文献速递口腔修复与种植

白榴石增强玻璃陶瓷冠13-15年临床结局

Clinical outcomes of tooth-supported leucite-reinforced glass-ceramic crowns after a follow-up time of 13-15 years.
PubMed 文献 · J Dent · 2021-06-09

最常见临床失败为不可接受的陶瓷折裂或崩瓷(5/93,5.4%)和牙周炎(4/93,4.3%),结论认为该冠长期生存率较高。

要点

  • 白榴石增强玻璃陶瓷冠平均观察14.4±1.2年总生存率为79.6%。
  • 不可接受的陶瓷折裂或崩瓷发生5/93颗(5.4%),牙周炎4/93颗(4.3%)。
  • 最常见技术并发症与咬合磨耗相关,生物学并发症不常见。

核心结论

  • 白榴石增强玻璃陶瓷冠在13-15年观察期显示79.6%的高生存率。
  • 陶瓷折裂和牙周炎构成多数临床失败原因。

研究设计与样本

  • 采用改良USPHS标准和牙周参数PPD、PI、SBI进行临床与影像学复查,并用问卷评估患者满意度和基牙术后敏感。
  • 以冠水平和患者水平计算总生存率及Kaplan-Meier生存估计,技术及生物学并发症在冠水平描述性报告,P<0.05为统计学显著。

主要发现

  • 所有冠总生存率为79.6%,多数失败发生在11.1年之后。
  • 不可接受的陶瓷折裂或崩瓷发生于5/93颗冠(5.4%)。
  • 牙周炎发生于4/93颗牙(4.3%)。
  • 最常见技术并发症与咬合磨耗相关,生物学并发症不常见。

关键数值与推荐

  • 总生存率79.6%,平均观察14.4±1.2年。
  • 不可接受陶瓷折裂或崩瓷5/93颗(5.4%)。
  • 牙周炎4/93颗(4.3%)。

临床怎么用

  • 白榴石增强玻璃陶瓷冠可用于前后牙修复,被视为安全且可预测的治疗选择。
  • 长期随访中需关注陶瓷折裂、崩瓷及牙周炎。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

OBJECTIVES: The aim of this retrospective clinical study was to investigate the survival rate, technical and biologic complications of leucite-reinforced glass-ceramic crowns after a follow-up time of 13-15 years. MATERIAL AND METHODS: Fifty-three patients with 131 crowns were invited to the follow-up visit. The reconstructions were re-examined clinically and radiographically using the modified USPHS criteria and periodontal parameters of probing pocket depth (PPD), plaque index (PI), sulcus bleeding index (SBI). Patient satisfaction and post-operative sensitivity of the abutment teeth were evaluated with a questionnaire. The overall survival rate and the Kaplan-Meier survival estimate were calculated both on crown and patient level. Technical and biological complications were reported descriptively on crown level. The p-value <0.05 was considered statistically significant. RESULTS: Thirty-eight patients (12 men, 26 women) with 93 crowns were examined. The overall survival rate of all the crowns was 79.6% after a mean observation period of 14.4 ± 1.2 years. Most of the failures occurred after 11.1 years. The most common clinical failures were inacceptable ceramic fractures or chippings, which occurred in 5 out of 93 crowns (5.4%) and periodontitis, seen in 4 out of 93 teeth (4.3%). The most frequent technical complications were related to occlusal wear. Biological complications were not common. CONCLUSIONS: Leucite-reinforced glass-ceramic crowns showed a high survival rate of 79.6% after an observation period of 13-15 years. Ceramic fractures and periodontitis accounted for the majority of clinical failures. CLINICAL SIGNIFICANCE: Leucite-reinforced glass-ceramic crowns can be considered a safe and predictable treatment choice for restoring both anterior and posterior teeth.

来源:J Dent,查看原文。版权归原作者所有。

引用

  1. Zürcher AN, Hjerppe J, Studer S, et al. Clinical outcomes of tooth-supported leucite-reinforced glass-ceramic crowns after a follow-up time of 13-15 years. J Dent. 2021. PMID: 34118285. doi:10.1016/j.jdent.2021.103721

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。