疝补片体内降解相关材料变化与临床特征的多变量分析
本研究对63例疝修补术后取出的聚丙烯补片(中位植入时间24个月)进行分析,表征表面氧化、结晶度和力学性能等材料变化,并采用多变量统计方法分析其与补片放置位置、病史和补片选择等临床特征的关联。结果显示,与原始对照样品相比,部分取出补片存在表面氧化、结晶度改变或力学性能变化;感染是影响补片刚度变化的显著因素,补片类别是影响聚丙烯结晶度变化的显著因素。
要点
- 63例取出聚丙烯补片(中位植入24个月)中部分出现表面氧化、结晶度或力学性能改变。
- 多变量分析显示感染是补片刚度变化的显著影响因素。
- 补片类别是聚丙烯结晶度变化的显著影响因素。
核心结论
- 体内高度可变的暴露条件使补片面临可能改变临床结局并潜在促进补片降解的机制。
- 取出聚丙烯补片在体内0.5至13年后表面化学、结晶度和力学性能发生可测量变化,且与补片放置、补片类别和感染等因素显著相关。
研究设计与样本
- 研究分析63例疝修补术后取出的补片植入物,中位植入时间24个月,采用多变量统计方法分析材料变化与临床特征的关联。
主要发现
- 与原始对照样品相比,部分取出补片存在表面氧化、结晶度改变或力学性能改变的证据。
- 多变量统计控制临床特征后,感染是影响补片刚度变化的显著因素。
- 多变量统计控制临床特征后,补片类别是影响聚丙烯结晶度变化的显著因素。
局限性
- 原文未述局限性
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
BACKGROUND: Proposed mechanisms that potentially contribute to polypropylene mesh degradation after in vivo exposure include oxidizing species and mechanical strains induced by normal healing, tissue integration, muscle contraction, and the immediate and chronic inflammatory responses. METHODS: This study explores these potential degradation mechanisms using 63 mesh implants retrieved from patients after a median implantation time of 24 months following hernia repair surgery (mesh explants) and analysis of multivariate associations between the material changes and clinical characteristics. Specifically, polypropylene mesh degradation was characterized in terms of material changes in surface oxidation, crystallinity and mechanical properties, and clinical characteristics included mesh placement location, medical history and mesh selection. RESULTS: Compared to pristine control samples, subsets of mesh explants had evidence of surface oxidation, altered crystallinity, or changed mechanical properties. Using multivariate statistical approach to control for clinical characteristics, infection was a significant factor affecting changes in mesh stiffness and mesh class was a significant factor affecting polypropylene crystallinity changes. CONCLUSIONS: Highly variable in vivo conditions expose mesh to mechanisms that alter clinical outcomes and potentially contribute to mesh degradation. These PP mesh explants after 0.5 to 13 years in vivo had measurable changes in surface chemistry, crystallinity and mechanical properties, with significant trends associated with factors of mesh placement, mesh class, and infection.
引用
- Lu X, Harman M, Todd Heniford B, et al. Analyzing material changes consistent with degradation of explanted polymeric hernia mesh related to clinical characteristics. Surg Endosc. 2022. PMID: 35257210. doi:10.1007/s00464-021-08882-4