文献速递关节外科

回收的高交联聚乙烯髌骨假体的短期表面损伤机制

Short-Term Surface Damage Mechanisms of Retrieved Highly Cross-Linked Polyethylene Patellar Components.
PubMed 文献 · J Arthroplasty · 2022-11-28

本研究通过多中心骨科植入物回收项目,比较了114例伽马惰性气体灭菌聚乙烯与76例高交联聚乙烯(HXLPE)髌骨假体的翻修原因和表面损伤机制。两组患者年龄和体质指数相似(P=0.27和P=0.42),但伽马惰性组植入时间更长(平均差异3.1年;P=0.005)。最常见翻修原因为感染、松动和不稳定,两组髌骨松动发生率相似(卡方检验P=0.60和P=0.59)。最常见表面损伤模式为抛光、划痕和点蚀,伽马惰性组总表面损伤显著更高(P=0.02),但在匹配亚组中无显著差异(P=0.46)。结论认为,在短期植入时间下,HXLPE髌骨假体的临床性能与传统聚乙烯相似,但仍需长期研究。

要点

  • 在短期植入的回收髌骨假体中,HXLPE与传统伽马惰性聚乙烯的翻修原因相似。
  • 最常见的翻修原因为感染、松动和不稳定,两组髌骨松动发生率相似。
  • 伽马惰性组总表面损伤显著更高,但在匹配亚组中无显著差异。

核心结论

  • 在短期植入时间下,HXLPE髌骨假体的临床性能与传统聚乙烯相似。
  • 本研究提供了HXLPE髌骨短期回收性能的信息,但仍需长期研究。

研究设计与样本

  • 多中心骨科植入物回收项目,共纳入114例伽马惰性气体灭菌聚乙烯和76例HXLPE髌骨假体。
  • 两组患者年龄和体质指数相似(P=0.27和P=0.42),但伽马惰性组植入时间更长(平均差异3.1年;P=0.005)。
  • 基于全膝关节置换设计、髌骨形状和植入时间创建了匹配亚组。
  • 翻修原因取自翻修手术记录,表面损伤采用Hood评分法检查。
  • HXLPE组与伽马惰性组之间的差异采用Mann-Whitney U检验评估。

主要发现

  • 最常见的翻修原因为感染、松动和不稳定。
  • 两组中最常见的导致翻修的髌骨并发症均为髌骨松动,发生率相似(卡方检验P=0.60和P=0.59)。
  • 两组中最常见的表面损伤模式均为抛光、划痕和点蚀。
  • 伽马惰性组的总表面损伤显著更高(P=0.02),但在匹配亚组中无显著差异(P=0.46)。

关键数值与推荐

  • 伽马惰性组与HXLPE组患者年龄相似(P=0.27)。
  • 伽马惰性组与HXLPE组体质指数相似(P=0.42)。
  • 伽马惰性组植入时间更长(平均差异3.1年;P=0.005)。
  • 两组髌骨松动发生率相似(卡方检验P=0.60和P=0.59)。
  • 伽马惰性组总表面损伤显著更高(P=0.02),匹配亚组中无显著差异(P=0.46)。

临床怎么用

  • 原文未据此给出推荐。

局限性

  • 本研究提供的是短期回收数据,仍需长期研究。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

BACKGROUND: Previous retrieval studies of patellar components for total knee arthroplasty focused on historical designs and polyethylene materials that are no longer clinically relevant. Therefore, this study aimed to compare revision reasons and surface damage mechanisms of conventional, gamma inert sterilized polyethylene and highly cross-linked polyethylene (HXLPE) patellar components in contemporary designs from a single manufacturer. METHODS: A total of 114 gamma inert and 76 HXLPE patellar components were gathered in a multicenter orthopaedic implant retrieval program. Patient age and body mass index were similar between cohorts (P = .27 and P = .42, respectively); however, the gamma inert cohort was implanted longer (μdifference = 3.1 years; P = .005). A matched subset was created based on the total knee arthroplasty design, patellar shape, and implantation time. Revision reasons were gathered from revision operating notes, and surface damage was examined via the Hood scoring method. Differences between HXLPE and gamma inert cohorts were evaluated using Mann-Whitney U-tests. RESULTS: The most common revision reasons were infection, loosening, and instability, with the most common patellar complication resulting in revision being patellar loosening for both cohorts with similar incidences for both (chi-square; P = .60, P = .59). The most common surface damage modes were burnishing, scratching, and pitting in both cohorts. Total surface damage was significantly higher in the gamma inert components (P = .02), but not in the matched subset (P = .46). CONCLUSION: Overall, the clinical performance of HXLPE was similar to that of conventional polyethylene for patellar components with short implantation times. While this study provides much needed information on the performance of HXLPE patellae in short-term retrievals, long-term studies are still needed.

来源:J Arthroplasty,查看原文。版权归原作者所有。

引用

  1. Derr T, MacDonald DW, Klein GR, et al. Short-Term Surface Damage Mechanisms of Retrieved Highly Cross-Linked Polyethylene Patellar Components. J Arthroplasty. 2022. PMID: 36574538. doi:10.1016/j.arth.2022.11.005

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。