3D打印树脂冠与预制氧化锆冠在乳磨牙的临床性能:分口对照研究
这项前瞻性分口临床研究纳入25名4-9岁儿童(50颗牙),比较3D打印树脂冠与预制氧化锆冠在乳磨牙的12个月临床性能。结果显示两组在固位、抗折和邻接方面成功率均高且无显著差异(p > 0.05),但树脂冠组牙龈指数和菌斑指数在所有时间点显著更高(p < 0.05),6和12个月咬合磨耗显著更大(p < 0.001)且逐渐变色(p < 0.001),而氧化锆冠保持颜色稳定且无咬合磨耗。结论认为树脂冠功能相当但牙周和美学结果较差。
要点
- 3D打印树脂冠与氧化锆冠在固位、抗折和邻接方面均高成功率且无显著差异(p > 0.05)。
- 树脂冠组牙龈指数和菌斑指数在所有时间点显著更高(p < 0.05)。
- 树脂冠在6和12个月咬合磨耗显著更大(p < 0.001)且逐渐变色(p < 0.001)。
核心结论
- 3D打印树脂冠功能性能与预制氧化锆冠相当,但牙周和美学结果较差。
研究设计与样本
- 前瞻性分口临床研究,纳入25名4-9岁儿童共50颗下颌乳磨牙,每名儿童一侧用预制氧化锆冠、对侧用3D打印树脂冠修复。
- 临床评估在3、6和12个月进行,包括固位、折裂、边缘完整性、牙龈指数、菌斑指数、邻接、咬合磨耗和颜色稳定性,数据分析用非参数检验(p < 0.05)。
主要发现
- 两组在固位、抗折和邻接方面均高成功率,随访期间无显著差异(p > 0.05)。
- 边缘完整性两组相当。
- 3D打印树脂冠组牙龈指数和菌斑指数在所有时间点显著更高(p < 0.05)。
- 3D打印树脂冠在6和12个月咬合磨耗显著更大(p < 0.001),并随时间逐渐变色(p < 0.001),而预制氧化锆冠保持颜色稳定且无咬合磨耗。
临床怎么用
- 3D打印树脂冠可作为成本有效的功能性替代,但需谨慎考虑菌斑控制、牙龈健康和长期美学稳定性。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVES: This study aimed to compare the 12-month clinical performance of prefabricated zirconia crowns and 3D-printed resin crowns in primary molars. The null hypothesis was that no difference would be observed between the two crown types. METHODS: This prospective split-mouth clinical study included 25 children (50 teeth) aged 4-9 years. In each participant, one mandibular primary molar was restored with a prefabricated zirconia crown and the contralateral molar with a 3D-printed resin crown. Clinical evaluations were performed at 3, 6, and 12 months, including crown retention, fracture, marginal integrity, gingival index, plaque index, proximal contact, occlusal wear, and color stability. Data were analyzed using non-parametric tests (p < 0.05). RESULTS: Both crown types demonstrated high success rates in terms of retention, fracture resistance, and proximal contact throughout follow-up, with no significant differences between groups (p > 0.05). Marginal integrity was comparable between groups. However, gingival and plaque index scores were significantly higher in the 3D-printed resin crown group at all time points (p < 0.05). Additionally, 3D-printed resin crowns showed significantly greater occlusal wear at 6 and 12 months (p < 0.001) and progressive discoloration over time (p < 0.001), whereas prefabricated zirconia crowns-maintained color stability and no occlusal wear. CONCLUSIONS: While 3D-printed resin crowns demonstrated comparable functional performance to prefabricated zirconia crowns, they were associated with inferior periodontal and esthetic outcomes. CLINICAL SIGNIFICANCE: 3D-printed resin crowns may represent a cost-effective functional alternative; however, their use requires careful consideration regarding plaque control, gingival health, and long-term esthetic stability.
引用
- Alper ES, Simsek H, Buyuk SK, et al. Clinical performance of 3D-printed resin versus prefabricated zirconia crowns in primary molars: A split-mouth clinical study. J Dent. 2026. PMID: 42142616. doi:10.1016/j.jdent.2026.106757
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。