二硅酸锂种植冠对颌牙釉质24个月体内磨耗——一项先导研究
本先导研究通过口内扫描和计算机分析,评估二硅酸锂种植冠与对颌牙釉质以及相邻天然牙釉质之间的磨耗比值差异,并观察相邻牙齿的移动。结果显示,12个月和24个月时两组磨耗比值均无显著差异;作者认为该方法可测量牙齿磨耗并检测长期磨耗表现。
要点
- 12个月时,釉质对颌牙对之间的磨耗比为0.95±0.27 µm,二硅酸锂/釉质之间的磨耗比为0.73±0.49 µm。
- 24个月时,釉质对颌牙对的磨耗比为1.04±0.28 µm,二硅酸锂/釉质之间的磨耗比为0.73±0.51 µm。
- 两组磨耗比值均无显著差异,口内扫描和计算机分析可用于测量牙齿磨耗。
核心结论
- 口内扫描和计算机分析显示,两年内釉质/釉质与釉质/二硅酸锂种植冠之间的磨耗比值无显著差异。
研究设计与样本
- 先导研究,对41例患者植入种植修复体后(基线)、12个月和24个月时进行咬合面口内扫描。
- 12个月时可分析9例患者的11对种植冠/釉质对颌牙对及相邻釉质对颌牙对;24个月时因1例种植冠脱粘,可分析8例患者的10颗种植冠。
- 采用半自动迭代最近点算法将基线扫描与随访扫描表面叠加,测量每个识别磨耗面的最大高度损失,计算每单位的平均最大牙齿磨耗和标准差(SD)。
- 通过单独的测量程序,以种植体为参考结构配准扫描表面,用平移和旋转描述牙齿移动。
主要发现
- 12个月时,釉质对颌牙对之间的磨耗比为0.95±0.27 µm,二硅酸锂/釉质之间的磨耗比为0.73±0.49 µm。
- 24个月时,釉质对颌牙对的磨耗比为1.04±0.28 µm,二硅酸锂/釉质之间的磨耗比为0.73±0.51 µm。
- 两组磨耗比值均无显著差异。
临床怎么用
- 作者指出,本研究所述方法可测量牙齿磨耗并检测长期磨耗表现。
- 作者认为,未来应将修复体的数字监测整合到临床工作流程中,以识别影响修复体寿命的潜在因素。
局限性
- 原文未报告局限性。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVES: To evaluate whether there is a significant difference between the ratio of wear of lithium disilicate implant crowns and their enamel antagonists and adjacent enamel/enamel antagonist contacts. Additionally, the movement of the adjacent teeth was determined. MATERIALS AND METHODS: Intraoral scans of the occlusal surfaces of 41 patients were performed after insertion of the implant restoration (baseline), after 12 and 24 months. From the initial study cohort, eleven implant crown/enamel antagonist pairs with adjacent enamel antagonist pairs could be analyzed in nine patients after 12 months. After 24 months, ten implant crowns of eight patients were available due to one decementation of an implant crown. A semiautomatic specifically developed iterative closest point algorithm was used to superimpose the surfaces of the baseline scan with the follow-up scans to measure the maximum height loss of each identified wear side. The mean maximum tooth wear and the standard deviation (SD) were calculated per unit. The ratio of wear of enamel/enamel antagonist teeth and the wear ratio of adjacent lithium disilicate implant crowns and their enamel antagonist surfaces were evaluated. Tooth movements were described by translations and rotations using a separate measurement procedure. The surfaces of the scans were superimposed setting the implant as a reference structure for registration. RESULTS: After 12 months the wear ratio between the enamel antagonist pairs was 0.95 ± 0.27 µm and the ratio between lithium disilicate/enamel was 0.73 ± 0.49 µm. After 24 months the ratio of enamel antagonist pairs was 1.04 ± 0.28 µm and the ratio of lithium disilicate/enamel was 0.73 ± 0.51 µm. The ratios did not differ significantly. CONCLUSIONS: Intraoral scanning and computer analysis showed that the two-years wear ratios between enamel/enamel and enamel/lithium disilicate implant crowns did not differ significantly. STATEMENT OF CLINICAL RELEVANCE: The methodology described in this study could measure tooth wear and detect long-term wear performance. In the future, digital monitoring of prosthetic restorations should be integrated into clinical workflow to identify potential factors affecting longevity.
引用
- Stück AV, Raith S, Reich S, et al. Twenty-four months in vivo wear of enamel antagonists to lithium disilicate implant crowns - a pilot study. J Dent. 2022. PMID: 35810925. doi:10.1016/j.jdent.2022.104215
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。