填料粒径对高填充3D打印牙科树脂性能的影响
本研究评估了两种含不同粒径硅烷化钡玻璃填料的高填充实验性3D打印牙科树脂(微米级1.5µm与亚微米级0.7µm)在热循环前后的可打印性、力学性能及表面性能。结果表明0.7µm配方初始弯曲强度和弹性模量更高、表面粗糙度更低,但热循环后力学差异消失,且打印时间显著延长。
要点
- 0.7µm配方初始弯曲强度和弹性模量显著高于1.5µm配方,但热循环后差异消失。
- 0.7µm配方表面粗糙度更低,但打印时间显著延长(122.37 vs 48.23 min)。
- 两种配方在维氏显微硬度和剪切粘接强度上无显著差异。
核心结论
- 减小高填充3D打印树脂的填料粒径可改善初始力学性能和降低表面粗糙度,但热循环后力学优势未维持,且打印时间显著延长。
研究设计与样本
- 实验性体外研究,配制两种含硅烷化钡玻璃的高填充树脂:微米级(1.5µm)和亚微米级(0.7µm)。
- 采用数字光处理3D打印制备试样,在热循环(5000次,5°C-55°C)前后进行弯曲强度、弹性模量、维氏显微硬度、表面粗糙度、接触角和剪切粘接强度分析。
- 同时评估打印时间,数据采用独立t检验、双因素方差分析和Tukey检验(α=.05)。
主要发现
- 0.7µm配方实际制造时间显著长于1.5µm配方(122.37 ± 12.10 对 48.23 ± 2.96 min;p<.001)。
- 热循环前,0.7µm配方弯曲强度显著更高(p=.012),弹性模量显著更高(p<.001),但老化后差异未维持。
- 热循环显著降低两种配方的弯曲强度(p<.001)。
- 0.7µm配方表面粗糙度更低、接触角更高,而维氏显微硬度和剪切粘接强度无显著差异。
- 任何评估性能均未检测到配方与老化的显著交互作用。
临床怎么用
- 临床选择高填充3D打印树脂时需权衡:减小填料粒径可改善初始力学性能和表面粗糙度,但可能显著增加打印时间且老化后力学优势消失。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
PURPOSE: The purpose of this study was to evaluate the effect of filler particle size on the printability, mechanical behavior, and surface properties of highly filled experimental 3D-printed dental resins before and after thermocycling. MATERIAL AND METHODS: Two highly filled experimental resins containing silanized barium glass with different particle sizes were formulated: microparticulated (1.5 µm) and submicroparticulated (0.7 µm). Specimens were additively manufactured by digital light processing and subjected to flexural strength (FS), elastic modulus (EM), Vickers microhardness (VHN), surface roughness (Ra), contact angle (θ), and shear bond strength (SBS) analyses before and after thermocycling (5000 cycles; 5°C-55°C). Printing time was also evaluated. Data were analyzed by independent t-test, 2-way ANOVA and Tukey tests (α=.05). RESULTS: The 0.7-µm formulation required significantly longer actual fabrication time than the 1.5-µm formulation (122.37 ± 12.10 versus 48.23 ± 2.96 min; p<.001). Before thermocycling, the 0.7-µm formulation showed significantly higher FS (p=.012) and EM (p<.001) but these differences were not maintained after aging. Thermocycling significantly reduced FS in both formulations (p<.001). The 0.7-µm formulation exhibited lower Ra and higher contact angle values than the 1.5-µm formulation, whereas no significant differences were observed for VHN or SBS. No significant formulation × aging interactions were detected for any evaluated property. CONCLUSIONS: The 0.7-µm formulation showed higher initial flexural strength and elastic modulus and lower surface roughness. However, the mechanical differences were not maintained after thermocycling and no advantages were observed for microhardness or shear bond strength. These changes were accompanied by substantially longer fabrication time. CLINICAL SIGNIFICANCE: Reducing filler particle size in highly filled 3D-printed resins may improve initial mechanical behavior and reduce surface roughness but these mechanical advantages were not maintained after thermocycling and were accompanied by substantially longer fabrication time.
引用
- Dascanio R, Özcan M. Effect of filler particle size on the printability, physicomechanical and adhesion properties of highly filled experimental 3D-printed dental resins. J Dent. 2026. PMID: 42918481. doi:10.1016/j.jdent.2026.107130
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。