粪肠球菌可水解牙科树脂复合材料与粘接剂
本研究检测粪肠球菌的酯酶样活性,并评估其降解甲基丙烯酸酯类树脂复合材料及全酸蚀与自酸蚀粘接剂的能力。结果显示粪肠球菌具有胆固醇酯酶样活性但无假性胆碱酯酶样活性,且能显著降解释放BisHPPP,以全酸蚀粘接剂最明显,自酸蚀粘接剂未见显著降解。
要点
- 粪肠球菌具有胆固醇酯酶样活性,可降解甲基丙烯酸酯类树脂材料。
- 全酸蚀粘接剂和树脂复合材料在全酸蚀条件下释放降解产物BisHPPP显著增加。
- 自酸蚀粘接剂在粪肠球菌存在下未显示显著降解。
核心结论
- 粪肠球菌具有酯酶样降解活性,可加速牙本质-甲基丙烯酸酯树脂界面降解,可能促进生物膜增殖和向根管系统渗透。
研究设计与样本
- 体外实验研究,检测粪肠球菌的酯酶样活性,并用高效液相色谱定量树脂降解产物BisHPPP。
主要发现
- 粪肠球菌显示胆固醇酯酶样活性为1.23 ± 0.13 U/μg干细菌,未检测到假性胆碱酯酶样活性。
- 孵育30天和/或14天后,全酸蚀粘接剂和树脂复合材料在细菌存在下BisHPPP释放量显著高于培养基对照(P < .05),自酸蚀粘接剂无显著差异。
- 孵育30天后细菌存在下BisHPPP释放量:全酸蚀粘接剂最高(23.69 ± 1.72 μg/cm2),树脂复合材料次之(3.43 ± 1.20 μg/cm2),自酸蚀粘接剂最低(0.86 ± 0.44 μg/cm2)(P < .05)。
关键数值与推荐
- 全酸蚀粘接剂孵育30天细菌存在下BisHPPP释放量为23.69 ± 1.72 μg/cm2。
- 树脂复合材料孵育30天细菌存在下BisHPPP释放量为3.43 ± 1.20 μg/cm2。
- 自酸蚀粘接剂孵育30天细菌存在下BisHPPP释放量为0.86 ± 0.44 μg/cm2。
临床怎么用
- 提示根管治疗后粪肠球菌感染可能加速全酸蚀粘接剂和树脂复合材料的降解,临床选择粘接系统时需考虑抗酶解性能。
局限性
- 本研究为体外实验,结果不能直接外推至临床复杂环境。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
INTRODUCTION: After root canal treatment, the dentin-sealer interface undergoes degradation, allowing for interfacial microbial biofilm proliferation and treatment failure. Saliva and cariogenic bacteria showed esterase-like activities (ie, cholesterol esterase [CE]-like and/or pseudocholinesterase [PCE]-like) that degrade methacrylate-based resin materials and/or the restoration-tooth interface, increasing microbial interfacial proliferation. Enterococcus faecalis is a gram-positive bacterium that is commonly detected in persistent endodontic infections. The aim of this study was to measure E. faecalis esterase-like, CE-like, and PCE-like activities and to assess the ability of the bacterium to degrade methacrylate-based resin composite (RC) and total-etch (TE) and self-etch (SE) adhesives. METHODS: CE-like and PCE-like activities from E. faecalis were measured using nitrophenyl and butyrylthiocholine substrates, respectively. The ability of E. faecalis to degrade resin composite, total-etch and self-etch adhesives was examined by quantifying the release of a universal resin degradation by-product (ie, Bis[hydroxypropoxy]-phenyl propane [BisHPPP]) using high-performance liquid chromatography. RESULTS: E. faecalis showed CE-like (1.23 ± 0.13 U/μg dry bacteria) but no PCE-like activity. After 30 days and/or 14 days of incubation, the amount of BisHPPP released was significantly higher in the presence of bacteria versus media for TE and RC but not SE (P < .05). The amount of BisHPPP released after 30 days of incubation with bacteria was highest for TE (23.69 ± 1.72 μg/cm2) followed by RC (3.43 ± 1.20 μg/cm2) and lowest for SE (0.86 ± 0.44 μg/cm2) (P < .05). CONCLUSIONS: E. faecalis possesses esterase-like degradative activity toward dental methacrylate resin restoration materials, which could accelerate the degradation of the dentin-methacrylate resin interface, increasing bacterial biofilm proliferation and penetration into the root canal system.
引用
- Marashdeh MQ, Gitalis R, Levesque C, et al. Enterococcus faecalis Hydrolyzes Dental Resin Composites and Adhesives. J Endod. 2018. PMID: 29397213. doi:10.1016/j.joen.2017.12.014
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。