镍钛旋转器械缺陷传播:非接触光学轮廓术分析
研究用非接触三维光学轮廓术评估Reciproc R25与WaveOne Primary各5支镍钛器械在模拟树脂根管中行两个循环前后的表面缺陷与传播,并检验该方法准确性。结果显示两组磨损均显著增加,WaveOne磨损值显著更高,表面粗糙度从第一到第二循环显著上升,且WaveOne更明显;定性分析显示使用后所有器械沟槽表面缺陷增多。
要点
- WaveOne Primary器械各阶段缺陷均多于Reciproc R25。
- 两组磨损随循环显著增加,WaveOne的Sz中位值更高。
- 非接触光学轮廓术可准确、可重复评估镍钛器械表面。
核心结论
- WaveOne Primary器械缺陷多于Reciproc R25,且与评估阶段无关;该方法可准确、可重复、可再现地评估镍钛器械不同时间点的表面状态。
研究设计与样本
- 体外研究:Reciproc R25(n=5)与WaveOne Primary(n=5)在透明树脂块模拟根管中行两个器械循环,于距尖端3 mm、211×211 μm区域用非接触三维光学轮廓术分析。
- 统计检验显著性水平为5%。
主要发现
- 两组磨损均显著增加(P=0.007),尤其基线至第二循环之间,WaveOne磨损值显著更高(Sz中位值分别为33.68 μm与2.89 μm)。
- 两组从第一到第二循环表面粗糙度显著增加(Sa P=0.016,Sq P=0.008),以WaveOne更明显。
- 定性分析显示使用后所有器械沟槽形貌缺陷数量增多。
关键数值与推荐
- 测量参数为Sa(测量场平均粗糙度)、Sq(均方根粗糙度)、Sz(测量场平均高度)。
- 分析区域为距器械尖端3 mm、面积211×211 μm。
- 磨损比较P=0.007;粗糙度比较Sa P=0.016、Sq P=0.008。
- Sz中位值:WaveOne 33.68 μm,Reciproc 2.89 μm。
临床怎么用
- 提示临床关注镍钛旋转器械使用后表面缺陷累积,尤其WaveOne Primary磨损更明显。
- 非接触光学轮廓术可作为器械表面状态的可重复评估手段。
局限性
- 为体外模拟根管研究,样本量小(每组n=5),结果外推到临床需谨慎。
- 仅评估距尖端3 mm的211×211 μm区域及两个器械循环。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
AIM: To evaluate the presence and propagation of defects and their effects on surfaces of nickel-titanium (NiTi) instruments using noncontact, three-dimensional optical profilometry, and to assess the accuracy of this method of investigation. METHODOLOGY: The flute surface areas of instruments from two commercial instrumentation systems, namely Reciproc R25 (n = 5) and WaveOne Primary (n = 5), were assessed and compared before and after performing two instrumentation cycles in simulated root canals in clear resin blocks. All the analyses were conducted on areas measuring 211 × 211 μm, located 3 mm from the tips of the instruments. A quantitative analysis was conducted before and after the first and second instrumentation cycles, using the Sa (average roughness over the measurement field), Sq (root mean square roughness) and Sz (average height over the measurement field) amplitude parameters. All the data were submitted to statistical analysis at a 5% level of significance. RESULTS: There was a significant increase (P = 0.007) in wear in both groups, especially between baseline and the second instrumentation cycle, with significantly higher wear values being observed on WaveOne instruments (Sz median values = 33.68 and 2.89 μm, respectively, for WO and RP groups). A significant increase in surface roughness (P = 0.016 and P = 0.008, respectively, for Sa and Sq) was observed in both groups from the first to the second instrumentation cycle, mostly in WaveOne specimens. Qualitative analysis revealed a greater number of defects on the flute topography of all the instruments after use. CONCLUSIONS: More defects were identified in WaveOne Primary instruments compared to Reciproc R25, irrespective of the evaluation stage. The investigation method provided an accurate, repeatable and reproducible assessment of NiTi instruments at different time-points.
引用
- Barbosa I, Ferreira F, Scelza P, et al. Defect propagation in NiTi rotary instruments: a noncontact optical profilometry analysis. Int Endod J. 2018. PMID: 29637579. doi:10.1111/iej.12936
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。