AH Plus Jet根管封闭剂混合方式对其理化机械性能的影响

Does the Mixing Method of AH Plus Jet Affect its Physicochemical and Mechanical Properties?
PubMed 文献 · J Endod · 2024-06-18

本研究评估AH Plus Jet封闭剂自动混合与手动混合是否影响其理化及机械性能。结果显示自动混合的固化时间更长、流动性更高,但推出粘结强度与手动混合相比较低,且孔隙率最高;溶解度与pH无组间差异。

要点

  • 自动混合AH Plus Jet固化时间显著长于手动混合。
  • 手动混合的推出粘结强度显著高于自动混合。
  • 自动混合孔隙率最高,SEM显示其表面孔隙更多。

核心结论

  • AH Plus Jet封闭剂的混合方式影响其部分理化与机械性能。

研究设计与样本

  • 体外研究,比较Auto Mix Tip自动混合与手动混合的AH Plus Jet封闭剂性能。
  • 样本量:阻射性n=5,初终凝时间n=5,流动性n=5,溶解度n=3,pH n=10,推出粘结强度n=30(牛牙),孔隙率n=5,SEM n=5。
  • 依据ISO 6876/2012与ADA Nº 57/2000规范评估;统计学采用单因素方差分析、Tukey检验、非配对t检验或Mann-Whitney检验,显著性水平5%。

主要发现

  • 阻射性:自动混合12.11 mmAl,手动混合12.55 mmAl(P > .05)。
  • 初凝时间:自动混合901分钟,手动混合631分钟;终凝时间:自动混合1779分钟,手动混合1504分钟(P < .05)。
  • 流动性:自动混合25.26 mm高于手动混合21.71 mm(P < .05)。
  • 推出粘结强度:手动混合14.52 MPa高于自动混合9.81 MPa(P < .05);两种方法均以混合破坏模式最常见。
  • 孔隙率自动混合最高(P < .05);SEM显示手动混合表面更光滑、孔隙更少、团聚体更小且分布更均匀。

关键数值与推荐

  • 溶解度与pH在两种混合方式间无统计学差异(P > .05)。

临床怎么用

  • 选择手动混合可能获得更高的推出粘结强度和更低的孔隙率。
  • 若需较长操作时间或较高流动性,可考虑自动混合,但需权衡粘结强度下降。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

INTRODUCTION: The purpose of this study was to evaluate whether the mixing method of AH Plus Jet sealer affects its physicochemical and mechanical properties. METHODS: The properties of AH Plus Jet sealer were analyzed when mixed using either the Auto Mix Tip or manual mixing. The evaluated properties included radiopacity (n = 5), initial and final setting times (n = 5), flow (n = 5), and solubility (n = 3), following specifications outlined in ISO 6876/2012 and ADA Nº 57/2000. pH levels were measured at intervals of 3, 24, 72, and 168 hours (n = 10). The push-out bond strength test was conducted using a universal testing machine and using bovine teeth (n = 30). Failure modes were analyzed with stereomicroscopy. Porosity was evaluated under micro-CT (n = 5), and scanning electron microscopy was also performed (n = 5). One-way analysis of variance and Tukey, unpaired t-tests, or Mann-Whitney tests were used with a significance level of 5%. RESULTS: The Auto Mix exhibited a radiopacity value of 12.11 mmAl, whereas manual mixing resulted in 12.55 mmAl (P > .05). For initial and final setting times, Auto Mix showed 901 minutes and 1779 minutes, respectively, while manual mixing recorded values of 631 minutes and 1504 minutes (P < .05). In terms of flow, Auto Mix demonstrated higher values (25.26 mm) than manual mixing (21.71 mm) (P < .05). No statistical differences were observed between the two methods for solubility and pH (P > .05). Manual mixing presented a higher bond strength value (14.52 MPa) than Auto Mix (9.81 MPa) (P < .05). The mixed failure mode was the most frequent outcome for both methods. The highest porosity was observed for Auto Mix (P < .05). Scanning electron microscopy analysis revealed that manual mixing resulted in a smoother surface with fewer pores and smaller, more evenly distributed agglomerates compared to automatic mixing. CONCLUSION: The mixing method employed for AH Plus Jet sealer influences some physicochemical and mechanical properties of the material.

来源:J Endod,查看原文。版权归原作者所有。

引用

  1. Rosa SJ, Duarte MAH, Silva EJNL, et al. Does the Mixing Method of AH Plus Jet Affect its Physicochemical and Mechanical Properties? J Endod. 2024. PMID: 38901643. doi:10.1016/j.joen.2024.06.006

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。