文献速递牙体牙髓病

环境温度显著影响镍钛旋转器械的弯曲疲劳抗力

Environmental Temperature Drastically Affects Flexural Fatigue Resistance of Nickel-titanium Rotary Files.
PubMed 文献 · J Endod · 2017-05-02

研究比较了6种镍钛旋转器械在室温20°C与冷却环境-20°C下的弯曲循环疲劳寿命,每种系统各40个新样本、每组20个。所有器械在冷却环境下的循环至失败次数均显著高于室温组,疲劳抗力增加幅度为274%至854%,断裂片段长度无差异。

要点

  • 冷却环境(-20°C)下所有测试镍钛器械的循环至失败次数均显著高于室温(20°C)组。
  • 循环疲劳抗力的增加幅度为274%至854%。
  • 各器械断裂片段长度在两组间无差异。

核心结论

  • 低环境温度使传统合金及不同热处理制造的镍钛根管器械的弯曲疲劳抗力大幅增加。

研究设计与样本

  • 体外研究,每种系统测试40个新样本,室温组(20°C±2°C)与冷却环境组(-20°C±2°C)各20个。
  • 测试系统包括ProTaper Universal F2、ProTaper Gold F2、Twisted Files SM2、Mtwo #25.06、Vortex Blue #30.04和#40.06。

主要发现

  • 所有测试系统的冷却环境组平均循环至失败次数均显著高于室温组(P < .05)。
  • 循环疲劳抗力的增加幅度为274%至854%。
  • 不同组间断裂片段长度无差异(P < .05)。

临床怎么用

  • 原文未据此给出临床推荐。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

INTRODUCTION: The aim of the present study was to analyze how a low environmental temperature can affect the fatigue life of instruments made by different types of heat-treated nickel-titanium alloys. METHODS: The flexural cyclic fatigue of 40 new specimens for each of the following systems was tested for cyclic fatigue resistance: ProTaper Universal F2 (Dentsply Maillefer, Ballaigues, Switzerland), ProTaper Gold F2 (Dentsply Tulsa Dental Specialties, Tulsa, OK), Twisted Files SM2 (SybronEndo, Orange, CA), Mtwo #25.06 (VDW, Munich, Germany), and Vortex Blue #30.04 and #40.06 (Dentsply Tulsa Dental Specialties). Instruments were tested at 2 different environmental temperatures: 20°C (±2°C) for room temperature (RT) group and -20°C (±2°C) for the cooled environment (CE) group (n = 20). The number of cycles to failure (NCF) and the length of the fractured fragment (FL) were recorded. The means and standard deviations of NCF and FL were then calculated; NCF data were statistically analyzed using a paired t test between groups RT and CE for each instrument tested (P < .05), whereas FL data were analyzed using analysis of variance (P < .05). RESULTS: The mean NCF values measured were significantly higher for the CE groups than the RT groups in all the systems tested (P < .05). The increase in cyclic fatigue resistance varied from 274%-854%. No differences in FL were registered among the different groups (P < .05). CONCLUSIONS: A low environmental temperature determines a drastic increase in the flexural fatigue resistance of NiTi endodontic instruments manufactured with traditional alloy and different heat treatments.

来源:J Endod,查看原文。版权归原作者所有。