实验性硼硅酸盐生物活性玻璃:牙髓细胞细胞相容性与力学表征
本研究在体外评估两种新型相分离硼硅酸盐玻璃(PSBS8不含氧化铝、PSBS16含氧化铝)对原代人牙髓细胞的影响,并与传统氟铝硅酸盐玻璃离子水门汀FUJI IX比较生物活性与力学性能。结果显示两种硼硅酸盐玻璃在直接和间接接触实验中均提高细胞活力,不含氧化铝的PSBS8在细胞活力、铺展及无细胞生物活性方面优于传统玻璃离子水门汀和含氧化铝的PSBS16。
要点
- 两种硼硅酸盐玻璃在直接和间接接触实验中均提高牙髓细胞活力。
- 接触3天后PSBS8组细胞活力率为152%,PSBS16组为145%,传统玻璃离子颗粒组为117%。
- PSBS8制备的水门汀维氏硬度显著高于PSBS16制备者(46.6 vs 36.7 MPa,p=.001)。
核心结论
- 不含氧化铝的硼硅酸盐生物活性玻璃在增强牙髓细胞活力、铺展及无细胞生物活性方面优于传统玻璃离子水门汀和含氧化铝的实验性硼硅酸盐玻璃。
研究设计与样本
- 体外研究,评估两种新型相分离硼硅酸盐玻璃(PSBS8不含氧化铝、PSBS16含氧化铝)对培养的原代人牙髓细胞的细胞相容性,并与传统氟铝硅酸盐玻璃离子水门汀FUJI IX比较生物活性和力学性能。
主要发现
- 两种硼硅酸盐玻璃在所有时间点的直接和间接接触实验中均提高细胞活力率。
- 接触3天后,不含氧化铝的PSBS8细胞活力率为152%,含氧化铝的PSBS16为145%,传统玻璃离子颗粒为117%。
- 浸泡3周后EDX分析显示45S5K的初始Ca/P比为2.1,不含氧化铝的PSBS8为2.08。
- PSBS8制备的水门汀维氏硬度值显著高于PSBS16制备者(46.6 vs 36.7 MPa,p=.001)。
- 成熟24小时后,PSBS8(不含氧化铝)的挠曲强度为12.9 MPa,商业对照为16.4 MPa;成熟1天和7天后,PSBS8的强度高于PSBS16(p=.001)。
以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。
原文
AIM: To assess in vitro the effect of two novel phase separated borosilicate glasses (PSBS) in the system SiO2 -B2 O3 -K2 O-CaO-Al2 O3 on dental pulp cells; and to compare their bioactivity and mechanical properties to a conventional fluoroaluminosilicate glass ionomer cement namely FUJI IX. METHODOLOGY: The cytocompatibility assessment of the two novel borosilicate glasses, one without alumina (PSBS8) and one containing alumina (PSBS16), was performed on cultured primary human pulp cells. Alamar blue assay was used to assess cell metabolic activity and cell morphology was evaluated by confocal imaging. The bioactivity in Stimulated Body Fluid was also evaluated after 1 and 3 weeks of immersion using SEM-EDX analysis. Vickers microhardness and flexural strength were assessed after incorporating the glass particles into a commercial glass ionomer cement (GIC) liquid containing both polyacrylic and polybasic carboxylic acid. RESULTS: The data revealed that the two borosilicate glasses enhanced cell viability ratios at all-time points in both direct and indirect contact assays. After 3 days of contact, PSBS8 without alumina showed higher viability rate (152%) compared to the PSBS16 containing alumina (145%) and the conventional glass ionomer particles (117%). EDX analysis confirmed an initial Ca/P ratio of 2.1 for 45S5K and 2.08 for PSBS8 without alumina after 3 weeks of immersion. The cement prepared using PSBS8 showed significantly higher Vickers hardness values (p = .001) than that prepared using PSBS16 (46.6 vs. 36.7 MPa). After 24 h of maturation, PSBS8 (without alumina) exhibited a flexural strength of 12.9 MPa compared to a value of 16.4 MPa for the commercial control. PSBS8 without alumina had a higher strength than PSBS16 with alumina, after 1 and 7 days of maturation (p = .001). CONCLUSIONS: The present in vitro results demonstrated that the borosilicate bioactive glass without alumina enhanced pulp cell viability, spreading and acellular bioactivity better than the conventional GIC and the experimental borosilicate glass containing alumina.
引用
- Lizzi F, Attik N, Goutaudier C, et al. Experimental borosilicate bioactive glasses: Pulp cells cytocompatibility and mechanical characterization. Int Endod J. 2022. PMID: 35862467. doi:10.1111/iej.13803
供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。