纤维桩不同预处理对根管牙本质推出粘接强度影响的评价

Evaluation of Various Pretreatments to Fiber Post on the Push-out Bond Strength of Root Canal Dentin.
PubMed 文献 · J Endod · 2017-05-17

这项体外研究将50颗新鲜拔除的下颌单根前磨牙行激光活化冲洗(17% EDTA 5 mL冲洗120秒),50根石英纤维桩随机分为喷砂、两种掺钕钇铝石榴石激光、9.7%氢氟酸酸蚀和对照5组,每组10根。结果显示各组推出粘接强度无统计学差异,纤维桩各种处理未提高根管牙本质的推出粘接强度。

要点

  • 激光活化冲洗联合17% EDTA对根管牙本质玷污层去除有明显效果。
  • 喷砂组中份推出粘接强度最高,对照组根尖份最低。
  • 纤维桩不同表面处理均未提高推出粘接强度,组间无统计学差异。

核心结论

  • 在本研究局限内,激光活化冲洗联合17% EDTA对根管牙本质玷污层去除有明显效果,并在断裂模式(粘接失败,树脂-桩界面)中体现。
  • 纤维桩的各种处理未提高根管牙本质的推出粘接强度。

研究设计与样本

  • 体外研究,50颗新鲜拔除的下颌单根前磨牙全部行激光活化冲洗,50根石英纤维桩随机分为5组,每组10根。

主要发现

  • 推出粘接强度最高值出现在喷砂组中份,最低值出现在对照组根尖份。
  • 无论牙本质部位如何,各组间均无统计学差异。
  • 在各处理组内比较不同牙本质部位的推出粘接强度时,除N2组外其余各组均观察到显著差异(P < .05)。

关键数值与推荐

  • 激光活化冲洗使用17% EDTA 5 mL冲洗120秒,铒铬钇钪镓石榴石激光参数为0.50 W、20 Hz、25 mJ。
  • 掺钕钇铝石榴石激光照射参数为2 W、200 mJ、10 Hz,脉冲持续时间分别为180或320微秒。
  • 氢氟酸组使用9.7%氢氟酸酸蚀,对照组不作处理。
  • 推出粘接强度测试前所有标本横断切成1 mm厚根切片,数据分析采用单因素方差分析/Tukey事后检验(α = 0.05)。

临床怎么用

  • 原文未据此给出推荐。

局限性

  • 原文在结论中写明「在本研究局限内」。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

INTRODUCTION: The aim of this in vitro study was to compare the effect of different pretreatments (fiber post) with the laser-activated irrigation (LAI) technique (for removal of the smear layer) on root canal dentin in terms of push-out bond strength (PBS) in a fiber post. METHODS: Fifty freshly extracted mandibular single-rooted premolars were prepared, and LAI was applied to all roots (17% EDTA was 5 mL for 120 seconds with an erbium, chromium:yttrium-scandium-gallium-garnet laser [0.50 W, 20 Hz, 25 mJ]). In addition, 50 quartz fiber posts were randomly assigned to 5 groups (n = 10) according to the surface treatments as follows: group S (sandblasting), group N1 and group N2 (neodymium:yttrium-aluminum-garnet laser irradiation [2 W, 200 mJ, 10 Hz, with pulse durations of 180 or 320 microseconds), group HF (9.7% hydrofluoric acid etched), and group C (control with no treatment). Dual-cure resin cement was adhered onto the fiber posts after they were covered with a silane agent, and then the posts were placed into the canal space using a Lentulo spiral. The PBS test was performed after all specimens were transversally sectioned (root slices of 1-mm thickness). Data were analyzed with 1-way analysis of variance/Tukey post hoc test (α = 0.05). RESULTS: The highest PBS value was observed in group S (middle part), and the lowest value was observed in group C (apical part). There were no statistical differences among the groups regardless of the part. Furthermore, when the PBS values of the different parts of dentin were compared within treated groups, significant differences were observed in all groups except group N2 (P < .05). CONCLUSIONS: Within the limitations of this study, it can be concluded that the LAI technique when used with 17% EDTA had a significant effect on the amount of smear layer removed from the root canal dentin, which was also detected in the fracture pattern (adhesive failure [resin-post interface]). However, the various treatments of the fiber post did not improve the PBS of the root dentin.

来源:J Endod,查看原文。版权归原作者所有。