文献速递牙体牙髓病

常规固化与快速固化生物陶瓷的钙离子动态比较:细胞毒性与磷灰石形成的影响

Comparative Analysis of Calcium Dynamics in Regular-Set versus Fast-Set Bioceramics: Impact on Cytotoxicity and Apatite Formation.
PubMed 文献 · J Endod · 2024-12-10

本研究比较了EndoSequence根修复材料常规固化型(ES)与快速固化型(ESF)的钙离子释放、pH变化、生物活性和细胞毒性。结果显示ESF在7天内释放更多Ca2+且pH更高,在PBS中钙磷比显著更高(2.95 vs 2.16),形成更成熟的羟基磷灰石晶体;两者对Huh-7细胞毒性均低。

要点

  • ESF在7天内钙离子释放显著高于ES,pH也更高。
  • ESF在PBS中钙磷比2.95,显著高于ES的2.16。
  • 两者细胞毒性均低,ESF生物活性动态更强。

核心结论

  • ES和ESF在模拟体液中均能形成磷灰石晶体,释放高钙离子并维持 prolonged 高pH,具有高生物活性潜力。
  • ESF钙离子释放更高,表明其动态生物活性更强,应与临床需求相匹配。

研究设计与样本

  • 实验研究,ES和ESF各10个样本(n=10),测试生物活性。
  • 对新鲜材料及在磷酸盐缓冲液(PBS)中浸泡30天的材料进行元素分析,并研究表面晶体形成。
  • 使用人肝癌细胞系(Huh-7)在不同材料浓度下评估细胞毒性。

主要发现

  • 两种材料主要元素包括Ca、P、Ta、Zr和Si,均含有限百分比的镱和钕。
  • 新鲜材料中,ES的Ca2+浓度更高且表面分布均匀;但ESF在7天内释放显著更多Ca2+(P < .05)且pH更高。
  • PBS浸泡后,ESF的钙磷比为2.95,显著高于ES的2.16(P < .05)。
  • ESF比ES具有更强的沉淀和生长羟基磷灰石(HA)的能力,表面形成更成熟的晶体。
  • ES和ESF对Huh-7细胞均显示低细胞毒性。

临床怎么用

  • ESF因钙离子释放更高和生物活性更强,可能更适用于需要动态生物活性的临床场景。
  • 两者细胞毒性均低,可根据临床需求选择合适固化类型。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

INTRODUCTION: The objective of this study was to assess the calcium ions (Ca2+) release, pH shift, bioactivity, and cytotoxicity of both forms of EndoSequence Root Repair Material: regular set (ES) and fast set (ESF). METHODS: ES (n = 10) and ESF (n = 10) forms were tested for their bioactivity. Elemental analysis was done on the fresh material and material immersed in phosphate-buffered saline (PBS) for 30 days. The surface crystal formation was studied. Cytotoxicity was evaluated at different material concentrations using a human hepatocellular cancer cell line (Huh-7). RESULTS: Both materials contain Ca, P, Ta, Zr, and Si as major elements. Both ES and ESF have a limited percentage of ytterbium and neodymium. In the fresh material, compared with the ESF, the ES had a higher Ca2+ concentration with a homogeneous surface distribution. However, the ESF released significantly more Ca2+ (P < .05) and had a higher pH over the 7-day course. When the material was immersed in PBS, the ESF exhibited a significantly higher Ca/P ratio of 2.95, while ES had 2.16 Ca/P ratio (P < .05). The ESF had a greater capacity to precipitate and grow hydroxyapatite (HA) than ES, resulting in more mature crystals forming on the surface. Both SE and ESF demonstrated low cytotoxicity against Huh-7 cells. CONCLUSIONS: When ES and ESF were submerged in simulated bodily fluid, both forms produced apatite crystals at the dentin material interface, releasing high Ca2+ and displaying a prolonged high pH with high bioactivity potential. Both forms had comparable low cytotoxicity. A higher Ca2+ release in ESF indicates dynamic bioactivity, which should be aligned with the clinical requirements.

来源:J Endod,查看原文。版权归原作者所有。

引用

  1. Khalil WA, Alharbi H. Comparative Analysis of Calcium Dynamics in Regular-Set versus Fast-Set Bioceramics: Impact on Cytotoxicity and Apatite Formation. J Endod. 2024. PMID: 39667664. doi:10.1016/j.joen.2024.12.002

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。