直型与角度螺丝通道钛基对两段式种植体失败载荷的影响
该体外研究将32颗前牙单颗螺丝固位氧化锆冠按种植体材料(钛锆或陶瓷)与钛基类型(直型SSC或25°角度型ASC)分为四组,每组8颗,经热力学疲劳加载后测定失败载荷与弯曲力矩。所有样本均通过疲劳测试且无并发症,ASC钛基与陶瓷种植体的弯曲力矩显著更高,陶瓷种植体失效表现为严重断裂而钛种植体仅为塑性变形。
要点
- ASC钛基显著提高失败载荷弯曲力矩(p=.001)。
- 陶瓷种植体弯曲力矩显著高于钛锆种植体(p<.001)。
- 所有样本经疲劳加载后存活且无并发症。
核心结论
- 从力学角度,ASC钛基可推荐用于陶瓷和钛种植体,临床应用安全。
- 陶瓷与钛种植体经疲劳加载后均表现出高可靠性,无失败发生。
研究设计与样本
- 体外研究,32颗前牙单颗螺丝固位氧化锆冠分为四组,每组8颗。
- 因素为种植体材料(两段式钛锆种植体为对照组,两段式陶瓷种植体为试验组)与钛基类型(SSC 0°与ASC 25°)。
- 统计方法为ANOVA与Mann-Whitney U检验。
主要发现
- 平均弯曲力矩(±SD):Ti-Zr-0为241±45 N cm,Ti-Zr-25为303±86 N cm,CI-0为326±58 N cm,CI-25为434±71 N cm。
- 钛基类型对结果有显著影响,支持ASC钛基(p=.001)。
- 种植体材料对结果有显著影响,支持陶瓷种植体(p<.001)。
- SLF后失效分析显示陶瓷种植体发生严重断裂,钛种植体仅限于塑性变形。
- 拉曼光谱显示存在残余压应力,FEG-SEM显示陶瓷种植体颈圈螺纹与抛光面之间表面粗糙。
关键数值与推荐
- ASC钛基角度为25°,SSC钛基角度为0°。
- 各组弯曲力矩均值与标准差见findings。
临床怎么用
- 对陶瓷与钛种植体的螺丝固位单颗氧化锆冠,可优先考虑ASC钛基以提升机械性能。
- 陶瓷种植体虽力学表现良好,但失效模式为严重断裂,临床需关注其断裂风险。
局限性
- 为体外研究,样本量每组8颗,结论需临床研究验证。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVE: To analyze the influence of titanium-base (straight [SSC]/angulated-screw-channel [ASC]) on failure-loads and bending-moments of two-piece ceramic and titanium-zirconium implants restored with monolithic-zirconia crowns after fatigue. MATERIALS AND METHODS: Thirty-two anterior monolithic-screw-retained zirconia crowns were divided into four groups (n = 8/group) according to the factors: (1) type of implant material: two-piece titanium-zirconium implant (Ti-Zr; control-group) versus two-piece ceramic implant (CI; test-group) and (2) type of titanium-base: SSC (0° angle) versus ASC (25°). An intact implant was used for field emission gun-scanning electronic microscopy (FEG-SEM) characterization and Raman spectroscopy for phase analyses and residual stress quantification. All samples were exposed to fatigue with thermodynamic loading (1.2-million-cycles, 49 N, 1.6 Hz, 5-55°C) at a 30° angle. Surviving specimens were loaded until failure (SLF) and bending moments were recorded. Failed samples were examined using light microscope and SEM. Statistical analyses included ANOVA and Mann-Whitney U-test. RESULTS: Raman-spectroscopy revealed the presence of residual compressive stresses. FEG-SEM revealed a roughened surface between threads and polished surface at the cervical-collar of the ceramic implant. All samples survived fatigue and were free of complications. Mean bending-moments (±SD) were: Ti-Zr-0: 241 ± 45 N cm, Ti-Zr-25: 303 ± 86 N cm, CI-0: 326 ± 58 N cm, CI-25: 434 ± 71 N cm. Titanium-base and implant-material had significant effects in favor of ASC titanium bases (p = .001) and ceramic-implants (p < .001). Failure analysis after SLF revealed severe fractures in ceramic implants, whereas titanium implants were restricted to plastic deformation. CONCLUSIONS: Ceramic and titanium implants exhibited high reliability after fatigue, with no failures. From a mechanical perspective, titanium bases with ASC can be recommended for both ceramic and titanium implants and are safe for clinical application.
引用
- Helal E, Gierthmuehlen PC, Bonfante EA, et al. Influence of straight versus angulated screw channel titanium bases on failure loads of two-piece ceramic and titanium implants restored with screw-retained monolithic crowns: An in-vitro study. Clin Oral Implants Res. 2023. PMID: 37565379. doi:10.1111/clr.14157
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。