碘涂层植入物碘流失后仍保持抗菌活性:大鼠模型与体外分析
本研究在大鼠体内评估碘涂层钛植入物碘含量随时间的变化,并在体外检测其残余抗菌活性。结果显示,4周和8周后碘含量分别降至72%和65%,但8周时对甲氧西林敏感金黄色葡萄球菌、耐甲氧西林金黄色葡萄球菌和铜绿假单胞菌的抗菌活性仍优于对照。
要点
- 碘涂层植入物在大鼠体内4周和8周后碘含量分别降至72%和65%。
- 8周时碘涂层植入物对三种测试细菌的抗菌活性仍优于Ti和Ti-O对照。
- 碘涂层植入物在8周内维持抗菌活性,但人体疗效尚待验证。
核心结论
- 碘涂层植入物在大鼠体内8周后仍保留碘含量,并对甲氧西林敏感金黄色葡萄球菌、耐甲氧西林金黄色葡萄球菌和铜绿假单胞菌保持抗菌活性。
研究设计与样本
- 研究分体内和体外两部分:体内实验用大鼠植入Ti、Ti-O和Ti-I垫圈,用ICP-MS测碘含量;体外实验用平板涂布法和荧光显微镜评估抗菌效果。
- 共使用24只大鼠和213个垫圈,其中体内实验2只大鼠15个垫圈,体外实验22只大鼠198个垫圈。
主要发现
- Ti-I植入大鼠4周和8周后碘含量分别降至72%(p=0.001)和65%(p<0.001)。
- 8周模型中,Ti-I对MSSA的菌落数中位数(IQR)为55(37-67)×10^5 CFU,低于Ti的112(104-165)×10^5(p=0.026)和Ti-O的147(111-162)×10^5(p=0.009)。
- 8周模型中,Ti-I对MRSA的菌落数中位数为26(9-31)×10^5 CFU,低于Ti的71(39-111)×10^5(p=0.026)和Ti-O的50(44-62)×10^5(p=0.034)。
- 8周模型中,Ti-I对铜绿假单胞菌的菌落数中位数为30(21-45)×10^6 CFU,低于Ti的77(74-83)×10^6(p=0.004)和Ti-O的111(95-117)×10^6(p=0.009)。
关键数值与推荐
- 体外实验中,Ti-I在4周和8周模型中对各菌种的活菌生物膜覆盖百分比中位数均低于Ti和Ti-O,死菌覆盖百分比无差异。
临床怎么用
- 碘涂层钛植入物在大鼠体内8周内具有抗菌活性,但大鼠模型结果不保证人体有效,需进一步临床研究。
局限性
- 研究为大鼠模型,非感染性关节植入模型,且荧光显微镜分析为非盲法。
- 需更大样本的感染动物模型(包括雌雄动物关节植入)评估更长期抗菌效力。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
BACKGROUND: We developed iodine-coated titanium implants to suppress microbial activity and prevent periprosthetic joint infection (PJI); their efficacy was demonstrated in animal and in vitro models. The iodine content in iodine-coated implants naturally decreases in vivo. However, to our knowledge, the effect of reduced iodine content on the implant's antimicrobial activity has not been evaluated to date. QUESTIONS/PURPOSES: (1) How much does the iodine content on the implant surface decrease after 4 and 8 weeks in vivo in a rat model? (2) What effect does the reduced iodine content have on the antimicrobial effect of the implant against multiple bacteria in an in vitro model? METHODS: This experiment was performed in two parts: an in vivo experiment to determine attenuation of iodine levels over time in rats, and an in vitro experiment in which we sought to assess whether the reduced iodine content observed in the in vivo experiment was still sufficient to deliver antimicrobial activity against common pathogens seen in PJI. For the in vivo experiment, three types of titanium alloy washers were implanted in rats: untreated (Ti), surface-anodized to produce an oxide film (Ti-O), and with an iodine layer on the oxidation film (Ti-I). The attenuation of iodine levels in rats was measured over time using inductively coupled plasma-mass spectrometry. Herein, only the Ti-I washer was used, with five implanted in each rat that were removed after 4 or 8 weeks. For the 4- and 8-week models, two rats and 15 washers were used. For the in vitro study, to determine the antibacterial effect, three types of washers (Ti, Ti-O, and Ti-I) (nine washers in total) were implanted in each rat. Then, the washers were removed and the antibacterial effect of each washer was examined on multiple bacterial species using the spread plate method and fluorescence microscopy. For the spread plate method, six rats were used, and five rats were used for the observation using fluorescence microscopy; further, 4- and 8-week models were made for each method. Thus, a total of 22 rats and 198 washers were used. Live and dead bacteria in the biofilm were stained, and the biofilm coverage percentage for quantitative analysis was determined using fluorescence microscopy in a nonblinded manner. Ti-I was used as the experimental group, and Ti and Ti-O were used as control groups. The total number of rats and washers used throughout this study was 24 and 213, respectively. RESULTS: Iodine content in rats implanted with Ti-I samples decreased to 72% and 65% after the in vivo period of 4 and 8 weeks, respectively (p = 0.001 and p < 0.001, respectively). In the in vitro experiment, the Ti-I implants demonstrated a stronger antimicrobial activity than Ti and Ti-O implants in the 4- and 8-week models. Both the median number of bacterial colonies and the median biofilm coverage percentage with live bacteria on Ti-I were lower than those on Ti or Ti-O implants for each bacterial species in the 4- and 8-week models. There was no difference in the median biofilm coverage percentage of dead bacteria. In the 8-week model, the antibacterial activity using the spread plate method had median (interquartile range) numbers of bacteria on the Ti, Ti-O, and Ti-I implants of 112 (104 to 165) × 105, 147 (111 to 162) × 105, and 55 (37 to 67) × 105 of methicillin-sensitive Staphylococcus aureus (Ti-I versus Ti, p = 0.026; Ti-I versus Ti-O, p = 0.009); 71 (39 to 111) × 105, 50 (44 to 62) × 105, and 26 (9 to 31)× 105 CFU of methicillin-resistant S. aureus (Ti-I versus Ti, p = 0.026; Ti-I versus Ti-O, p = 0.034); and 77 (74 to 83) × 106, 111 (95 to 117) × 106, and 30 (21 to 45) × 106 CFU of Pseudomonas aeruginosa (Ti-I versus Ti, p = 0.004; Ti-I versus Ti-O, p = 0.009). Despite the decrease in the iodine content of Ti-I after 8 weeks, it demonstrated better antibacterial activity against all tested bacteria than the Ti and Ti-O implants. CONCLUSION: Iodine-coated implants retained their iodine content and antibacterial activity against methicillin-sensitive S. aureus, methicillin-resistant S. aureus, and P. aeruginosa for 8 weeks in vivo in rats. To evaluate the longer-lasting antibacterial efficacy, further research using larger infected animal PJI models with implants in the joints of both males and females is desirable. CLINICAL RELEVANCE: Iodine-coated titanium implants displayed an antibacterial activity for 8 weeks in rats in vivo. Although the findings in a rat model do not guarantee efficacy in humans, they represent an important step toward clinical application.
引用
- Ueoka K, Kabata T, Tokoro M, et al. Antibacterial Activity in Iodine-coated Implants Under Conditions of Iodine Loss: Study in a Rat Model Plus In Vitro Analysis. Clin Orthop Relat Res. 2021. PMID: 33847603. doi:10.1097/CORR.0000000000001753