文献速递关节外科

初次与翻修双动全髋关节置换的微动腐蚀、第三体聚乙烯损伤与髋臼杯位置

Fretting Corrosion, Third-Body Polyethylene Damage, and Cup Positioning in Primary vs Revision Dual Mobility Total Hip Arthroplasty.
PubMed 文献 · J Arthroplasty · 2021-01-21

研究对56例取出的双动全髋关节置换假体进行分析,评估聚乙烯内衬损伤、微动腐蚀及髋臼杯位置。结果显示最常见翻修原因为感染、松动和不稳定/脱位,聚乙烯损伤以划痕、点蚀、抛光及嵌入碎屑为主,碎屑成分与多孔钛涂层一致,多数假体髋臼杯位置在Lewinnek安全区内。

要点

  • 翻修最常见原因为感染(36%)、松动(21%)和不稳定/脱位(18%)。
  • 聚乙烯损伤主要为划痕、点蚀、抛光及嵌入碎屑,初次与翻修病例总损伤无差异。
  • 碎屑形态与成分符合多孔钛涂层,来源于髋臼杯松动或螺钉/垫块断裂。

核心结论

  • 双动全髋关节置换中表面损伤最显著的机制为第三体碎屑,尤其影响与钴铬钼股骨头及髋臼内衬对偶的聚乙烯表面。
  • 股骨头及金属内衬因碎屑产生的划痕可能支持未来在双动摩擦界面中使用陶瓷的临床实践。

研究设计与样本

  • 共收集56例取出的双动全髋关节置换假体,评估聚乙烯内衬内外面7种损伤机制及股骨柄、股骨头和模块化内衬的微动腐蚀。
  • 对嵌入碎屑最多的3个聚乙烯内衬行扫描电子显微镜及能量色散X射线光谱分析,并使用EBRA法放射学分析髋臼杯方位。

主要发现

  • 装置翻修最常见原因为感染(36%)、松动(21%)和不稳定/脱位(18%)。
  • 聚乙烯最常见损伤机制为划痕、点蚀、抛光和嵌入碎屑,初次与翻修病例总损伤无差异。
  • 扫描电镜/能谱分析显示碎屑形态和成分与多孔钛涂层一致,源于髋臼杯松动或螺钉和垫块断裂。
  • 分别有71%和50%的假体髋臼杯前倾角和外展角位于Lewinnek安全区内。

关键数值与推荐

  • 分别有71%和50%的假体髋臼杯前倾角和外展角位于Lewinnek安全区内。

临床怎么用

  • 翻修时需关注双动全髋关节置换中第三体碎屑对聚乙烯内衬及股骨头的损伤。
  • 髋臼杯位置与碎屑来源相关,术中应确保髋臼杯及螺钉/垫块稳定以减少多孔钛涂层碎屑。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

BACKGROUND: Dual mobility (DM) articulations were introduced for total hip arthroplasty to reduce the risk of instability for patients who have a high risk of dislocation. The use of DM constructs in both primary and revision total hip arthroplasty has been steadily increasing, leading to concerns regarding potential risks of fretting corrosion, polyethylene wear, metal release, and failure due to component positioning. METHODS: A total of 56 retrieved DM constructs were collected. The inner and outer polyethylene liner surfaces were assessed for 7 damage mechanisms, and fretting corrosion was evaluated for the femoral stem, head, and modular liner. Three polyethylene liners with the greatest amounts of embedded debris were examined using scanning electron microscopy. Energy-dispersive X-ray spectroscopy was used to determine the elemental content of the debris. Acetabular cup orientation was analyzed radiographically using the EBRA (Einzel-Bild-Roentgen-Analyse) method. RESULTS: The devices were revised most frequently for infection (36%), loosening (21%), and instability/dislocation (18%). The most common polyethylene damage mechanisms were scratching, pitting, burnishing, and embedded debris, and no difference in total damage was found between primary and revision cases. Scanning electron microscopy/energy-dispersive X-ray spectroscopy revealed that debris morphology and composition were consistent with porous titanium coating, resulting from cup loosening or broken screws and augments. A total of 71% and 50% of the constructs were determined to be within the Lewinnek safe zone for inclination and anteversion, respectively. CONCLUSION: The most notable mechanisms of surface damage were due to third-body debris, especially for the polyethylene surfaces which articulate against cobalt-chromium femoral heads and acetabular liners. Scratching of the femoral head and the metal liner from this debris may support the clinical use of ceramic for DM bearing surfaces in the future.

来源:J Arthroplasty,查看原文。版权归原作者所有。

引用

  1. Spece H, Ouellette ES, Jones OL, et al. Fretting Corrosion, Third-Body Polyethylene Damage, and Cup Positioning in Primary vs Revision Dual Mobility Total Hip Arthroplasty. J Arthroplasty. 2021. PMID: 33610405. doi:10.1016/j.arth.2021.01.035

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。