带袖套陶瓷股骨头的体内腐蚀:一项取回物研究
研究对1995至2004年收集的16个带袖套陶瓷股骨头取回物进行定性和定量腐蚀评估,平均体内留存70个月。多数(31%无腐蚀、31%轻度)损伤轻微,1例(6%)严重4级腐蚀发生于唯一非工厂组装的头-袖套并与TMZF合金柄配合的病例。锥部界面平均最大线性腐蚀深度为7.7微米。
要点
- 16个带袖套陶瓷股骨头取回物中,31%无可见腐蚀、31%轻度、31%中度、6%严重4级腐蚀。
- 唯一4级腐蚀病例为研究中唯一非工厂组装的头-袖套,并与TMZF合金柄配合。
- 坐标测量机测得锥部界面平均最大线性腐蚀深度为7.7微米(范围0.9-32.9微米)。
核心结论
- 本研究首次量化带袖套陶瓷股骨头钛界面处的腐蚀,少数失败取回物中观察到可能具有临床意义的损伤和腐蚀模式,但大多数病例表现为轻微或无损伤。
研究设计与样本
- 经IRB批准的植入物取回数据库用于识别1995年至2004年收集的所有带袖套陶瓷股骨头,共16个植入物,平均体内留存70个月(范围13-241个月)。
- 14例股骨柄已知,均为钛合金;无因金属相关并发症翻修;10个植入物(63%)来自初次全髋关节置换术,6个(38%)来自翻修术。
- 损伤和腐蚀采用改良Goldberg方法进行定性分级,并使用坐标测量机(CMM)进行定量评估。
主要发现
- 16个取回植入物中,1个(6%)显示严重4级腐蚀,5个(31%)为中度3级腐蚀,5个(31%)为轻度2级腐蚀,5个(31%)在与柄锥配合的内袖套处无可见腐蚀。
- 唯一的4级腐蚀病例发生于研究中唯一非工厂组装的头-袖套,并与钛钼锆铁(TMZF)合金柄配合。
- CMM测得的锥部界面平均最大线性腐蚀深度为7.7微米(范围0.9-32.9微米)。
局限性
- 原文未报告局限性。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
BACKGROUND: The purpose of this study was to evaluate a series of retrieved sleeved ceramic femoral heads used in total hip arthroplasty (THA) and determine qualitative and quantitative damage and corrosion patterns. METHODS: An IRB-approved implant retrieval database was utilized to identify all sleeved ceramic femoral heads collected from 1995 to 2004. There were 16 implants with an average duration of in situ of 70 months (range, 13-241 months). The femoral stem was known in 14 cases and was titanium alloy in each of those cases. None were revised for metal-related complications. Ten implants (63%) were from primary THAs, and 6 (38%) were from revision THAs. Damage and corrosion were qualitatively graded using a modified Goldberg method. A quantitative assessment was performed with a coordinate measurement machine (CMM). RESULTS: Among the 16 retrieved implants, 1 (6%) demonstrated severe Grade 4 corrosion, 5 (31%) had moderate Grade 3 corrosion, 5 (31%) had mild Grade 2 corrosion, and 5 (31%) had no visible corrosion at the inner sleeve that interfaces with the stem trunnion. The only case of grade 4 corrosion occurred in the only head-sleeve in the study that was not factory assembled and was mated with a titanium molybdenum zirconium ferrous (TMZF) alloy stem. The mean maximum linear corrosion depth at the taper interface, as measured by the CMM, was 7.7 microns (range, 0.9-32.9 microns). CONCLUSION: This study is the first to quantify corrosion at the titanium interface of sleeved ceramic femoral heads. Potentially clinically significant damage and corrosion patterns were observed in a few failed retrievals; however, the majority of cases demonstrated minimal or no damage.
引用
- Wyles CC, Kolz JM, Van Citters DW, et al. In Vivo Corrosion of Sleeved Ceramic Femoral Heads: A Retrieval Study. J Arthroplasty. 2020. PMID: 33121849. doi:10.1016/j.arth.2020.10.005
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。