文献速递关节外科

全髋关节置换术中高交联聚乙烯的磨损率不因大直径关节界面而增加:一项随机对照试验

The Wear Rate of Highly Cross-Linked Polyethylene in Total Hip Replacement Is Not Increased by Large Articulations: A Randomized Controlled Trial.
PubMed 文献 · J Bone Joint Surg Am · 2016-01-01

该随机对照试验将56例接受初次全髋关节置换的老年患者术中随机分配至36 mm或28 mm金属对高交联聚乙烯关节界面,采用放射立体照相测量分析比较术后1至3年的平均磨损率。结果显示36 mm组与28 mm组年均近端磨损率分别为0.00和0.01 mm/yr,无患者近端磨损率>0.1 mm/yr,36 mm关节界面磨损率在近端、内侧二维及三维方向上均不显著大于28 mm关节界面。作者结论认为1至3年时36 mm关节界面磨损率低且不大于28 mm关节界面,但在广泛推荐前需确定长期磨损率及磨损与假体周围骨溶解的关联。

要点

  • 56例老年初次全髋关节置换患者术中随机接受36 mm或28 mm金属对高交联聚乙烯关节界面。
  • 术后1至3年年均近端磨损率36 mm组0.00 mm/yr,28 mm组0.01 mm/yr,无患者近端磨损率>0.1 mm/yr。
  • 36 mm关节界面磨损率在近端、内侧二维及三维方向上均不显著大于28 mm关节界面。

核心结论

  • 初次全髋关节置换术后1至3年,较大36 mm金属对高交联聚乙烯关节界面的磨损率低,且不大于28 mm关节界面。
  • 在广泛推荐36 mm金属对高交联聚乙烯关节界面之前,尤其在年轻活跃患者中,应确定长期磨损率及磨损与假体周围骨溶解的关联。

研究设计与样本

  • 随机对照试验,56例接受初次全髋关节置换的老年患者术中随机分配至36 mm或28 mm金属对高交联聚乙烯关节界面。
  • 通过研究设计控制可能影响磨损的因素,采用放射立体照相测量分析测量磨损。
  • 证据等级:治疗性II级。

主要发现

  • 术后1至3年年均近端磨损率36 mm关节界面组为0.00 mm/yr,28 mm关节界面组为0.01 mm/yr。
  • 无患者近端磨损率>0.1 mm/yr。
  • 所有方向平均磨损均很低。
  • 基于近端、内侧二维及三维磨损,36 mm关节界面磨损率不显著大于28 mm关节界面。

局限性

  • 在广泛推荐36 mm金属对高交联聚乙烯关节界面之前,尤其在年轻活跃患者中,应确定长期磨损率及磨损与假体周围骨溶解的关联。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

BACKGROUND: Larger articulations reduce the risk of dislocation following primary total hip arthroplasty, leading to increased use of these articulations. The wear rate of highly cross-linked polyethylene (XLPE) is low in standard-diameter articulations but remains unclear in larger articulations. The aim of this randomized controlled trial was to compare the mean wear rates of 36-mm and 28-mm metal-on-XLPE articulations between 1 and 3 years postoperatively. METHODS: Fifty-six elderly patients undergoing primary total hip arthroplasty were randomized intraoperatively to receive either a 36-mm or 28-mm metal-on-XLPE articulation. Factors that may affect wear were controlled by study design. Wear was measured using radiostereometric analysis. RESULTS: Mean annual proximal wear rates between 1 and 3 years were 0.00 and 0.01 mm/yr for the 36 and 28-mm articulation cohorts, respectively. No patient had a proximal wear rate of >0.1 mm/yr. Mean wear was very low in all directions, and the wear rate of 36-mm articulations was not significantly greater than that of 28-mm articulations on the basis of proximal, medial 2-dimensional, and 3-dimensional wear. CONCLUSIONS: The wear rate of a larger 36-mm metal-on-XLPE articulation between 1 and 3 years following primary total hip arthroplasty was low and no greater than that of a 28-mm articulation. However, before a 36-mm metal-on-XLPE articulation is widely recommended, particularly in young active patients, long-term wear rates and association between wear and periprosthetic osteolysis should be determined. LEVEL OF EVIDENCE: Therapeutic Level II. See Instructions for Authors for a complete description of levels of evidence.

来源:J Bone Joint Surg Am,查看原文。版权归原作者所有。

引用

  1. Howie DW, Holubowycz OT, Callary SA, et al. The Wear Rate of Highly Cross-Linked Polyethylene in Total Hip Replacement Is Not Increased by Large Articulations: A Randomized Controlled Trial. J Bone Joint Surg Am. 2016. PMID: 27807110