文献速递牙体牙髓病

新型自固化树脂与光固化树脂在Ⅴ类洞充填中的表面与内部适合性比较

[Superficial and internal adaptations of a new self-curing composite resin restored class Ⅴ cavity].
PubMed 文献 · Zhonghua Kou Qiang Yi Xue Za Zhi · 2020-01-01

研究将56颗离体上颌前磨牙制备Ⅴ类洞并分为两组,分别用新型自固化树脂(Bondfill SB)和光固化复合树脂(Z100)充填,经疲劳实验后用扫描电镜和透射电镜评价边缘与界面适合性。结果显示光固化树脂在牙釉质界面适合性较好,而自固化树脂在牙本质界面适合性良好。

要点

  • 疲劳实验后光固化树脂牙釉质表面完整边缘百分率显著高于自固化树脂。
  • 疲劳实验前自固化树脂牙釉质界面银沉淀物长度显著大于光固化树脂。
  • 自固化树脂在牙本质界面适合性良好,光固化树脂在牙釉质界面适合性较好。

核心结论

  • 充填Ⅴ类洞时,本研究所用光固化复合树脂在牙釉质界面有较好的表面边缘和内部界面适合性,新型自固化复合树脂在牙本质界面有良好的表面边缘和内部界面适合性。

研究设计与样本

  • 研究选用因正畸拔除的无龋人上颌前磨牙56颗,制备Ⅴ类洞后分为两组,每组28颗。
  • 实验组用预处理剂Tooth primer和新型自固化树脂Bondfill SB充填,对照组用自酸蚀粘接剂Scotchbond Universal和光固化复合树脂Z100充填。

主要发现

  • 疲劳实验前实验组牙本质表面边缘间隙较对照组小。
  • 疲劳实验前对照组牙釉质界面银沉淀物长度[(0.67±0.15)μm]显著小于实验组[(33.54±10.27)μm](P<0.05)。
  • 疲劳实验后对照组牙釉质表面完整边缘百分率[(55.08±15.20)%]显著大于实验组[(25.15±12.47)%](P<0.05)。
  • 疲劳实验后实验组充填体表面和内部更易观察到内聚破坏。
  • 透射电镜显示疲劳实验前对照组牙本质界面比实验组有更多银沉淀物,疲劳实验后对照组牙本质界面破坏主要发生于混合层下方,实验组主要发生于混合层下方和充填体内部。

临床怎么用

  • 根据牙釉质或牙本质界面选择树脂类型:光固化复合树脂在牙釉质界面适合性较好,自固化树脂在牙本质界面适合性良好。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

Objective: To investigate the superficial and internal adaptations of a new self-curing composite resin in Class Ⅴ cavities. Methods: Class Ⅴ cavities were prepared in 56 caries-free human maxillary premolars (collected from Department of Oral and Maxillofacial Surgery, Capital Medical University School of Stomatology) extracted for orthodontic reasons, and these premolars were assigned into two groups (28 specimens each group). Experimental group were restored with a pretreating agent (Tooth primer) and a new self-curing composite resin (Bondfill SB). Control group were restored with a self-etching adhesive (Scotchbond Universal) and a light-curing composite resin (Z100). The restored teeth were subjected to a fatigue test to simulate temperature change and occlusal load in oral environment: mechanical cycles (1 200 000 cycles at 49 N with a frequency of 1 Hz) and thermocycles (3 000 cycles from 5 ℃ to 55 ℃ with a dwelling time of 1 min each). Before and after fatigue test, restored teeth were immersed in an 50% ammoniacal silver nitrate solution and reduced. Superficial perfect margin percentage value and length of silver deposit along the internal interface were quantified by scanning electron microscopy (SEM). Ultrastructure of dentin bonding interface was analyzed by transmission electron microscope (TEM). Results: Before fatigue test, superficial gaps at dentin side in the specimens in experimental group were narrower than those in control group, and length of silver deposit at enamel side [(0.67±0.15) μm] in specimens in the control group was significantly lower than that in the experimental group [(33.54± 10.27) μm] (P<0.05). After the fatigue test, control group showed higher perfect margin percentage value to enamel [(55.08±15.20)%] than experimental group [(25.15±12.47)%] did (P<0.05). After the fatigue test, cohesive failures could be more easily found in experimental group than in control group at surficial and internal interfaces. In TEM results, more silver deposits were found at dentin bonding interface in control group than in experimental group before the fatigue test. After the fatigue test, the deterioration at dentin bonding interface mostly happened at the bottom of the hybrid layer in control group, while in experimental group it could be found at the bottom of the hybrid layer and in the restorative material. Conclusions: When restored in Class Ⅴ cavity, the studied light-curing composite shows better superficial and internal adaptations for enamel than the new self-curing composite resin and the new self-curing composite resin shows good superficial and internal adaptations for dentin. 目的: 探讨新型自固化树脂充填Ⅴ类洞后充填体的表面边缘和内部界面适合性。 方法: 选用因正畸需要拔除的无龋人上颌前磨牙56颗(首都医科大学口腔医学院口腔颌面外科提供),制备Ⅴ类洞,分为2组(每组28颗)。实验组用预处理剂(Tooth primer)和新型自固化树脂(Bondfill SB)充填,对照组用自酸蚀粘接剂(Scotchbond Universal)和光固化复合树脂(Z100)充填。充填后样本牙进行疲劳实验:机械循环加载(49 N、1 Hz频率120万次)和冷热循环加载(5和55 ℃的水中分别浸泡1 min,共3 000次),模拟口腔环境的咀嚼负荷和温度变化。疲劳实验前后样本牙浸入50%氨化硝酸银溶液并还原银离子。用扫描电镜检测分析充填体表面完整边缘百分率和内部界面银沉淀物长度。用透射电镜观察牙本质界面超微结构。 结果: 扫描电镜显示,疲劳实验前实验组牙本质表面边缘间隙较对照组小。疲劳实验前对照组牙釉质界面银沉淀物长度[(0.67±0.15)μm]显著小于实验组[(33.54±10.27)μm](P<0.05)。疲劳实验后对照组牙釉质表面完整边缘百分率[(55.08±15.20)%]显著大于实验组[(25.15±12.47)%](P<0.05)。疲劳实验后实验组充填体表面和内部更易观察到内聚破坏。透射电镜显示,疲劳实验前对照组牙本质界面比实验组有更多的银沉淀物;疲劳实验后对照组牙本质界面破坏主要发生于混合层下方;实验组牙本质界面破坏主要发生于混合层下方和充填体内部。 结论: 充填Ⅴ类洞时本项研究所用光固化复合树脂在牙釉质界面有较好的表面边缘和内部界面适合性,而新型自固化复合树脂在牙本质界面有良好的表面边缘和内部界面适合性。.

来源:Zhonghua Kou Qiang Yi Xue Za Zhi,查看原文。版权归原作者所有。

引用

  1. Zhang C, Yang B, Wang Y, et al. [Superficial and internal adaptations of a new self-curing composite resin restored class Ⅴ cavity]. Zhonghua Kou Qiang Yi Xue Za Zhi. 2020. PMID: 32193913. doi:10.3760/cma.j.issn.1002-0098.2020.03.005

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。