新型相稳定环氧树脂封闭剂与六种根管封闭剂对牙胶粘接强度的比较

Bond Strength to Gutta-Percha of a Novel Phase-Stable Epoxy Resin Sealer Compared With Six Endodontic Sealers.
PubMed 文献 · Int Endod J · 2026-10-06

本研究采用微剪切粘接强度测试,比较新型环氧树脂封闭剂AH Plus Ribbon与另外六种不同化学类别根管封闭剂对牙胶的粘接强度。结果显示封闭剂类型显著影响粘接强度(p < 0.001),AH Plus Ribbon与AH Plus粘接强度最高且无显著差异(p = 0.722),而EndoSequence BC Sealer、NeoSealer Flo和Sealapex最低。结论认为在实验条件下AH Plus Ribbon对牙胶的粘接强度与AH Plus相当,且显著高于其他五种封闭剂。

要点

  • AH Plus Ribbon对牙胶的粘接强度与AH Plus相当(p = 0.722)。
  • AH Plus Ribbon粘接强度显著高于其他五种封闭剂。
  • 封闭剂类型显著影响对牙胶的粘接强度(p < 0.001)。

核心结论

  • 在实验条件下,AH Plus Ribbon对牙胶的粘接强度与AH Plus相当,且显著高于EndoSequence BC Sealer、NeoSealer Flo、Pulp Canal Sealer、Endomethasone N和Sealapex。

主要发现

  • 封闭剂类型显著影响对牙胶的粘接强度(p < 0.001)。
  • AH Plus Ribbon与AH Plus粘接强度最高,二者无显著差异(p = 0.722)。
  • Pulp Canal Sealer和Endomethasone N呈中等粘接强度。
  • EndoSequence BC Sealer、NeoSealer Flo和Sealapex粘接强度最低,三者间无显著差异(p > 0.05)。

关键数值与推荐

  • 粘接强度以微剪切粘接强度(MPa)表示,采用万能试验机以0.5 mm/min十字头速度测定。
  • 封闭剂标准体积0.1 mL置于两个牙胶圆片间,恒定载荷0.0981 N持续200 s。
  • 标本在37°C下与磷酸盐缓冲盐水润湿纱布接触储存7天。
  • 统计分析采用单因素方差分析和Tukey's HSD事后检验(α = 0.05)。

临床怎么用

  • 对于需要与牙胶形成较高粘接强度的根管充填,AH Plus Ribbon可作为与AH Plus相当的选择。
  • 若临床关注封闭剂对牙胶的粘接性能,生物陶瓷类及氢氧化钙类封闭剂在本实验条件下表现较低。

局限性

  • 本研究为体外微剪切粘接强度测试,结果不能直接外推至临床性能。
  • 样本为标准化牙胶圆片,未涉及牙本质壁、根管解剖形态及体内环境的影响。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

AIM: To evaluate the bond strength of the reformulated epoxy resin-based sealer AH Plus Ribbon to gutta-percha using a previously described microshear bond strength test, and to compare its performance with that of six commercially available endodontic sealers representing different chemical classes. METHODOLOGY: One hundred and forty gutta-percha discs (10 mm × 2 mm) were fabricated from standardized sheets and randomly allocated to seven groups (n = 10 microshear specimens per group, assembled from 20 discs) according to the sealer evaluated: AH Plus Ribbon, AH Plus, EndoSequence BC Sealer, NeoSealer Flo, Pulp Canal Sealer, Endomethasone N and Sealapex. A standardized volume of sealer (0.1 mL) was placed between two gutta-percha discs under a constant load (0.0981 N) for 200 s. After storage at 37°C for 7 days in contact with phosphate-buffered saline-moistened gauze, microshear bond strength was determined using a universal testing machine at a crosshead speed of 0.5 mm/min. Bond strength values (MPa) were analysed by one-way ANOVA and Tukey's HSD post hoc test (α = 0.05). RESULTS: No premature failures occurred during specimen preparation, storage, or testing. Sealer type significantly influenced bond strength to gutta-percha (p < 0.001). AH Plus Ribbon and AH Plus exhibited the highest bond strengths and did not differ significantly from each other (p = 0.722). Pulp Canal Sealer and Endomethasone N showed intermediate bond strength, whereas EndoSequence BC Sealer, NeoSealer Flo and Sealapex exhibited the lowest values, with no significant differences among them (p > 0.05). CONCLUSIONS: AH Plus Ribbon exhibited bond strength to gutta-percha comparable to that of AH Plus and significantly higher than that of EndoSequence BC Sealer, NeoSealer Flo, Pulp Canal Sealer, Endomethasone N and Sealapex under the experimental conditions employed.

来源:Int Endod J,查看原文。版权归原作者所有。