使用过与全新根管疏通路径锉的循环疲劳抗力比较
本研究比较使用过与全新ProGlider和PathFile #2旋转根管疏通路径锉的循环疲劳抗力。40支ProGlider和40支PathFile #2用于预备40个J形透明丙烯酸块,另设新锉对照组,在5mm曲率半径、60°弯曲角的不锈钢人工根管内旋转至折断并记录折断循环数。使用过锉的折断循环数低于新锉但差异无统计学意义(P > .05);PathFile #2的循环疲劳抗力显著高于ProGlider(P < .05)。
要点
- 使用过与全新根管疏通路径锉的折断循环数差异无统计学意义(P > .05)。
- PathFile #2的循环疲劳抗力显著高于ProGlider(P < .05)。
- 本研究结果需在研究的局限性范围内解读。
核心结论
- 在本研究的局限性范围内,使用过的根管疏通路径锉折断循环数低于新锉,但差异无统计学意义(P > .05)。
- PathFile #2的循环疲劳抗力显著高于ProGlider(P < .05)。
研究设计与样本
- 共使用40支ProGlider和40支PathFile #2器械。
- 第1组20支PathFile #2和第2组20支ProGlider用于预备共40个J形透明丙烯酸块。
- 第3组(对照组)20支新PathFile和第4组(对照组)20支新ProGlider纳入研究。
- 循环疲劳测试在不锈钢人工根管中进行,曲率半径为5 mm,弯曲角度为60°。
- 全部80支器械旋转至折断,记录折断循环数(NCF)。
主要发现
- 使用过的根管疏通路径锉的NCF低于新锉,但差异无统计学意义(P > .05)。
- 使用过和全新的PathFile #2的循环疲劳抗力均显著高于ProGlider(P < .05)。
局限性
- 原文提及结论需在本研究的局限性范围内解读,但摘要未具体列出局限性内容。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
INTRODUCTION: The purpose of this study was to compare the cyclic fatigue resistance of used and new ProGlider (Dentsply Maillefer, Ballaigues, Switzerland) and PathFile (Dentsply Maillefer) rotary glide path files. METHODS: Forty ProGlider and 40 PathFile #2 instruments were used in the present study. In group 1, 20 PathFile #2 files and, in group 2, 20 ProGlider files were used to prepare a total of 40 J-shaped transparent acrylic blocks. In group 3 (control group), 20 new PathFile files and, in group 4 (control group), 20 new ProGlider files were included. Cyclic fatigue testing of instruments was performed in a stainless steel artificial canal with a 5-mm radius of curvature and a 60° angle of curvature. All 80 instruments were rotated until fracture, and the number of cycles to failure (NCF) was recorded. Data were analyzed using 1-way analysis of variance to determine any statistical difference; the significance was determined at the 95% confidence level. RESULTS: The used glide path files' NCF was lower than the new ones; however, this difference was not statistically significant (P > .05). The cyclic fatigue resistance of the used and new PathFile #2 files was statistically significantly higher than that of the ProGlider files (P < .05). CONCLUSIONS: Within the limitations of the present study, the used glide path files' NCF was lower than the new ones; however, this difference was not statistically significant.
引用
- Özyürek T, Uslu G, İnan U, et al. A Comparison of the Cyclic Fatigue Resistance of Used and New Glide Path Files. J Endod. 2017. PMID: 28139286. doi:10.1016/j.joen.2016.10.044
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。