钴铬股骨假体在模拟磨损中产生划痕并释放金属碎屑,而陶瓷假体未出现

Cobalt-chromium femoral components developed scratches and released metal debris in simulated wear whereas ceramic femoral components did not.
PubMed 文献 · Bone Joint J · 2021-01-01

本研究利用光学轮廓仪评估全膝关节置换术中钴铬股骨假体表面磨损,并与陶瓷股骨假体比较。结果显示钴铬假体表面粗糙度在最初1000次磨损周期内快速增加后达稳态,但材料以每百万周期1,778,000 μm³的速率持续丢失,碳化物脱落形成第三体磨损颗粒导致新划痕产生;陶瓷假体经15M磨损周期测试后未发现划痕、材料丢失或其他表面损伤。

要点

  • 钴铬股骨假体在模拟磨损中表面粗糙度快速增加并持续释放金属碎屑。
  • 钴铬假体材料丢失速率与磨损周期呈线性关系,碳化物脱落形成第三体磨损。
  • 陶瓷股骨假体在15M磨损周期测试后未出现划痕或材料丢失。

核心结论

  • 钴铬股骨假体在模拟磨损中因划痕和微磨粒磨损导致材料丢失,且丢失量与周期呈线性关系。
  • 陶瓷股骨假体在模拟磨损中未出现划痕和粗糙化,提示在磨损率和避免金属过敏方面具有优势。

研究设计与样本

  • 采用光学轮廓仪评估膝关节磨损模拟器中股骨假体表面粗糙度及磨损特征。
  • 开发方法测量五个钴铬股骨假体表面变化并量化关节面材料丢失。
  • 检查既往测试中三个陶瓷股骨假体的关节面,与钴铬假体比较表面损伤证据。

主要发现

  • 钴铬假体表面粗糙度在最初1000次磨损周期内快速增加,随后达到稳态。
  • 钴铬假体材料以每百万周期1,778,000 μm³的速率持续从表面丢失,碳化物从基质中脱落。
  • 脱落的碳化物形成第三体磨损颗粒,导致新划痕形成,即使旧划痕被磨掉。
  • 陶瓷假体在15M磨损周期测试后,以1纳米分辨率评估未发现划痕、材料丢失或其他表面损伤。

临床怎么用

  • 本研究结果提示陶瓷股骨假体在磨损率和避免金属过敏方面可能具有优势。
  • 上述发现可能对全膝关节置换术后持续疼痛的管理有启示意义。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

AIMS: The aims of this study were to evaluate wear on the surface of cobalt-chromium (CoCr) femoral components used in total knee arthroplasty (TKA) and compare the wear of these components with that of ceramic femoral components. METHODS: Optical profilometry was used to evaluate surface roughness and to examine the features created by the wear process in a knee wear simulator. We developed a method of measuring surface changes on five CoCr femoral components and quantifying the loss of material from the articular surface during the wear process. We also examined the articular surface of three ceramic femoral components from a previous test for evidence of surface damage, and compared it with that of CoCr components. RESULTS: We found that the surface roughness of CoCr components rapidly increased during the first 1,000 wear cycles, then reached a steady state, but material loss from the surface continued at a rate of 1,778,000 μm3 per million cycles as carbides were removed from its matrix. These carbides formed third-body wear particles, leading to the formation of new scratches even as older scratches were worn away. In contrast, no scratching, loss of material, or other surface damage, when evaluated with one nanometer resolution, was found on the surface of the ceramic components after a 15 M wear cycle test. CONCLUSION: This study showed wear and loss of CoCr material from scratching and microabrasive wear in TKA. The material loss from the surface continued in a linear relationship with increasing cycles. We also found the absence of scratching and roughening of ceramic femoral components in simulated wear, suggesting an advantage in wear rate and avoiding metal sensitivity. This may have implications in the management of persistent pain after TKA. Cite this article: Bone Joint J 2021;103-B(6 Supple A):94-101.

来源:Bone Joint J,查看原文。版权归原作者所有。

引用

  1. Roy ME, Whiteside LA, Ly KK, et al. Cobalt-chromium femoral components developed scratches and released metal debris in simulated wear whereas ceramic femoral components did not. Bone Joint J. 2021. PMID: 34053284. doi:10.1302/0301-620X.103B6.BJJ-2020-2429.R1

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。