文献速递口腔修复与种植

表面底涂对热固化、切削与3D打印义齿基托聚合物润湿性的影响:一项体外研究

Effect of surface priming on the wettability of heat-polymerized polymethylmethacrylate, milled and 3D printed denture base polymers: An in vitro study.
PubMed 文献 · J Dent · 2025-11-06

本研究用30个试件比较三种义齿基托聚合物(热固化、切削、3D打印)在涂布光固化甲基丙烯酸酯底涂后的表面接触角,分别以蒸馏水和1-溴萘测试。结果显示底涂增加对极性液体的疏水性,但改善对非极性液体的润湿性,且存在材料、底涂与测试液体三因素交互作用。

要点

  • 光固化甲基丙烯酸酯底涂可改变热固化、切削和3D打印义齿基托的润湿性。
  • 底涂后蒸馏水接触角升高,提示疏水性增加;1-溴萘接触角降低,润湿性改善。
  • 三因素交互作用显著(P<0.001),材料与底涂效果因测试液体而异。

核心结论

  • 光固化甲基丙烯酸酯底涂影响所评价义齿基托聚合物的润湿性。
  • 底涂增加对极性液体(蒸馏水)的疏水性,同时改善对非极性液体(1-溴萘)的润湿性。
  • 底涂可增强对非极性液体的润湿性,可能有利于使用具有非极性特性的修复材料。

研究设计与样本

  • 体外研究,共制作30个试件,3种义齿基托聚合物(Lucitone 199、IvoBase CAD、NextDent Denture 3D+)每组10个。
  • 试件一侧涂布光固化甲基丙烯酸酯底涂(VisioLink;Bredent),另一侧不处理。
  • 用蒸馏水和1-溴萘通过光学测角仪评估表面接触角,数据采用重复测量三因素方差分析和Step-down Bonferroni校正事后两两比较。

主要发现

  • 底涂、基托材料与测试液体三因素交互作用有统计学意义(P<0.001)。
  • 蒸馏水测试:底涂后热固化PMMA接触角73.6±0.9°、3D打印PMMA 76±0.7°、切削PMMA 64.6±0.5°;未底涂时分别为43.2±0.8°、53.6±0.9°、48.2±0.8°。
  • 1-溴萘测试:未底涂接触角热固化PMMA 16±0.7°、切削PMMA 14±1°、3D打印光聚合物12±1°;底涂后分别降至11.2±0.8°、7.8±0.8°、10.8±0.8°。
  • 事后分析显示未底涂时材料间差异有统计学意义(P<0.05),同一材料底涂前后差异有统计学意义(P<0.05)。
  • 底涂后3D打印光聚合物与热固化PMMA之间、以及两种PMMA材料在1-溴萘测试下差异有统计学意义(P<0.05);蒸馏水测试也观察到类似结果(P<0.05)。

临床怎么用

  • 临床使用非极性修复材料(如某些重衬或粘接材料)前,可考虑对义齿基托表面涂布光固化甲基丙烯酸酯底涂以改善润湿性。
  • 底涂会增加基托对极性液体(如水)的疏水性,需根据后续材料性质选择是否处理。
  • 不同基托材料(热固化、切削、3D打印)对底涂的润湿性反应存在差异,临床操作应结合材料类型评估。

局限性

  • 本研究为体外研究,结果不能直接推广到临床长期表现。
  • 仅评估了单一底涂产品(VisioLink)和两种测试液体,未涉及其他底涂或唾液等复杂口腔环境。
  • 样本量有限(每组10个试件),且未报告盲法或随机化等偏倚控制细节。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

OBJECTIVE: Computer-aided design and computer-aided manufacturing (CAD-CAM) complete dentures are commonly used with adhesives, relines, and repair materials to enhance comfort and function. However, to work satisfactorily, the reline material and the surface of the denture base must be compatible, or the latter should be treated to alter its surface properties to ensure a strong union. Research on the effect of surface priming on the wettability of heat-polymerized, milled, and 3D printed denture base polymers is limited. This systematic review aimed to analyse, summarise, and evaluate the available evidence on the integration of nanomaterials into COAs, with a focus on progress achieved, limitations regarding antibacterial effectiveness, and potential future directions in orthodontic therapy. METHODS: A total of 30 specimens were fabricated with 3 denture base polymers (Lucitone 199, IvoBase CAD, and NextDent Denture 3D+); 10 specimens for each group. One side of the specimens was primed with a light-polymerized methacrylate primer (VisioLink; Bredent), while the other side was left untreated. Subsequently, sterile water and 1-bromonaphthalene (1BrN) were used to evaluate the surface contact angle with an optical goniometer. The resulting data were analyzed using repeated measures 3-way ANOVA and post-hoc Step-down Bonferroni-corrected pairwise comparisons. RESULTS: The statistical analysis suggrsted a 3-way interaction between the effect of the primer, the denture base material, and the testing liquid on the wettability of the different groups (P < 0.001). The primed heat-polymerized PMMA (73.6 ± 0.9°), 3D printed PMMA (76 ± 0.7°), and milled PMMA denture bases (64.6 ± 0.5°) exhibited high contact angles with distilled water, suggesting poor wettability to this liquid. Without priming, the distilled water contact angle was lower for the 3D printed photopolymer (53.6 ± 0.9°), milled PMMA (48.2 ± 0.8°), and heat-polymerized PMMA (43.2 ± 0.8°) denture base groups. For 1BrN, the contact angles were considerably lower across all groups. Non-primed surfaces exhibited contact angle values ranging from 16 ± 0.7° for heat-polymerized PMMA,14± 1° for milled PMMA, and 12 ± 1° for the 3D printed photopolymer specimens. Surface priming reduced these values to 11.2 ± 0.8°, 7.8 ± 0.8°, and 10.8 ± 0.8 °, respectively. The post-hoc analysis revealed statistically significant differences between materials without surface priming (P < 0.05). Similarly, significant differences were noticed when the same materials were evaluated before and after surface treatment (P < 0.05). When different denture base materials treated with the same surface treatment were evaluated, significant differences were detected between the primed 3D printed photopolymer and heat-polymerized PMMA, and between both PMMA groups treated with 1BrN (P < 0.05). Similar results were observed when distilled water was used as testing liquid (P < 0.05). CONCLUSIONS: The light-polymerized methacrylate primer affected the wettability of the denture base polymers evaluated. The primer increased hydrophobicity toward polar liquids (distilled water), while improving wettability for the non-polar testing liquid (1-bromonaphthalene). Primer applications can enhance wettability to non-polar liquids, which can be beneficial when restorative materials with non-polar properties are to be used.

来源:J Dent,查看原文。版权归原作者所有。

引用

  1. Aldosari AM, Azpiazu-Flores FX, Azer S, et al. Effect of surface priming on the wettability of heat-polymerized polymethylmethacrylate, milled and 3D printed denture base polymers: An in vitro study. J Dent. 2025. PMID: 41205990. doi:10.1016/j.jdent.2025.106221

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。