环氧树脂基封闭剂溶解的新见解
本研究评估了牙科不常用溶剂对环氧树脂基封闭剂AH Plus的溶解效果及超声搅拌(UA)的影响。通过失重、维氏显微硬度、扫描电镜(SEM)和X射线衍射(XRD)量化溶解能力,并在离体牙中初步验证。结果显示乙酸乙酯和甲基乙基酮(MEK)溶解能力接近氯仿,UA可增强溶解,MEK尤其适合作为AH Plus的替代溶剂。
要点
- MEK和乙酸乙酯是氯仿或二甲苯的良好替代溶剂。
- 超声搅拌可增强AH Plus封闭剂的溶解。
- MEK在短时间内具有高溶解能力,尤其配合超声搅拌。
核心结论
- MEK和乙酸乙酯是氯仿或二甲苯的优良替代溶剂。
- MEK在短时间内对AH Plus封闭剂具有高溶解能力,尤其配合超声搅拌,且无氯仿的潜在危害。
- 结果应鼓励进一步研究以确认其临床相关性。
研究设计与样本
- 体外实验量化AH Plus封闭剂在多种溶剂(桉叶油醇、二甲苯、氯仿、EndoSolv R、EndoSolv E、MEK、乙酸乙酯)中的溶解及超声搅拌影响。
- 采用失重、维氏显微硬度、SEM和XRD评估溶解能力,结果用析因方差分析比较,显著性水平0.05。
- 在离体牙中进行初步离体研究,以MEK配合超声搅拌作为最终冲洗,SEM评估根管壁清洁度。
主要发现
- 新溶剂乙酸乙酯和MEK表现出高溶解能力,几乎达到氯仿水平。
- 超声搅拌增加了溶解。
- 维氏值证实了溶解实验的结果。
- SEM和XRD显示溶剂主要影响封闭剂的有机成分。
- 离体实验结果证实了浸泡模型的发现。
临床怎么用
- 可考虑使用MEK或乙酸乙酯替代氯仿或二甲苯溶解AH Plus封闭剂。
- 配合超声搅拌可增强MEK的溶解效果。
- MEK可在短时间内有效溶解封闭剂,且避免氯仿危害。
局限性
- 结果需进一步研究以确认临床相关性。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
INTRODUCTION: The purpose of this study was to evaluate the use of solvents that are not traditionally used in dentistry for the dissolution of an epoxy resin-based sealer and the effect of ultrasonic agitation (UA). METHODS: The dissolution of the AH Plus sealer (Dentsply DeTrey, Konstanz, Germany) and the effect of UA in various solvents (eucalyptol, xylene, chloroform, EndoSolv R [Septodont, Cedex, France], EndoSolv E [Septodont], methyl ethyl ketone [MEK], and ethyl acetate) were quantified. The dissolving capacity was assessed by weight loss, Vicker microhardness, scanning electron microscopy (SEM), and X-ray diffraction (XRD). The results were compared with factorial analysis of variance using IBM SPSS Statistics 23.0 software (IBM, Armonk, NY), considering a 0.05 significance level. A preliminary ex vivo study was performed in extracted teeth, with MEK activated by UA as the final irrigation after mechanical removal of the filling material. SEM was used for assessing the cleanliness of the root canal walls. RESULTS: The new solvent proposals, ethyl acetate and MEK, exhibited high dissolution ability, almost reaching chloroform. UA increased dissolution. Vicker values corroborated the dissolution assays. SEM and XRD revealed that solvents affected mainly the organic component of the sealer. Ex vivo results confirmed the immersion model findings. CONCLUSIONS: MEK and ethyl acetate proved to be excellent alternatives to chloroform or xylene solvents. MEK presented a high sealer dissolving ability in a short period, especially with UA, without the potential hazards of chloroform, suggesting it is a good approach to AH Plus sealer's dissolution empowered by UA. These results should encourage further studies in order to confirm their clinical relevance.