文献速递关节外科

取出的氧化镁稳定氧化锆股骨头表现出极小的粗糙化和研磨潜力

Retrieved Magnesia-Stabilized Zirconia Femoral Heads Exhibit Minimal Roughening and Abrasive Potential.
PubMed 文献 · J Arthroplasty · 2017-07-25

本研究对69个氧化钇稳定氧化锆(Y-TZP)和86个氧化镁稳定氧化锆(Mg-PSZ)取出的股骨头及5个未植入对照进行X射线衍射和光学轮廓仪检测,发现Y-TZP股骨头随时间发生相变、粗糙化和研磨性增加,而Mg-PSZ股骨头无相变、无点蚀、未粗糙化并保持负表面极性。

要点

  • Y-TZP股骨头在体内随时间发生相变,部分出现点蚀,但并非所有都发生灾难性粗糙化。
  • Mg-PSZ股骨头在体内长达19.2年未观察到相变、点蚀或粗糙化,并保持负表面极性。
  • CeramTec制造的Y-TZP股骨头降解程度低于Morgan和Saint Gobain制造的产品。

核心结论

  • 所有Y-TZP股骨头随体内时间增加相变,但并非所有Y-TZP股骨头都发生灾难性粗糙化。
  • Mg-PSZ股骨头在体内长达19.2年未观察到相变,其降解缺失提示关节置换中较低的磨损潜力。

研究设计与样本

  • 共检测69个Y-TZP和86个Mg-PSZ取出的股骨头,每种类型各5个从未植入的股骨头作为对照。
  • 选定股骨头通过X射线衍射测量单斜相百分比;所有股骨头通过光学轮廓仪扫描以寻找降解视觉证据并测量表面粗糙度、表面极性和功能粗糙度参数。
  • 将单斜相百分比和粗糙度数据与体内时间作图。

主要发现

  • 在Y-TZP股骨头中观察到相变的视觉证据,部分出现点蚀。
  • Y-TZP股骨头在体内粗糙化并变得更具研磨性,但CeramTec制造的产品降解程度低于Morgan和Saint Gobain制造的产品。
  • Mg-PSZ股骨头未出现点蚀、未发生相变、未在体内粗糙化,并保持负表面极性。

关键数值与推荐

  • Mg-PSZ股骨头在体内长达19.2年未观察到相变。

临床怎么用

  • 原文未据此给出推荐。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

BACKGROUND: The degradation of ceramic femoral heads made of yttria-stabilized zirconia (Y-TZP) because of tetragonal-to-monoclinic phase transformation in vivo is well-described, whereas magnesia-stabilized zirconia (Mg-PSZ) ceramics resist phase transformation in a warm aqueous environment. The purpose of this study was to evaluate phase transformation, changes in surface topography, and roughness parameters, including changes in surface polarity and abrasiveness, among retrieved zirconia femoral heads. METHODS: A total of 69 Y-TZP and 86 Mg-PSZ-retrieved femoral heads were examined, with 5 never-implanted heads of each type as controls. Selected heads were scanned by x-ray diffraction, to measure % monoclinic phase. All heads were scanned by optical profilometry to find visual evidence of degradation and to measure surface roughness, surface polarity, and the functional roughness parameters. Monoclinic phase % and roughness data were plotted vs time in vivo. RESULTS: Visual evidence of phase transformation was observed among Y-TZP femoral heads, and some exhibited pitting. Y-TZP femoral heads roughened and become more abrasive in vivo, although those made by CeramTec exhibited less degradation than those by Morgan and Saint Gobain. In contrast, Mg-PSZ heads did not exhibit pitting, undergo phase transformation, or roughen in vivo, and retained a negative surface polarity. CONCLUSION: All Y-TZP femoral heads exhibited increased phase transformation with time in vivo, although not all Y-TZP heads exhibited catastrophic roughening. No phase transformation was observed on Mg-PSZ femoral heads after up to 19.2 years in vivo. The lack of degradation among Mg-PSZ retrievals suggests a lower wear potential in joint replacement.