MTA根尖屏障厚度对未成熟牙抗折强度的影响
本研究比较不同厚度MTA根尖屏障对模拟未成熟上颌前牙抗折强度的影响。结论建议使用MTA根尖屏障而非全根管充填以提高未成熟牙抗折强度。
要点
- 3mm MTA根尖屏障组抗折强度最高(P < .05)。
- 3mm与6mm MTA屏障组间抗折强度无显著差异(P > .05)。
- 建议使用MTA根尖屏障而非全根管充填以增强未成熟牙抗折强度。
核心结论
- MTA应作为根尖屏障而非根管充填材料使用,以提高未成熟牙的抗折强度。
主要发现
- 负对照组的抗折强度最低。
- 3mm根尖屏障组的抗折强度最高(P < .05)。
- 3mm与6mm根尖屏障组之间无显著差异(P > .05)。
关键数值与推荐
- 3mm MTA根尖屏障组抗折强度最高(P < .05)。
- 3mm与6mm MTA根尖屏障组间无显著差异(P > .05)。
临床怎么用
- 在未成熟牙根尖屏障术中,使用3mm厚度MTA即可有效提高抗折强度,无需全根管充填MTA。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
INTRODUCTION: The aim of this study was to compare the fracture resistance of simulated immature teeth after using different thicknesses of mineral trioxide aggregate (MTA) apical plugs. METHODS: Fifty-two human maxillary anterior teeth were used. Five teeth were the positive control group; they were prepared using Peeso reamers to simulate immature teeth without any access cavity preparation. Access cavities of the 47 teeth were prepared, and the canals were instrumented with Peeso reamers. Five teeth served as the negative control; they were filled with calcium hydroxide. Forty-two teeth were divided into 3 groups; in groups 1, 2, and 3, MTA was placed into canals as a 3-mm and a 6-mm apical plug and a thorough canal length, respectively. The rest of the canals in groups 1 and 2 were filled with gutta-percha and AH Plus sealer (Dentsply DeTrey, Konstanz, Germany). After the storage period, the roots were covered with a polyether impression material and were embedded into self-curing resin blocks. Each specimen was then subjected to fracture testing using a universal testing machine. Data were analyzed using 1-way analysis of variance with the Tukey post hoc test for multiple comparisons. RESULTS: The negative group showed the lowest fracture resistance compared with the other groups. The 3-mm apical plug group showed the highest fracture resistance (P < .05). No significant differences were found between the 3-mm and 6-mm apical plug groups (P > .05). CONCLUSIONS: MTA should be used as an apical plug instead of root canal filling material to increase the fracture resistance of immature teeth.
引用
- Çiçek E, Yılmaz N, Koçak MM, et al. Effect of Mineral Trioxide Aggregate Apical Plug Thickness on Fracture Resistance of Immature Teeth. J Endod. 2017. PMID: 28735788. doi:10.1016/j.joen.2017.05.007
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。