文献速递眼整形与眼眶眼外伤

BMP2-HAH修饰PEEK用于眼眶骨折修复的可行性

[Feasibility of polyetheretherketone loaded with bone morphogenetic protein 2 for orbital fracture repair].
PubMed 文献 · Zhonghua Yan Ke Za Zhi · 2025-01-01

该实验研究于2022年7月至2023年7月开展,将骨形态发生蛋白2复合透明质酸凝胶修饰的聚醚醚酮(PEEK-BMP2-HAH)与大鼠骨髓间充质干细胞及大鼠眼眶缺损模型结合,评估其成骨活性与骨再生能力。结果显示修饰材料在细胞黏附、增殖、碱性磷酸酶活性、矿化结节形成及成骨相关基因表达方面均优于未修饰PEEK,并在动物模型中促进新骨形成与骨钙素表达。结论提示BMP2-HAH修饰PEEK具有用于眼眶骨折修复的可行性。

要点

  • PEEK-BMP2-HAH组碱性磷酸酶活性高于PEEK组,差异有统计学意义(P<0.001)。
  • PEEK-BMP2-HAH组茜素红半定量吸光度值高于PEEK组,差异有统计学意义(P<0.001)。
  • 大鼠眼眶缺损模型中PEEK-BMP2-HAH植入组新生骨组织增加,OCN表达高于PEEK组(P<0.001)。

核心结论

  • BMP2-HAH修饰的PEEK修补材料比未修饰PEEK具有更强的大鼠细胞黏附能力、促大鼠细胞增殖活性和成骨活性。
  • BMP2-HAH修饰的PEEK可促进大鼠眼眶缺损模型骨组织再生。

研究设计与样本

  • 实验研究,于2022年7月至2023年7月开展。
  • 将大鼠骨髓间充质干细胞接种于PEEK试件与PEEK-BMP2-HAH试件并行成骨诱导培养。
  • 构建大鼠眼眶缺损模型,分别植入PEEK试件与PEEK-BMP2-HAH试件。

主要发现

  • 骨髓间充质细胞在PEEK和PEEK-BMP2-HAH试件表面均能黏附、生长。
  • 成骨诱导7 d,PEEK-BMP2-HAH组碱性磷酸酶活性[(2.36±0.18)μmol·min⁻¹·ng⁻¹蛋白]高于PEEK组[(1.00±0.18)μmol·min⁻¹·ng⁻¹蛋白],P<0.001。
  • 成骨诱导14 d,PEEK-BMP2-HAH组茜素红半定量吸光度值(0.55±0.05)高于PEEK组(0.22±0.03),P<0.001。
  • 成骨诱导7和14 d,PEEK-BMP2-HAH组Runx2的mRNA相对表达水平(3.25±0.22和2.36±0.14)均高于PEEK组(1.01±0.05和1.03±0.07),均P<0.001;OPN的mRNA相对表达水平(1.71±0.11和2.11±0.15)均高于PEEK组(1.03±0.08和1.04±0.10),均P<0.001。
  • 成骨诱导7 d,PEEK组(1.01±0.08)与PEEK-BMP2-HAH组(1.12±0.09)的Osterix mRNA相对表达水平差异无统计学意义(P>0.05);成骨诱导14 d,PEEK-BMP2-HAH组(1.77±0.17)高于PEEK组(1.02±0.06),P<0.001。

关键数值与推荐

  • 碱性磷酸酶活性:PEEK-BMP2-HAH组(2.36±0.18)μmol·min⁻¹·ng⁻¹蛋白 vs PEEK组(1.00±0.18)μmol·min⁻¹·ng⁻¹蛋白,P<0.001。
  • 茜素红半定量吸光度值:PEEK-BMP2-HAH组0.55±0.05 vs PEEK组0.22±0.03,P<0.001。
  • Runx2 mRNA相对表达水平:7 d PEEK-BMP2-HAH组3.25±0.22 vs PEEK组1.01±0.05;14 d 2.36±0.14 vs 1.03±0.07,均P<0.001。
  • OPN mRNA相对表达水平:7 d PEEK-BMP2-HAH组1.71±0.11 vs PEEK组1.03±0.08;14 d 2.11±0.15 vs 1.04±0.10,均P<0.001。
  • 植入12周后OCN表达:PEEK-BMP2-HAH植入组1.98±0.25 vs PEEK组0.98±0.11,P<0.001。

临床怎么用

  • BMP2-HAH修饰可增强PEEK材料体外成骨活性,并促进大鼠眼眶缺损模型骨组织再生。
  • 该结果为眼眶骨折修复材料改进提供实验依据,但尚未提供人体应用数据。

局限性

  • 原文未报告人体临床试验数据。
  • 原文未报告长期植入安全性或并发症数据。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

Objective: To investigate the osteogenic activity of polyetheretherketone (PEEK) modified with bone morphogenetic protein 2 (BMP2) composite hyaluronic acid hydrogel (HAH) and its feasibility for orbital fracture repair. Methods: An experimental study was conducted from July 2022 to July 2023. PEEK scaffolds were modified with BMP2-loaded HAH to form PEEK-BMP2-HAH specimens. Rat bone marrow mesenchymal cells were transplanted into PEEK or PEEK-BMP2-HAH specimens and cultured for osteogenesis induction. Cell adhesion was observed using scanning electron microscopy (SEM). Cell proliferation was assessed using the Cell Counting Kit-8 (CCK-8). Osteogenic activity was evaluated by alkaline phosphatase (ALP) staining. Mineralized nodule formation was detected by Alizarin red staining. The relative messenger ribonucleic acid (mRNA) expression levels of Runt-related transcription factor 2 (Runx 2), osteoblast-specific transcription factor (Osterix), and osteopontin (OPN) were measured by real-time quantitative polymerase chain reaction (qPCR). A rat orbital defect model was established, and PEEK specimens (PEEK implantation group) and PEEK-BMP2-HAH specimens (PEEK-BMP2-HAH implantation group) were implanted. Bone formation was observed by hematoxylin-eosin (HE) staining, and osteocalcin (OCN) expression was detected by immunohistochemical staining. Results: Bone marrow mesenchymal cells adhered to and grew on the surface of both PEEK and PEEK-BMP2-HAH specimens. After 7 days of osteogenic induction, ALP staining revealed brown-black aggregated areas on PEEK discs, while PEEK-BMP2-HAH discs exhibited distinct black particles. The ALP activity in the PEEK-BMP2-HAH group [(2.36±0.18) μmol·min⁻¹·ng⁻¹ protein] was higher than that in the PEEK group [(1.00±0.18) μmol·min⁻¹·ng⁻¹ protein], with a statistically significant difference (t=12.15, P<0.001). After 14 days of osteogenic induction, Alizarin red staining demonstrated red aggregated areas on PEEK discs, whereas the PEEK-BMP2-HAH group displayed prominent reddish-brown mineralized nodules. The semi-quantitative absorbance value of Alizarin red staining in the PEEK-BMP2-HAH group (0.55±0.05) was more pronounced than that in the PEEK group (0.22±0.03), with a statistically significant difference (t=13.33, P<0.001). After 7 and 14 days of osteogenic induction, the relative mRNA expression of Runx 2 in the PEEK-BMP2-HAH group (3.25±0.22, 2.36±0.14) was significantly higher than that in the PEEK group (1.01±0.05, 1.03±0.07), with statistically significant differences (t=22.33, P<0.001; t=17.50, P<0.001). The relative mRNA expression of OPN in the PEEK-BMP2-HAH group (1.71±0.11, 2.11±0.15) was also significantly higher than that in the PEEK group (1.03±0.08, 1.04±0.10), with statistically significant differences (t=10.47, P<0.001; t=11.10, P<0.001). After 7 days of osteogenic induction, there was no significant difference in the mRNA expression of Osterix between the PEEK group (1.01±0.08) and the PEEK-BMP2-HAH group (1.12±0.09) (t=1.87, P=0.099). However, after 14 days of osteogenic induction, the relative mRNA expression of Osterix in the PEEK-BMP2-HAH group (1.77±0.17) was significantly higher than that in the PEEK group (1.02±0.06), with a statistically significant difference (t=8.95, P<0.001). HE staining of the bone defect model showed that the formation of new bone tissue was increased in the PEEK-BMP2-HAH group compared to the PEEK group. Immunohistochemical staining revealed that 12 weeks after implantation, the expression of OCN in the PEEK-BMP2-HAH group (1.98±0.25) was significantly higher than that in the PEEK group (0.98±0.11), with a statistically significant difference (t=8.07, P<0.001). Conclusion: The BMP2-HAH-modified PEEK repair material exhibits stronger cell adhesion ability, proliferation activity, and osteogenic activity compared with unmodified PEEK repair material, and can promote bone tissue regeneration in a rat orbital defect model. 目的: 探讨骨形态发生蛋白2(BMP2)复合透明质酸凝胶(HAH)修饰的聚醚醚酮(PEEK)的成骨活性及其用于眼眶骨折修复的可行性。 方法: 实验研究,于2022年7月至2023年7月开展。在PEEK试件上修饰BMP2-HAH,形成PEEK-BMP2-HAH试件。将大鼠骨髓间充质干细胞分别接种于PEEK 试件(PEEK组)和PEEK-BMP2-HAH试件(PEEK-BMP2-HAH组)上并行成骨诱导培养。扫描电子显微镜观察细胞黏附,细胞计数试剂盒8(CCK-8)检测细胞增殖,碱性磷酸酶染色检测成骨活性,茜素红染色检测矿化结节形成,实时定量聚合酶链式反应(qPCR)检测Runt相关转录因子2(Runx 2)、成骨细胞特异性转录因子(Osterix)和骨桥蛋白(OPN)的信使RNA(mRNA)相对表达水平。构建大鼠眼眶缺损模型,并植入PEEK试件(PEEK植入组)和PEEK-BMP2-HAH试件(PEEK-BMP2-HAH植入组),苏木精-伊红(HE)染色观察骨形成,免疫组织化学染色观察骨钙素(OCN)表达。 结果: 骨髓间充质细胞在PEEK 和PEEK-BMP2-HAH试件表面均能黏附、生长。成骨诱导7 d,碱性磷酸酶染色显示PEEK组可见棕黑色聚集区域,而 PEEK-BMP2-HAH组可见明显黑色颗粒,且PEEK-BMP2-HAH组细胞碱性磷酸酶活性[(2.36±0.18)μmol·min-1·ng-1蛋白]高于PEEK组[(1.00±0.18)μmol·min-1·ng-1蛋白],差异有统计学意义(P<0.001)。成骨诱导14 d,茜素红染色显示PEEK组未见明显矿化结节,而PEEK-BMP2-HAH组可见明显的红褐色矿化结节,且PEEK-BMP2-HAH组茜素红半定量吸光度值(0.55±0.05)高于PEEK组(0.22±0.03),差异有统计学意义(P<0.001)。成骨诱导7和14 d,PEEK-BMP2-HAH组Runx2的mRNA相对表达水平(3.25±0.22和2.36±0.14)均高于PEEK组(1.01±0.05和1.03±0.07),差异均有统计学意义(均P<0.001);PEEK-BMP2-HAH组OPN的mRNA相对表达水平(1.71±0.11和2.11±0.15)均高于PEEK组(1.03±0.08和1.04±0.10),差异均有统计学意义(均P<0.001)。成骨诱导7 d,PEEK组(1.01±0.08)和PEEK-BMP2-HAH组(1.12±0.09)的Osterix的mRNA相对表达水平差异无统计学意义(P>0.05),但成骨诱导14 d,PEEK-BMP2-HAH组Osterix的mRNA相对表达水平(1.77±0.17)高于PEEK组(1.02±0.06),差异有统计学意义(P<0.001)。骨缺损模型的HE染色显示,与PEEK植入组相比,PEEK-BMP2-HAH植入组新生骨组织增加。免疫组织化学染色显示,植入12周后,PEEK-BMP2-HAH植入组OCN表达(1.98±0.25)高于PEEK组(0.98±0.11),差异有统计学意义(P<0.001)。 结论: BMP2-HAH修饰的PEEK修补材料比未修饰的PEEK修补材料具有更强的大鼠细胞黏附能力、促大鼠细胞增殖活性和成骨活性,可促进大鼠眼眶缺损模型骨组织再生。.

来源:Zhonghua Yan Ke Za Zhi,查看原文。版权归原作者所有。

引用

  1. Liu JH, Liu CH, Wu YJ, et al. [Feasibility of polyetheretherketone loaded with bone morphogenetic protein 2 for orbital fracture repair]. Zhonghua Yan Ke Za Zhi. 2025. PMID: 41218902. doi:10.3760/cma.j.cn112142-20241203-00560

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。