CAD-CAM钴铬与氧化锆基台在锥形连接种植体上的微渗漏评估:一项体外比较研究
研究评估氧化锆和CAD-CAM或铸造钴铬种植体基台的边缘及细菌微渗漏,将64枚锥形连接种植体及基台分为四组,经咀嚼模拟和热循环老化后浸入含牙龈卟啉单胞菌的0.2%亚甲蓝溶液48小时,结果显示30枚(47%)出现微渗漏,基台材料和制作工艺影响微渗漏,尽管CAD-CAM基台结果较好,但所有测试组均存在微渗漏。
要点
- 30枚(47%)种植体-基台出现微渗漏,其中氧化锆1枚、钴铬铣削1枚、钴铬激光烧结14枚、铸造14枚。
- 钴铬铣削组菌落数最低(5.17E+02 CFUs/ml),其次为氧化锆组(7.70E+03 CFUs/ml)。
- 铸造组(9.39E+03 CFUs/ml)和激光烧结组(2.4E+05 CFUs/ml)细菌计数较高,铸造与激光烧结间差异有统计学意义(p < .05),利于钴铬铸造组。
核心结论
- 基台材料和制作工艺影响种植体-基台微渗漏,尽管CAD-CAM基台结果较好,但所有测试组均存在微渗漏。
研究设计与样本
- 体外研究,将64枚锥形连接种植体及其相应基台分为四组:钴铬(铣削、激光烧结、铸造)和氧化锆(铣削)。
- 所有标本经咀嚼模拟和热循环老化后,浸入含牙龈卟啉单胞菌的0.2%亚甲蓝溶液48小时。
主要发现
- 30枚(47%)种植体-基台出现微渗漏并进行PCR检测:氧化锆1枚、钴铬铣削1枚、钴铬激光烧结14枚、铸造14枚。
- 7枚标本(钴铬激光烧结1枚、铸造6枚)菌落数低于PCR检测限(< 100 CFUs)。
- 钴铬铣削组菌落数最低(5.17E+02 CFUs/ml),其次为氧化锆组(7.70E+03 CFUs/ml)。
- 钴铬铸造组(9.39E+03 CFUs/ml)和激光烧结组(2.4E+05 CFUs/ml)细菌计数较高。
- 钴铬铸造组与激光烧结组菌落数比较差异有统计学意义(p < .05),利于钴铬铸造组。
局限性
- 原文未报告局限性。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
OBJECTIVE: To assess the marginal and bacterial microleakage in zirconia and CAD-CAM or cast Co-Cr implant abutments. METHODS: Sixty-four conical connection implants with their respective abutments were divided into four groups (Co-Cr (milled, laser-sintered, and cast) and Zirconia (milled)). All specimens were subjected to a chewing simulation and thermocycling. After aging process, specimens were submerged in a 0.2% methylene blue solution with Porphyromonas gingivalis (P.g) for 48 h. The marginal microleakage was measured using a 40× optical microscopy at the internal part of the implant, and when positive microleakage was observed, a DNA isolation with a polymerase chain reaction (PCR) test was used. The microbiological assessment was based on colony forming units (CFUs). RESULTS: Thirty (47%) implant-abutments presented microleakage and the PCR was performed on those specimens (1 Zirconia, 1 Co-Cr milled, 14 Co-Cr laser-sintered and 14 cast). Seven specimens (1 Co-Cr laser-sintered and six cast) presented values below the PCR detection limit (< 100 CFUs). The lowest CFUs count occurred in the Co-Cr milled group (5.17E+02 CFUs/ml) followed by zirconia (7.70E+03 CFUs/ml). The Co-Cr cast (9.39E+03 CFUs/ml) and laser-sintered (2.4E+05 CFUs/ml) groups had higher bacterial count. The CFU count comparison performed between Co-Cr cast and laser-sintered resulted in a statistically significant differences in favor of Co-CrCL (p < .05). CONCLUSIONS: The abutment material and fabrication technique affected the implant-abutment microleakage. Although the CAD-CAM abutments presented favorable results, all tested groups presented microleakage.
引用
- Molinero-Mourelle P, Roccuzzo A, Yilmaz B, et al. Microleakage assessment of CAD-CAM Cobalt-Chrome and Zirconia abutments on a conical connection dental implant: A comparative in vitro study. Clin Oral Implants Res. 2022. PMID: 35818785. doi:10.1111/clr.13973