PubMed 文献 · Int Endod J · 2025-05-23

本研究用差示扫描量热法(DSC)分析ProTaper Universal与ProTaper Gold F2镍钛器械的相变温度,并在20±1°C与35±1°C下测试循环疲劳强度。结果显示两种器械在20°C下断裂时间均显著长于35°C(p<0.05),ProTaper Gold在35°C下疲劳强度下降幅度更大(58%),但两个温度下均保持更优的循环疲劳强度(p<0.05)。

要点

  • ProTaper Gold的R相开始温度(Rs)为44.0°C、结束温度(Rf)为28.6°C,ProTaper Universal分别为16.2°C与-12.7°C。
  • 两种器械在20°C下的断裂时间均显著长于35°C(p<0.05)。
  • ProTaper Gold在35°C下疲劳强度降低58%,但两个温度下均优于ProTaper Universal(p<0.05)。

核心结论

  • 镍钛器械的循环疲劳强度取决于温度,凸显了在单一预设温度下评估性能的局限。
  • DSC可提供相变的关键信息,有助于在机械测试之外更好地解读力学性能。
  • 将冶金学表征与循环疲劳分析相结合可改进镍钛器械的评价。

研究设计与样本

  • 比较50支镍钛器械:ProTaper Universal F2(n=25)与ProTaper Gold F2(n=25)。
  • 比较几何设计(刃长、螺旋数、螺旋密度、螺旋几何、尖端设计与表面质量)及冶金学性能(能量色散X射线光谱元素分析与相变温度)。
  • 在20±1°C与35±1°C下用标准化人工根管进行循环疲劳强度测试,记录断裂时间(秒)。
  • 组间用独立样本Student t检验、组内用配对Student t检验(α=5%)。

主要发现

  • 两种器械均为17 mm刃长、10个螺旋(0.59螺旋/mm),几何形态相似,镍钛丝镍钛比接近等原子比,仅合金颜色不同。
  • DSC显示ProTaper Universal的R相开始温度(Rs)为16.2°C、结束温度(Rf)为-12.7°C;ProTaper Gold的Rs为44.0°C、Rf为28.6°C,两者相变均逐渐发生。
  • 两种器械在20°C下的断裂时间均显著长于35°C(p<0.05)。
  • ProTaper Gold在35°C下疲劳强度下降幅度更大(58%),但在两个温度下均保持更优的循环疲劳强度(p<0.05)。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

AIM: This study aims to demonstrate that phase transformation analysis, assessed via differential scanning calorimetry (DSC), offers a more comprehensive understanding of NiTi instruments' mechanical behaviour than traditional fixed-temperature fatigue testing by evaluating phase transformation temperatures and their impact on cyclic fatigue strength of ProTaper Universal and ProTaper Gold at 20 and 35°C. METHODOLOGY: Fifty ProTaper Universal F2 (n = 25) and ProTaper Gold F2 (n = 25) NiTi instruments were compared for geometric design (blade length, helical spirals, spiral density, spiral geometry, tip design and surface quality) and metallurgical properties including elemental analysis (energy-dispersive X-ray spectroscopy) and phase transformation temperatures. Then, cyclic fatigue strength was tested at room (20 ± 1°C) and body (35 ± 1°C) temperatures using a standardized artificial canal and cyclic fatigue resistance test. Time to fracture (in seconds) was recorded, and data were statistically analysed using the independent Student's t-test for intergroup analysis and the paired Student's t-test for intragroup analysis (α = 5%). RESULTS: Both instruments had a 17 mm blade with 10 spirals (0.59 spirals/mm), similar geometry and NiTi wires with near-equiatomic nickel-titanium ratios, differing only in metal alloy colour. DSC analysis showed distinct phase transformation temperatures, with ProTaper Universal exhibiting an R-phase start (Rs) at 16.2°C and finish (Rf) at -12.7°C, while ProTaper Gold had an Rs at 44.0°C and Rf at 28.6°C, though both transitions occurred gradually. Fracture time was significantly longer at 20°C than at 35°C for both instruments (p < 0.05), with ProTaper Gold showing a greater reduction (58%) but maintaining superior cyclic fatigue strength at both temperatures (p < 0.05). CONCLUSION: The cyclic fatigue strength of NiTi instruments depends on temperature, highlighting the limits of assessing performance at a single predefined temperature. DSC offers key insights into phase transformation, enabling a better interpretation of mechanical properties beyond mechanical testing alone. Integrating metallurgical characterization with cyclic fatigue analysis improves the evaluation of NiTi instruments, ensuring a more accurate understanding of their mechanical performance.

来源:Int Endod J,查看原文。版权归原作者所有。