本研究合成Ag@SiO2纳米颗粒并按其2.5 wt%、5 wt%、10 wt%比例掺入实验性双固化树脂根管封闭剂,评估其对理化与生物学性能的影响。结果显示10 wt%组在即刻与9个月水储存后均降低粪肠球菌生物膜活力,且未降低细胞活力,但放射阻射率低于ISO 6876要求,10 wt%组 subsurface 硬度损失更高。

要点

  • Ag@SiO2平均粒径683.51 nm±93.58,呈规则球形。
  • 10 wt%组在24小时与9个月均降低粪肠球菌生物膜活力。
  • 各封闭剂放射阻射率均低于ISO 6876要求值。

核心结论

  • 添加10 wt% Ag@SiO2在即刻与纵向分析中降低粪肠球菌活力,同时维持所开发封闭剂的理化性能。

研究设计与样本

  • 体外研究:采用溶胶-凝胶法基于Stöber法合成Ag@SiO2纳米颗粒并进行FTIR、XRD、TGA、UV-Vis、SEM与TEM表征。
  • 实验性双固化树脂根管封闭剂配方为70 wt% UDMA、15 wt% GDMA与15 wt% BisEMA,光引发剂分置于两组糊剂中。
  • Ag@SiO2以2.5 wt%、5 wt%、10 wt%掺入封闭剂,并设不含纳米颗粒的对照组。
  • 评估封闭剂的流动性、膜厚度、转化度、溶剂软化、放射阻射率、细胞毒性与抗菌活性,时间点为即刻与水中储存9个月后。

主要发现

  • Ag@SiO2化学表征检出银,颗粒呈规则球形,平均直径683.51 nm±93.58 nm。
  • 封闭剂具有足够的流动性与膜厚度,但放射阻射率值低于ISO 6876要求。
  • 所有组浸泡溶剂后均发生软化,10 wt%组显示更高的 subsurface 硬度损失(∆KHN%)。
  • 未观察到细胞活力降低。
  • 10 wt%组在24小时与9个月后均降低粪肠球菌生物膜活力。

关键数值与推荐

  • Ag@SiO2平均直径683.51 nm±93.58 nm。
  • 封闭剂配方:70 wt% UDMA、15 wt% GDMA、15 wt% BisEMA。
  • Ag@SiO2掺入浓度为2.5 wt%、5 wt%、10 wt%。
  • 放射阻射率低于ISO 6876要求值。
  • 10 wt%组在24小时与9个月降低粪肠球菌生物膜活力,且未降低细胞活力。

临床怎么用

  • 原文未据此给出临床推荐。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

AIM: To avoid root canal recontamination and endodontic treatment failure, endodontic sealers with antibacterial activity could be an alternative. Silver nanoparticles have antibacterial activity and this study aimed to synthesize Ag@SiO2 nanoparticles, incorporate them into an experimental endodontic resin sealer and evaluate their influence on physicochemical and biological properties. METHODOLOGY: Ag@SiO2 nanoparticles were produced using the sol-gel process, based on the Stöber method. The particles were characterized in terms of their chemical structure by Fourier transform-infrared spectroscopy (FTIR), X-ray diffraction (XRD), thermogravimetric analysis (TGA), UV-Vis spectral analysis, scanning electron microscopy, and transmission electron microscopy, where the particle morphology and diameter were analysed. A dual-cured experimental endodontic resin sealer was formulated using 70 wt% UDMA, 15 wt% GDMA, and 15 wt% BisEMA. The photoinitiators were added separately in two pastes. The Ag@SiO2 nanoparticles were incorporated into the endodontic sealer at the concentrations of 2.5 wt%, 5 wt%, and 10 wt%, and a control group without nanoparticles was also formulated. The endodontic sealers were evaluated for their flow, film thickness, degree of conversion, softening in solvent, radiopacity, cytotoxicity and antibacterial activity immediately and after 9 months in water storage. RESULTS: Silver was detected in the chemical characterization of Ag@SiO2 that presented a spheric regular shape and average 683.51 nm ± 93.58 diameter. Sealers presented adequate flow and film thickness while radiopacity values were below the ones required by ISO 6876. All groups underwent softening after immersion in a solvent. The 10 wt% groups showed a higher loss of subsurface hardness (∆KHN%). No reduction in cell viability was observed. Enterococcus faecalis viability in biofilm was reduced in 10 wt% groups after 24 h and 9 months. CONCLUSION: The addition of 10 wt% Ag@SiO2 reduced E. faecalis viability at immediate and longitudinal analysis while maintaining the physicochemical properties of developed sealers.

来源:Int Endod J,查看原文。版权归原作者所有。

引用

  1. Rücker VB, Balbinot GS, Collares FM, et al. Synthesis of silver core-shell nanoparticles and their influence on an experimental resin endodontic sealer: An in vitro analysis. Int Endod J. 2022. PMID: 36314859. doi:10.1111/iej.13859

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。