文献速递关节外科

第二代高交联聚乙烯上大直径金属头与陶瓷头的磨损率:平均6年随访

Wear Rates With Large Metal and Ceramic Heads on a Second Generation Highly Cross-Linked Polyethylene at Mean 6-Year Follow-Up.
PubMed 文献 · J Arthroplasty · 2017-09-14

匹配60例32或36毫米三角陶瓷头全髋关节置换与60例同尺寸金属头全髋关节置换,平均随访6年,陶瓷组与金属组线性磨损率分别为0.012 mm/y与0.018 mm/y(P=0.724),容积磨损率分别为11.9与17.3(P=0.398),均无显著差异。作者认为第二代退火高交联聚乙烯磨损率低,并因金属头锥部腐蚀问题继续将陶瓷头作为标准治疗。

要点

  • 平均6年随访,陶瓷头与金属头在全髋关节置换中的线性及容积磨损率均无显著差异。
  • 陶瓷组线性磨损率0.012 mm/y,金属组0.018 mm/y,P=0.724。
  • 作者因金属头锥部腐蚀问题,继续将陶瓷头作为标准治疗。

核心结论

  • 第二代高交联聚乙烯磨损率低,32或36毫米金属头与陶瓷头的磨损率未检测到显著差异。
  • 作者认为该结果源于第二代高交联聚乙烯优异的摩擦学性能。
  • 作者因金属头锥部腐蚀问题,继续将陶瓷头作为标准治疗。

研究设计与样本

  • 匹配研究:60例接受32或36毫米三角陶瓷头非骨水泥全髋关节置换的患者,按性别、头尺寸、随访时间和加州大学洛杉矶分校活动评分与60例32或36毫米金属头全髋关节置换匹配。
  • 测量线性磨损率和容积磨损率。

主要发现

  • 平均6年随访,陶瓷组线性磨损率0.012 mm/y(标准差0.045;95%CI 0.001-0.024),金属组0.018 mm/y(标准差0.025;95%CI 0.012-0.025),P=0.724。
  • 陶瓷组容积磨损率11.9(标准差43.0;95%CI 0.7-23.0),金属组17.3(标准差23.9;95%CI 11.1-23.4)。
  • 线性磨损率P=0.380,容积磨损率P=0.398,均无显著差异。

临床怎么用

  • 作者基于金属头锥部腐蚀问题,继续将陶瓷头作为标准治疗。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

BACKGROUND: Bearing surface wear and osteolysis are major factors limiting the durability of total hip arthroplasty (THA). Second generation annealed highly cross-linked polyethylene (HXLPE) and ceramics were introduced to THA for their excellent wear rates. However, there is little data comparing the wear rates of metal and ceramic heads on second generation HXLPE. METHODS: Sixty patients who received a noncemented THA with a 32- or 36-mm delta ceramic head were matched with 60 THAs with a 32- or 36-mm metal head based on gender, head size, follow-up, and University of California, Los Angeles activity score. Linear and volumetric wear rates were measured. RESULTS: At mean 6-year follow-up, the mean linear wear rates were 0.012 mm/y (standard deviation [SD] 0.045; 95% confidence interval [CI] 0.001-0.024) and 0.018 mm/y (SD 0.025; 95% CI 0.012-0.025) for the ceramic and metal groups, respectively (P = .724). The mean volumetric wear rates for the ceramic and metal head groups were 11.9 (SD 43.0; 95% CI 0.7-23.0) and 17.3 (SD 23.9; 95% CI 11.1-23.4), respectively. No significant differences were detectable in either the mean linear or volumetric wear rates (P = .380 and P = .398, respectively). CONCLUSION: Second generation HXLPE had low wear rates and we were unable to detect a significant difference in wear rates with 32- or 36-mm metal and ceramic heads. We believe that this is due to the excellent tribological properties of second generation HXLPE. We continue to use ceramic as standard of care because of issues of trunnionosis with metal heads.

来源:J Arthroplasty,查看原文。版权归原作者所有。

引用

  1. Gaudiani MA, White PB, Ghazi N, et al. Wear Rates With Large Metal and Ceramic Heads on a Second Generation Highly Cross-Linked Polyethylene at Mean 6-Year Follow-Up. J Arthroplasty. 2017. PMID: 29079168. doi:10.1016/j.arth.2017.09.006

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。