文献速递牙体牙髓病

壳聚糖预处理在唾液获得性膜存在下促进牙釉质白斑病变再矿化

Remineralisation of enamel white spot lesions pre-treated with chitosan in the presence of salivary pellicle.
PubMed 文献 · J Dent · 2018-02-21

该体外研究将50个人工牙釉质白斑病变用于实验,其中48个分为6组,在pH循环7天并每次处理前形成3分钟唾液获得性膜的条件下,评估壳聚糖预处理联合生物活性玻璃的再矿化效果。结果显示壳聚糖预处理组表面及表层下显微硬度均高于阴性对照,CS-BG组表层下结构较BG组致密,但标准再矿化液仅改善表面。结论认为短期唾液膜存在时壳聚糖预处理可增强生物玻璃对白斑病变的再矿化。

要点

  • 壳聚糖预处理可增强生物玻璃对牙釉质白斑病变的表层下再矿化。
  • 短期唾液获得性膜存在下,壳聚糖预处理仍显示再矿化优势。
  • 标准再矿化液仅改善表面,表层下力学与结构无显著变化。

核心结论

  • 在短期唾液获得性膜存在时,壳聚糖预处理可增强生物玻璃对牙釉质白斑病变的再矿化。
  • 建议进一步采用长期pH循环模型与成熟获得性膜开展研究以支持临床应用。

研究设计与样本

  • 体外研究,创建50个人工牙釉质白斑病变,2个用于观察唾液获得性膜形成,48个随机分为6组(每组n=8)。
  • 分组包括生物活性玻璃浆液、含聚丙烯酸的生物活性玻璃浆液、壳聚糖预处理后生物玻璃、壳聚糖预处理后含聚丙烯酸生物玻璃、标准再矿化液和去离子水阴性对照。
  • 采用pH循环模型再矿化7天,每次处理前在病变表面形成3分钟唾液获得性膜。
  • 通过拉曼强度映射、努氏显微硬度和扫描电镜评估矿物含量变化、表面及表层下显微硬度和超微结构。
  • 数据采用单因素方差分析和Tukey检验,p<0.05认为有统计学意义。

主要发现

  • 尽管获得性膜形成不均匀,所有组在pH循环后表面矿物含量均增加。
  • 两个壳聚糖预处理组的表面和表层下显微硬度均高于阴性对照。
  • CS-BG组表层下结构较BG组致密;CS-BG+PAA组晶体尺寸较BG+PAA组大但更接近釉质样。
  • 标准再矿化液的再矿化仅限于表面,表层下力学性能与结构无显著变化。

关键数值与推荐

  • 再矿化效果以表面矿物含量增加、表面及表层下显微硬度、超微结构为评价指标。
  • 壳聚糖预处理组表面和表层下显微硬度均高于阴性对照(p<0.05)。
  • 标准再矿化液组表层下力学性能与结构无显著变化。

临床怎么用

  • 壳聚糖预处理有望临床用于再矿化表层下病变以实现病变巩固。
  • 当前证据来自短期唾液获得性膜的体外pH循环模型,临床转化需成熟获得性膜和长期模型验证。

局限性

  • 为体外研究,使用人工白斑病变与短期(3分钟)唾液获得性膜。
  • 再矿化周期仅7天,未采用长期pH循环模型与成熟获得性膜。
  • 获得性膜形成不均匀可能影响结果解释。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

OBJECTIVE: To investigate the remineralisation of chitosan pre-treated enamel white spot lesions (WSLs) by bioglass in the presence of the pellicle layer. METHODS: 50 artificial enamel white spot lesions were created by acidic gel. Two lesions were used to investigate the formation of the pellicle layer by treating with human whole saliva for 3 min. 48 lesions were assigned to 6 experimental groups (n = 8): (1) bioactive glass slurry, (2) bioactive glass containing polyacrylic acid (BG + PAA) slurry, (3) chitosan pre-treated WSLs with BG slurry (CS-BG), (4) chitosan pre-treated WSLs with BG + PAA slurry (CS-BG + PAA), (5) "standard" remineralisation solution (RS) and (6) de-ionised water (negative control, NC). Remineralisation was carried out using a pH-cycling model for 7 days. Before each treatment using remineralising agents, 3-min pellicle was formed on lesions' surfaces. Mineral content changes, surface and subsurface microhardness and ultrastructure were evaluated by Raman intensity mapping, Knoop microhardness and scanning electron microscopy, respectively. Data were statistically analysed using one-way ANOVA with Tukey's test (p < 0.05 is considered as significant). RESULTS: Despite the heterogeneously formed pellicle layer, all groups showed an increase in surface mineral content after pH-cycling. Chitosan pre-treatment enhanced the subsurface remineralisation of WSLs using bioglass as both pre-treated groups showed greater surface and subsurface microhardness compared to NC. CS-BG exhibited denser subsurface structure than BG, while in CS-BG + PAA the crystals were bigger in size but resemble more enamel-like compared to BG + PAA as shown in SEM observations. Remineralisation of RS was limited to the surface as no significant subsurface changes of mechanical properties and structure were found. CONCLUSIONS: Chitosan pre-treatment can enhance WSL remineralisation with bioglass biomaterials when a short-term salivary pellicle is present. A further investigation using a long-term pH-cycling model with mature pellicle is suggested with regards to clinical application. CLINICAL SIGNIFICANCE: Chitosan pre-treatment has the potential in clinical application to remineralise subsurface lesions to achieve lesion consolidation.

来源:J Dent,查看原文。版权归原作者所有。

引用

  1. Zhang J, Lynch RJM, Watson TF, et al. Remineralisation of enamel white spot lesions pre-treated with chitosan in the presence of salivary pellicle. J Dent. 2018. PMID: 29474950. doi:10.1016/j.jdent.2018.02.004

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。