WaveOne与WaveOne Gold小号、初号和大号器械循环疲劳抗性的比较
在两种不同弯曲角度和半径的模拟根管中,比较WaveOne(WO)与WaveOne Gold(WOG)小号、初号和大号镍钛器械的循环疲劳抗性。每种曲率下每组10根器械旋转至折断,记录折断时间与折断尖端长度。所有型号及两种曲率下WOG抗性均高于WO(P < .001),折断长度组间相似(P > .05)。
要点
- 所有型号及两种曲率下,WOG器械循环疲劳抗性均高于对应型号WO器械(P < .001)。
- 60°曲率下WOG抗折断能力约为WO的2倍,90°曲率下约为3倍。
- 各组器械折断部分长度相似(P > .05)。
核心结论
- 在本研究局限性范围内,WOG器械比WO器械更抗循环疲劳。
研究设计与样本
- 在两种不同角度和曲率半径的弯曲人工根管中测试120根镍钛根管器械,WO与WOG小号、初号和大号器械每组每种曲率n=10,每根器械旋转至折断,记录折断时间并测量折断尖端长度。
主要发现
- 在所有测试型号和两种曲率下,WOG器械的循环疲劳抗性均高于对应型号的WO器械(P < .001)。
- 在60°弯曲角度下,WOG器械抗折断能力约为WO器械的2倍;在90°弯曲角度下,WOG器械抗折断能力为WO器械的3倍。
- 所有组间器械折断部分长度相似(P > .05)。
临床怎么用
- 原文未据此给出推荐。
局限性
- 原文未报告局限性。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
INTRODUCTION: To compare the cyclic fatigue of resistance of WaveOne (WO; Dentsply Maillefer, Ballaigues, Switzerland) and WaveOne Gold (WOG, Dentsply Maillefer) small, primary, and large instruments in simulated root canals. Each instrument was rotated until fracture occurred. METHODS: One hundred twenty nickel-titanium endodontic instruments were tested in two different curved artificial canals with different angles and radii of curvatures. WO and WOG small, primary, and large instruments were evaluated (n = 10 for each curvature). Each instrument was rotated until fracture occurred. The time to failure was recorded, and the length of the fractured tip was measured. An independent Student't test was used to compare the means between the 2 groups. One-way analysis of variance and Tukey' post hoc tests were used for multiple comparisons (P < .05). RESULTS: At all the sizes tested and both curvatures, the cyclic fatigue resistance of the WOG instruments was higher than that of the WO instruments of corresponding sizes (P < .001). The WOG instruments were approximately twice as resistant to failure as the WO instruments were at a 60° angle of curvature, whereas the WOG instruments were 3 times more resistant at a 90° angle of curvature. The length of the fractured part of the instruments was similar among all the groups (P > .05). CONCLUSIONS: Within the limitations of this study, WOG instruments were more resistant to cyclic fatigue than WO instruments.
引用
- Adıgüzel M, Capar ID. Comparison of Cyclic Fatigue Resistance of WaveOne and WaveOne Gold Small, Primary, and Large Instruments. J Endod. 2017. PMID: 28216272. doi:10.1016/j.joen.2016.11.021