文献速递口腔修复与种植

后牙全瓷混合基台冠与混合基台加独立冠的力学行为:一项实验室研究

Mechanical behavior of posterior all-ceramic hybrid-abutment-crowns versus hybrid-abutments with separate crowns-A laboratory study.
PubMed 文献 · Clin Oral Implants Res · 2018-12-23

本研究通过体外实验比较后牙氧化锆与二硅酸锂混合基台冠及混合基台加独立冠在短钛基座上的疲劳抗力、断裂抗力和失败模式。结果显示咀嚼模拟中氧化锆组18.8%、二硅酸锂组43.8%失败,断裂抗力中位数从ZC组3730 N至LC组849 N不等,提示后牙区应用需谨慎。

要点

  • 氧化锆修复体咀嚼模拟失败率18.8%,低于二硅酸锂的43.8%。
  • ZC组断裂抗力显著高于LC和LS组,但与ZS组无显著差异。
  • 短钛基座混合修复体在后牙区应用需谨慎评估。

核心结论

  • 氧化锆和二硅酸锂混合种植修复体使用短(3 mm)钛基座时,相当数量在咀嚼模拟中已失败,尽管断裂强度高,后牙区应用应慎重考虑。

主要发现

  • 咀嚼模拟过程中,氧化锆修复体18.8%失败,二硅酸锂修复体43.8%失败。
  • 断裂抗力中位值:ZC组3,730 N,ZS组3,400 N,LS组1,295 N,LC组849 N。
  • ZC组断裂抗力显著高于LC和LS组(p ≤ 0.05),但与ZS组无显著差异。
  • 失败见于钛基座和陶瓷上部结构。

临床怎么用

  • 后牙区使用短钛基座的氧化锆或二硅酸锂混合修复体时,应充分评估疲劳失败风险,尤其二硅酸锂组失败率较高。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

OBJECTIVE: The purpose of this laboratory study was to evaluate the fatigue resistance, fracture resistance and mode of failure of posterior hybrid-abutment-crown vs. hybrid-abutment with separate crown, both bonded to short titanium bases. MATERIALS AND METHODS: Thirty-two titanium implants were embedded perpendicularly in auto-polymerizing resin. Implant-supported restorations simulating a maxillary first premolar were designed and milled using a CAD/CAM system and divided into 2 groups according to material (n = 16): zirconia (Z) and lithium disilicate (L). Each group was subdivided into two subgroups according to design (n = 8): hybrid-abutment-crown (ZS, LS) and hybrid-abutment with separate crown (ZC, LC). Each group was subjected to 1.2 million cycles of thermo-mechanical fatigue loading in a dual-axis chewing simulator at 120 N load. Surviving specimens were subjected to quasi-static loading in a universal testing machine. Mode of failure was determined under a low magnification optical microscope. RESULTS: During chewing simulation, 18.8% of zirconia and 43.8% of lithium disilicate restorations failed. The fracture resistance median values ranged from 3,730 N for group ZC, 3,400 N for group ZS, 1,295 N for group LS to 849 N for group LC. Group ZC had a statistically significant higher fracture resistance than groups LC and LS; however, it did not differ significantly from group ZS (p ≤ 0.05). Failures were seen in both titanium bases and ceramic superstructure. CONCLUSIONS: Zirconia and lithium disilicate hybrid implant-supported restorations with short (3 mm) titanium bases failed in a considerable number already during chewing simulation. Therefore, despite their high fracture strength the use in the posterior region should be considered critically.

来源:Clin Oral Implants Res,查看原文。版权归原作者所有。

引用

  1. Nouh I, Kern M, Sabet AE, et al. Mechanical behavior of posterior all-ceramic hybrid-abutment-crowns versus hybrid-abutments with separate crowns-A laboratory study. Clin Oral Implants Res. 2018. PMID: 30521070. doi:10.1111/clr.13395

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。