纳米磷灰石接枝玻璃纤维桩的物理力学与三维结构实验室研究
本研究制造并表征了纳米羟基磷灰石(nHA)接枝与非接枝玻璃纤维桩,以EverStick®玻璃纤维桩为对照。结果显示ex-HA桩弯曲强度最高,第7天和第30天推出粘接强度显著高于ex-P和eS桩,但转化度低于ex-P和eS桩,空隙体积组间无显著差异。
要点
- nHA接枝玻璃纤维桩的弯曲强度和早期推出粘接强度优于非接枝桩和对照桩。
- nHA接枝桩的转化度显著低于非接枝桩和对照桩。
- 各组桩的空隙体积无显著差异,但实验桩空隙体积低于对照桩。
核心结论
- 实验桩制造成功,ex-HA桩的弯曲强度和推出粘接强度高于ex-P桩。
- ex-HA桩的转化度低于ex-P和eS桩。
- ex-HA和ex-P桩的空隙体积低于eS桩。
研究设计与样本
- 实验室研究,制造硅烷化nHA接枝(ex-HA)和非接枝(ex-P)玻璃纤维桩,以EverStick®(eS)为对照。
- 采用傅里叶变换红外光谱和扫描电镜分析结构与形貌。
- 测试转化度、弯曲强度、弯曲模量,并在人离体牙根管中评估第7、30、90天推出粘接强度。
- 第1、7、30、90天用micro-CT测量界面空隙。
- 统计采用Shapiro-Wilk检验和单因素方差分析post-hoc Tukey检验,显著性水平0.05。
主要发现
- SEM和FTIR证实玻璃纤维表面存在硅烷偶联剂。
- ex-HA桩转化度显著低于ex-P桩(p = .0008),但显著高于eS桩(p = .0014)。
- ex-HA桩弯曲强度最高,与ex-P桩差异不显著(p = .366),与eS桩差异显著(p = .029)。
- ex-HA、ex-P和eS桩的弯曲模量显著不同(p = .037)。
- ex-HA桩第7天和第30天推出粘接强度显著高于ex-P和eS桩(p = .037)。
关键数值与推荐
- 转化度:ex-HA vs ex-P p = .0008;ex-HA vs eS p = .0014。
- 弯曲强度:ex-HA vs ex-P p = .366;ex-HA vs eS p = .029。
- 弯曲模量组间比较p = .037。
- 推出粘接强度:ex-HA第7天和第30天显著高于ex-P和eS(p = .037)。
- 空隙体积组间无显著差异。
临床怎么用
- nHA接枝玻璃纤维桩可能提供更高的弯曲强度和早期粘接强度,但转化度较低需关注。
- 空隙体积组间无显著差异,实验桩空隙体积低于对照桩。
- 临床选择纤维桩时可参考其力学和粘接性能,但需结合长期效果。
局限性
- 原文未报告
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
AIM: To fabricate and characterize nano-hydroxyapatite (nHA) grafted and non-grafted glass fibre-based endodontic posts. METHODOLOGY: Experimental glass fibre posts were fabricated using silanized nHA grafted (ex-HA) and non-grafted glass fibre (ex-P) reinforced resins. The structural analysis and morphological patterns were analysed with Fourier transform infrared spectroscopy and scanning electron microscopy, respectively. EverStick® glass fibre posts (eS) were used as a control group. The degree of conversion, flexural strength, and flexural modulus was investigated and the fractured structure was evaluated with a scanning electron microscope. Root canals were prepared in human extracted teeth restored with experimental and control posts. The push-out bond strength was evaluated with radicular dentine at days 7, 30, and 90, and the presence of voids at the interface were measured at day 1, 7, 30, and 90 with micro-computed tomography. The Shapiro-Wilk test and one-way ANOVA post-hoc Tukey's test were performed. The level of significance was set at 0.05. RESULTS: The SEM and FTIR confirmed the presence of a silane-coupling agent on the glass fibres. The ex-HA post had a significantly lower degree of conversion compared to the ex-P post (p = .0008), but a significantly higher conversion than the eS post (p = .0014). The maximum flexural strength value was obtained with the ex-HA post with an insignificant difference (p = .366) compared to ex-P post and a significant difference (p = .029) compared to the eS post. The flexural modulus of ex-HA, ex-P, and eS posts were significantly different (p = .037). Similarly, the ex-HA post had a significantly higher push-out bond strength at days 7 and 30 (p = .037) compared to the ex-P and eS posts. The volume of voids had a nonlinear behaviour amongst the groups with no significant difference between the posts. CONCLUSION: The fabrication of the experimental posts was successful and the ex-HA post had greater flexural strength and push-out bond strength compared to the ex-P post. The degree of conversion of the ex-HA post was lower than the ex-P and eS posts. The volume of voids of ex-HA and ex-P posts was lower than that of eS posts.
引用
- Khan AS, AlMaimouni YK, Benrashed MA, et al. A laboratory study to assess the physical, mechanical, and 3-D structural properties of nano-apatite grafted glass fibre-based endodontic posts. Int Endod J. 2021. PMID: 34496045. doi:10.1111/iej.13630