文献速递牙体牙髓病口腔修复与种植

修复体负荷与继发龋损的关联受修复材料弹性调节

The association between loading of restorations and secondary caries lesions is moderated by the restoration material elasticity.
PubMed 文献 · J Dent · 2017-01-05

本研究将模拟界面间隙的牙本质-修复体标本在10天内暴露于产龋的鼠李糖乳杆菌生物膜,同时施加不同载荷(每标本0/42/84/126克,每组12个),使用两种弹性模量不同的复合树脂(低弹性模量复合树脂、高弹性模量复合树脂),用横向显微放射照相评估表层和界面(壁)病损的矿物质丢失。结果显示,表层矿物质丢失与载荷、材料及其交互作用均无显著关联;深部界面(壁)病损中,载荷(p=0.023)而非材料(p=0.382)有显著效应,两者交互作用显著(p=0.01),每标本≥84克的载荷与更高的壁病损矿物质丢失相关。结论认为超过某一阈值的载荷显著增加界面(壁)病损矿物质丢失,该关联受修复材料弹性调节,但临床相关性尚不明确,需未来研究进一步理解。

要点

  • 深部界面(壁)病损中载荷有显著效应(p=0.023),材料无显著效应(p=0.382)。
  • 载荷与材料交互作用显著影响壁病损矿物质丢失(p=0.01)。
  • 每标本≥84克的载荷与更高的壁病损矿物质丢失相关。

核心结论

  • 超过某一阈值的载荷显著增加界面(壁)病损矿物质丢失,该关联受放置的修复材料弹性调节。
  • 作者指出其发现的临床相关性尚不明确,需要未来研究理解载荷和材料弹性如何确切影响继发病损诱导。

研究设计与样本

  • 体外研究:将模拟界面间隙的牙本质-修复体标本暴露于产龋的鼠李糖乳杆菌生物膜10天,同时施加不同载荷(每标本0/42/84/126克,每组12个),使用两种复合树脂(低弹性模量复合树脂、高弹性模量复合树脂)。
  • 采用横向显微放射照相评估表层和界面(壁)病损的矿物质丢失,用广义线性模型评估载荷、材料及其交互作用与矿物质丢失的关联。

主要发现

  • 表层矿物质丢失与载荷、材料或其交互作用均无显著关联(p值范围0.062至0.526)。
  • 深部界面(壁)病损中,施加的载荷有显著效应(p=0.023),材料无显著效应(p=0.382)。
  • 载荷与材料的交互作用显著影响矿物质丢失(p=0.01)。
  • 每标本≥84克的载荷与更高的壁病损矿物质丢失相关。

临床怎么用

  • 原文未据此给出推荐。

局限性

  • 作者指出其发现的临床相关性尚不明确,需要未来研究理解载荷和材料弹性如何确切影响继发病损诱导。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

OBJECTIVES: Secondary caries limits the longevity of restorations and is thought to be associated with faulty restorations, e.g. dentin-restoration interfacial gaps. Recent evidence indicates that loading of restorations might aggravate the effects of gaps on interfacial mineral loss. It is unclear if this effect of loading is dose-dependent or not, and if restoration material properties like elasticity moderate the association between load and mineral loss. We hypothesized that mineral loss of secondary lesions increases with increasing load, and that this association is moderated by the elastic modulus of the placed restoration material. METHODS: Dentin-restoration specimens with simulated interfacial gaps were submitted to cariogenic Lactobacillus-rhamnosus-biofilms for 10days, and concurrently loaded with different loads (0/42/84/126g per specimen, n=12/group). Two different composites (LEC: low elastic-modulus composite, HEC: high elastic-modulus composite) were employed. Transversal microradiography was used to evaluate the superficial and interfacial (wall) lesion mineral loss. Generalized linear modeling (GLM) was used to evaluate the association between loading, material and their interaction on mineral loss. RESULTS: Surface mineral loss was not significantly associated with loading, material, or their interaction (p-values ranged between p=0.062 and 0.526). For deep interfacial (wall) lesions, the applied load (p=0.023) but not the material (p=0.382) showed a significant effect. The interaction between both significantly affected mineral loss (p=0.01). Loads of ≥84g per specimens were associated with higher wall lesion mineral loss. CONCLUSIONS: Loads above a certain threshold significantly increased interfacial (wall) lesion mineral loss. This association was moderated by the elasticity of the placed restoration materials. CLINICAL SIGNIFICANCE: The clinical relevance of our findings remains unclear, as future studies are needed to understand how exactly both load and material elasticity affect secondary lesion induction.

来源:J Dent,查看原文。版权归原作者所有。