负载三氯生的壳聚糖作为粘接树脂抗菌剂的研究
本研究配制含壳聚糖或负载三氯生壳聚糖的实验性粘接树脂,评估其即刻与长期理化及抗菌性能。结果显示5 wt.%负载三氯生壳聚糖组具有最高抗菌活性并诱导牙本质/粘接界面稳定性,而壳聚糖组生物膜形成更高。
要点
- 5 wt.%负载三氯生壳聚糖粘接树脂即刻及6个月后抗菌活性最高。
- 负载三氯生壳聚糖组诱导牙本质/粘接界面随时间稳定。
- 壳聚糖组生物膜形成高于对照组,无浮游菌抗菌活性。
核心结论
- 5 wt.%负载三氯生壳聚糖加入实验性粘接树脂显示可靠性能,即刻及六个月后抗菌活性最高,并诱导牙本质/粘接界面随时间稳定。
研究设计与样本
- 实验性粘接树脂由甲基丙烯酸酯单体和光引发剂配制,壳聚糖或负载三氯生壳聚糖以2或5 wt.%加入基础树脂,基础树脂为对照。
主要发现
- 各组转化率无差异(p > 0.05)。
- 初始Knoop硬度范围17.36(±1.56)至20.38(±1.72),GQT5%高于GCTRL(p < 0.05)。
- GCTRL的软化百分比最低(p < 0.05)。
- 即刻及长期微拉伸粘接强度无差异(p > 0.05),GCTRL和GQ2%储存后微拉伸粘接强度下降(p < 0.05)。
- 壳聚糖组生物膜形成更高(p < 0.05),负载三氯生壳聚糖组生物膜形成更低(p < 0.05),对浮游菌无活性(p > 0.05)。
关键数值与推荐
- 负载三氯生壳聚糖在5 wt.%添加时显示可靠性能,即刻及六个月后抗菌活性最高。
临床怎么用
- 负载三氯生壳聚糖粘接树脂具抗菌活性并诱导牙本质/粘接界面稳定性,可能积极影响长期边缘封闭。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVES: The aim of this study was to formulate and to evaluate the immediate and long-term physical, chemical and antibacterial properties of an experimental adhesive resin with chitosan or triclosan-loaded chitosan. MATERIALS AND METHODS: Chitosan, triclosan and triclosan-loaded chitosan were evaluated for scanning electron microscopy (SEM) and micro-Raman spectroscopy. An experimental adhesive resin was formulated with methacrylate monomers and photoinitiators. Chitosan or triclosan-loaded chitosan were added at 2 (GQ2% and GQT2%) or 5 (GQ5% and GQT5%) wt.% in the base resin. The base resin was used as control (GCTRL). The adhesives were evaluated for degree of conversion (DC), Knoop hardness (KHN), softening in solvent (ΔKHN), immediate and long-term microtensile bond-strength (μ-TBS) and antibacterial activity. RESULTS: SEM indicated triclosan sticks and chitosan porosity. Triclosan-loaded chitosan presented structures on chitosan. Micro-Raman indicated no chemical interaction between chitosan and triclosan. There was no difference among groups for DC (p > 0.05). Initial KHN ranged from 17.36 (±1.56) to 20.38 (±1.72), with higher value for GQT5% compared to GCTRL (p < 0.05). GCTRL presented the lowest ΔKHN% (p < 0.05). There were no differences in the immediate or long-term μ-TBS (p > 0.05). GCTRL and GQ2% decreased the μ-TBS after storage (p < 0.05). Chitosan groups showed higher biofilm formation (p < 0.05). Triclosan-loaded chitosan groups presented lower biofilm formation (p < 0.05). There was no activity against planktonic bacteria regardless the time of evaluation (p > 0.05). CONCLUSION: Triclosan-loaded chitosan at 5 wt.% addition in an experimental adhesive resin showed reliable properties, with the highest antibacterial activity immediately and after six months, and induced dentin/adhesive interface stability over time. CLINICAL SIGNIFICANCE: Triclosan-loaded chitosan groups showed antibacterial activity immediately and over time and induced dentin/adhesive interface stability, may positively affecting long-lasting marginal sealing.
引用
- Machado AHS, Garcia IM, Motta ASD, et al. Triclosan-loaded chitosan as antibacterial agent for adhesive resin. J Dent. 2019. PMID: 30794843. doi:10.1016/j.jdent.2019.02.002
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。