PubMed 文献 · J Am Dent Assoc · 2018-01-01

本文报告2例根管充填Ultracal XS糊剂后意外超出根尖进入根周组织、形成硬化外源性材料并伴炎症症状的病例,对活检材料行组织病理学检查及扫描电镜、能谱、傅里叶变换红外光谱和X射线衍射分析。结论认为硫酸钡与碳酸钙与挤出后硬化材料相关,且该糊剂中氢氧化钙百分比约为厂商报告比例的2倍。

要点

  • 氢氧化钙联合硫酸钡糊剂挤出至根周或黏膜下组织可形成持续存在的硬化外源性材料
  • 该硬化材料与炎症体征和症状相关
  • 操作时应谨慎,避免糊剂超出根尖

核心结论

  • 硫酸钡和碳酸钙与Ultracal XS糊剂挤出后的硬化材料相关。
  • Ultracal XS糊剂中氢氧化钙百分比约为厂商报告比例的2倍。

研究设计与样本

  • 病例研究,报告2例根管治疗后意外挤出Ultracal XS糊剂的病例。
  • 对活检材料行组织病理学分析,并用扫描电镜、能谱、傅里叶变换红外光谱和X射线衍射进行表征。
  • 分析糊剂成分并与厂商报告比例及挤出材料进行比较。

主要发现

  • 2例根管清理成形后以Ultracal XS糊剂充填,糊剂意外超出进入根周组织。
  • 根周组织处观察到硬化外源性材料,并伴炎症体征和症状。

临床怎么用

  • 应用氢氧化钙联合硫酸钡糊剂时应谨慎操作,避免其挤出至根周和黏膜下组织。
  • 挤出可能形成持续存在的硬化外源性材料并伴炎症体征和症状。

局限性

  • 原文未报告研究局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

BACKGROUND AND OVERVIEW: Although calcium hydroxide (Ca[OH]2) paste associated with barium sulfate (BaSO4) is considered a safe agent, there is a lack of clinical research on its effects on periodontal and submucosal tissues. The aim of the authors was to report the effects of extrusion of Ultracal XS paste (Ultradent Products) in 2 cases. The authors also analyzed the paste constituents and compared them with the proportion reported by the manufacturer and the material extruded. CASE DESCRIPTION: The authors present 2 cases in which root canals were restored with Ultracal XS paste after cleaning and shaping, and there was unintentional overextension of the paste into periradicular tissues, with a hardened exogenous material observed associated with inflammatory signs and symptoms. A biopsy was performed, and the material was subjected to histopathologic analysis and characterization through scanning electron microscopy, energy dispersive x-ray spectroscopy, Fourier transform infrared spectroscopy, and x-ray diffraction. CONCLUSIONS: BaSO4 and calcium carbonate (CaCO3) were associated with a hardened material after Ultracal XS paste extrusion. The Ca(OH)2 percentage on the Ultracal XS paste was approximately 2 times greater than the proportion reported by the manufacturer. PRACTICAL IMPLICATIONS: Ca(OH)2 with BaSO4 paste application should be performed carefully, and its extrusion to periradicular and submucosal tissues should not occur. Its extrusion may result in the formation of a persistent exogenous material of hardened consistency associated with inflammatory signs and symptoms.

来源:J Am Dent Assoc,查看原文。版权归原作者所有。