种植体成形术对标准直径种植体抗折强度及表面粗糙度的影响
本体外研究对20枚标准直径(4.1 mm)外连接钛种植体进行测试,其中10枚行种植体成形术,另10枚为对照。结果显示,成形术平均耗时10分48秒,最终表面粗糙度Sa值0.1±0.02 μm显著低于原始0.75±0.08 μm(p=.005),种植体内体直径最小缩减0.19±0.03 mm,试验组与对照组最大抗压力无统计学显著差异(896 N vs 880 N)。结论认为种植体成形术虽技术敏感且耗时,但似乎不显著改变标准直径外连接种植体的抗折强度。
要点
- 种植体成形术平均耗时10分48秒,最终表面粗糙度Sa值0.1±0.02 μm,显著低于原始0.75±0.08 μm(p=.005)。
- 种植体内体直径最小缩减0.19±0.03 mm,试验组与对照组最大抗压力无统计学显著差异(896 N vs 880 N)。
- 结论认为种植体成形术不显著改变标准直径外连接种植体的抗折强度,但需更大样本确认。
核心结论
- 种植体成形术虽技术敏感且耗时,但似乎不显著改变标准直径外连接种植体的抗折强度。
研究设计与样本
- 体外研究,共20枚外连接螺纹状钛种植体,10枚行种植体成形术,10枚为对照。
主要发现
- 种植体成形术平均耗时10分48秒(标准差1分22秒)。
- 最终表面粗糙度Sa值0.1±0.02 μm,显著低于原始0.75±0.08 μm(p=.005)。
- 种植体内体直径最小缩减0.19±0.03 mm。
- 试验组与对照组最大抗压力分别为896 N和880 N,无统计学显著差异。
- 宏观表面光滑,但存在小的钛屑和硅碎屑。
关键数值与推荐
- 使用硅抛光器可获得Sa值低于0.1 μm的光滑表面。
临床怎么用
- 种植体成形术可用于标准直径外连接种植体,但需注意技术敏感性和耗时。
- 术后表面粗糙度显著降低,可能有利于减少菌斑附着。
局限性
- 需要更大样本以确认种植体成形术不显著影响标准直径外连接种植体的最大抗压力。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVE: To assess the effect of implantoplasty on the fracture resistance, surface roughness, and macroscopic morphology of standard diameter (4.1 mm) external connection dental implants. MATERIALS AND METHODS: An in vitro study was conducted in 20 screw-shaped titanium dental implants with an external connection. In 10 implants, the threads and surface were removed and polished with high-speed burs (implantoplasty), while the remaining 10 implants were used as controls. The final implant dimensions were recorded. The newly polished surface quality was assessed by scanning electron microscopy (SEM) and by 3D surface roughness analysis using a confocal laser microscope. Finally, all the implants were subjected to a mechanical pressure resistance test. A descriptive analysis of the data was made. Also, Student's t tests were employed to detect differences regarding the compression tests. RESULTS: Implantoplasty was carried out for a mean time of 10 min and 48 s (standard deviation (SD) of 1 min 22 s). Macroscopically, the resulting surface had a smooth appearance, although small titanium shavings and silicon debris were present. The final surface roughness (Sa values 0.1 ± 0.02 μm) was significantly lower than that of the original (0.75 ± 0.08 μm Sa ) (p = .005). There was minimal reduction in the implant's inner body diameter (0.19 ± 0.03 mm), and no statistically significant differences were found between the test and control implants regarding the maximum resistance force (896 vs 880 N, respectively). CONCLUSIONS: Implantoplasty, although technically demanding and time-consuming, does not seem to significantly alter fracture resistance of standard diameter external connection implants. A smooth surface with Sa values below 0.1 μm can be obtained through the use of silicon polishers. A larger sample is required to confirm that implantoplasty does not significantly affect the maximum resistance force of standard diameter external connection implants.
引用
- Costa-Berenguer X, García-García M, Sánchez-Torres A, et al. Effect of implantoplasty on fracture resistance and surface roughness of standard diameter dental implants. Clin Oral Implants Res. 2017. PMID: 28736922. doi:10.1111/clr.13037
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。