文献速递牙体牙髓病

牛源羟基磷灰石与蒙脱石纳米复合材料的牙髓应用体外研究

Development of a Nano-Hybrid Composite Using Bovine Hydroxyapatite and Montmorillonite for Endodontic Applications-An In Vitro Study.
PubMed 文献 · Int Endod J · 2026-04-15

本研究开发了含牛源羟基磷灰石(BHA)和蒙脱石纳米黏土(MMT)的复合水门汀,以氧化锆为阻射剂、硅酸钙为凝固剂,并与ProRoot MTA对比理化、生物学及再矿化性能。结果显示复合材料pH>11、抗压强度21.2–23.8 MPa、凝固时间13–14 min,重金属与阻射性符合ISO标准,B20和B25细胞活性良好,M20再矿化增强。结论提示该材料具潜力,但需体内研究验证临床适用性。

要点

  • BHA-MMT复合材料理化性能符合ISO标准,凝固时间13–14 min。
  • B20和B25细胞活性良好,M20再矿化性能增强。
  • 临床用于活髓治疗或根尖充填前仍需体内研究验证。

核心结论

  • BHA-MMT复合材料展现出良好的理化、生物学和再矿化性能,符合ISO标准要求。
  • 该材料是有前景的生物活性复合体系,但需进一步体内研究确认临床适用性。

研究设计与样本

  • 体外研究,制备三种BHA与MMT比例不同的复合材料(B20、B25、M20),并与ProRoot MTA对比。
  • BHA由废弃牛骨经脱脂脱蛋白制得,MMT经球磨剥离为纳米黏土。

主要发现

  • 材料pH在24小时后升至11以上,并保持至21天。
  • B20、B25、M20的21天抗压强度分别为23.63、21.2、23.8 MPa。
  • 复合材料平均凝固时间为13–14分钟,重金属浓度在ISO标准允许限内。
  • 实验复合材料阻射性值在ISO推荐范围内。
  • B20和B25细胞活性良好,M20(更高MMT比例)显示增强的磷灰石形成和再矿化。

关键数值与推荐

  • BHA用量为20%和25% wt,氧化锆30% wt,剥离MMT为15%和20% wt。
  • 重金属浓度符合ISO标准允许限,阻射性符合ISO推荐范围。

临床怎么用

  • 该材料可能用于活髓治疗(直接/间接盖髓、活髓切断)和根尖充填,但需体内研究确认。

局限性

  • 仅为体外研究,需进一步体内研究确认临床适用性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

AIM: Hydraulic calcium silicate cements are widely employed in endodontics due to their excellent biocompatibility, bioactivity, sealing ability, and remineralisation potential. However, currently used products such as mineral trioxide aggregate (MTA) exhibit several limitations, including discolouration, cost, and poor handling properties. Therefore, this study aimed to develop and characterise a bovine-derived hydroxyapatite (BHA) and montmorillonite (MMT) nanoclay hybrid composite (BHA-MMT), incorporating zirconium oxide as a radiopacifier and calcium silicate phases as setting agents. METHODOLOGY: BHA was produced from waste bovine bones using a defatting and deproteination method. MMT clay was exfoliated into nanoclay using shear force with a planetary ball mill. The composite powders were prepared by combining BHA (20% and 25% wt), zirconium oxide (30% wt), setting agents with exfoliated MMT (15% and 20% wt) to produce three composite materials with different BHA and MMT ratios, namely B20, B25, and M20. The resulting powders were mixed with deionised water to form hydraulic cements. The composite materials were tested for chemical, mechanical, and physical properties compared with the commercially available ProRoot MTA. The biocompatibility, bioactivity, and remineralisation potential of the materials were also examined using established in vitro assays. RESULTS: The pH of the material increased above 11 after 24 h and remained constant up to 21 days. The compressive strengths of B20, B25, and M20 were 23.63, 21.2, and 23.8 MPa, respectively, after 21 days. The mean setting time of the composites ranged from 13 to 14 min, and the concentrations of heavy metals were within the permissible limits specified by ISO standards. The experimental composite materials demonstrated radiopacity values within the range, consistent with ISO recommendations. Among the variants, B20 and B25 demonstrated good cell viability, while M20, containing a higher proportion of MMT, showed enhanced apatite formation and remineralization, indicating improved bioactivity. CONCLUSION: The developed BHA-MMT composites demonstrated promising physicochemical, biological, and remineralisation properties consistent with ISO standard requirements. Overall, the product represents a bioactive composite material system; further investigations, including in vivo studies, are necessary to confirm its clinical applicability in vital pulp treatment (direct/indirect pulp capping, pulpotomy) and root-end filling procedures.

来源:Int Endod J,查看原文。版权归原作者所有。

引用

  1. Kumara PAASP, Cooper PR, Cathro P, et al. Development of a Nano-Hybrid Composite Using Bovine Hydroxyapatite and Montmorillonite for Endodontic Applications-An In Vitro Study. Int Endod J. 2026. PMID: 41982174. doi:10.1111/iej.70163

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。