过氧化脲对压膜保持器生物力学性能的影响:分口随机对照试验
结果显示美白侧拉伸强度显著降低,硬度和内部粗糙度显著增加,牙齿颜色变化更大。结论提示以压膜保持器作为美白托盘虽能显著改变牙齿颜色,但会损害保持器的生物力学性能。
要点
- 10%过氧化脲美白两周可显著降低压膜保持器的拉伸强度。
- 美白侧保持器的硬度和内部粗糙度显著增加。
- 以压膜保持器作为美白托盘可能损害其机械性能。
核心结论
- 基于短期研究,使用压膜保持器作为美白托盘进行过氧化脲美白可实现明显的牙齿颜色改变,但会改变保持器的生物力学性能,包括拉伸强度降低、硬度和内部粗糙度增加。
主要发现
- 美白侧拉伸强度(均值±标准差:40.93±3.96 MPa)显著低于对照侧(47.40±5.03 MPa),差异6.47 MPa,95%CI 4.51-8.42,p<0.001。
- 美白侧硬度(VHN=14.63±2.29 N/mm²)显著大于对照侧(12.22±1.86 N/mm²),差异2.41 N/mm²,95%CI 1.56-3.25,p<0.001。
- 美白侧内部粗糙度(Ra=1.33±0.35 µm)显著大于对照侧(0.96±0.29 µm),差异0.37 µm,95%CI 0.23-0.51,p<0.001。
- 美白侧牙齿颜色变化(ΔE=6.00±3.32)大于对照侧(ΔE=2.50±1.70),差异3.50,95%CI 2.43-4.56,p<0.001。
临床怎么用
- 临床应用过氧化脲美白时,若使用压膜保持器作为美白托盘,需注意其机械性能可能下降,应评估保持器的更换时机。
局限性
- 本研究为短期研究,局限性未在原文中明确报告。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVE: To investigate the effect of tooth whitening on biomechanical properties of vacuum-formed retainers (VFRs). METHODS: Using a split-mouth, randomised controlled trial design, thirty participants were randomly allocated to receive whitening on either the upper or the lower arch, using 10 % carbamide peroxide for two weeks. Biomechanical properties such as hardness, tensile strength, and surface roughness were assessed two weeks after whitening was completed. RESULTS: Tensile strength of the whitening arch (mean ± SD: 40.93 ± 3.96 MPa) was significantly lower than that of the control (47.40 ± 5.03 MPa) (difference 6.47 MPa, 95 % CI 4.51 - 8.42, p < 0.001). Hardness and internal roughness of the whitening arch (VHN = 14.63 ± 2.29 N/mm2 and Ra = 1.33 ± 0.35 µm, respectively) were significantly greater than those of the control (12.22 ± 1.86 N/mm2 and 0.96 ± 0.29 µm, respectively) (differences 2.41 N/mm2, 95 % CI 1.56 - 3.25, p < 0.001 and 0.37 µm, 95 % CI 0.23 - 0.51, p < 0.001, respectively). The whitening arch showed greater tooth colour change (ΔE = 6.00 ± 3.32) than the control (ΔE = 2.50 ± 1.70) (difference = 3.50, 95 % CI 2.43 - 4.56, p < 0.001). CONCLUSIONS: Based on this short-term study, marked tooth colour change was achieved by whitening with VFRs as the whitening trays, but this changed the VFRs' biomechanical properties, including a decrease in tensile strength and an increase in hardness and internal roughness. CLINICAL SIGNIFICANCE: The application of carbamide peroxide in VFRs may compromise their mechanical properties.
引用
- Jin C, Gray AR, Brunton PA, et al. Effect of carbamide peroxide on biomechanical properties of vacuum-formed retainers: A split-mouth randomized controlled trial. J Dent. 2024. PMID: 38432352. doi:10.1016/j.jdent.2024.104902
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。