光固化复合树脂管技术移除折断根管器械:聚合循环与机械暴露的影响
本研究用改良管技术结合光固化复合树脂粘接折断的Mtwo器械碎片,评估聚合循环次数(1、2、4、6次,每次30秒,800 mW/mm2)和机械暴露方式(未处理、平行化、倒锥形预备)对粘接力的影响。结果显示失败载荷随聚合循环次数显著增加(P < .0001),超过4次无进一步获益(P > .05);倒锥形组失败载荷显著低于平行组和未处理组(P < .0001)。
要点
- 增加聚合循环次数可提高管技术粘接折断器械的失败载荷。
- 超过4次30秒聚合循环未进一步提升粘接力。
- 倒锥形机械暴露显著降低粘接力,应避免。
核心结论
- 聚合循环次数和机械暴露方式均显著影响管技术粘接折断器械的粘接力。
研究设计与样本
- 体外实验:80根Mtwo器械(15.05)切断后用于聚合循环实验,每组20根。
- 粘接材料为SDR复合树脂与Prime & Bond Active,插入玻璃纤维后光固化。
- 用拉伸测试装置(2 mm/min)测定失败载荷和失败模式。
- 统计采用Kruskal-Wallis检验或卡方检验。
主要发现
- 失败载荷随聚合循环次数显著增加(P < .0001)。
- 超过4次聚合循环无进一步获益(P > .05)。
- 倒锥形组失败载荷显著低于平行组和未处理组(P < .0001)。
- 平行组和倒锥形组粘接失败频率(20/20)显著高于未处理组(16/20)(P < .05)。
临床怎么用
- 采用管技术粘接折断器械时,可进行4次30秒光固化循环以获得较高粘接力。
- 机械暴露时应避免形成倒锥形,以维持粘接强度。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
INTRODUCTION: The purpose of this study was to investigate the influence of both polymerization cycles and mechanical exposure procedures on the adhesion of instrument fragments using a modified tube technique with a light-curing composite. METHODS: Eighty Mtwo instruments (size 15.05; VDW, Munich, Germany) were cut at a diameter of 35/100 mm and clamped in a vice with an overlap of 2 mm. Matching cannulas were filled with SDR composite (Dentsply, York, PA) and placed over the instruments. Prime & Bond Active (Dentsply Sirona, Bensheim, Germany) was used as the bonding material. Glass fiber was inserted from the opposite side into the cannula, and 1, 2, 4, or 6 polymerization cycles of 30 seconds were applied (800 mW/mm2) (n = 20/group). Sixty further identical instruments (n = 20/group) were divided into the following groups: group 1, cut at 10 mm and left unprepared (taper = 5%); group 2, parallelized using diamond instruments (taper = 0%); and group 3, prepared in a way that an inverted conical taper resulted (taper = 2%). Polymerization was performed for 2 minutes. The failure load and mode of failure were determined using a tensile testing device (2 mm/min). Data were statistically analyzed using the Kruskal-Wallis or chi-square test. RESULTS: The failure load increased significantly with the number of polymerization cycles (P < .0001). More than 4 polymerization cycles had no further benefit (P > .05). The failure load in the inverted conical group was significantly lower (P < .0001) compared with the parallel and the unprepared groups. Adhesive failure was significantly more frequent in groups 2 and 3 (20/20) than in group 1 (16/20) (P < .05). CONCLUSIONS: Both the number of polymerization cycles and the mechanical exposure procedures had a significant impact on the adhesive force when using the tube technique.
引用
- Brühl M, Urban K, Donnermeyer D, et al. Tube Technique with Light-curing Composite for Removing Fractured Root Canal Instruments: Influence of Polymerization Cycles and Mechanical Exposure. J Endod. 2020. PMID: 32037054. doi:10.1016/j.joen.2019.12.006
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。