLA+Cur+ 2 %AgNPs exhibited the lowest release rate, while those with PLA+Cur+ 3 %AgNPs showed the highest release. Assessment of mechanical properties revealed that the tensile strength of the nanofibers increased by adding curcumin to polylactic acid, while the addition of a high content of AgNPs led to a decrease in tensile strength. Also, the PLA+Cur dressing demonstrated 84.06 % and the PLA+Cur+ 3 %AgNPs dressing exhibited 99.12 % antibacterial properties. The cell culture test demonstrated that the incorporation of curcumin and AgNPs increasedboth the growth and proliferation, as well as the adhesion on the nanofibrous wound dressing. Thus, the PLA+Cur+ 1 %AgNPs nanofibrous scaffold, as a multipurpose dressing, presented considerable promise for wound healing and burn treatment.