文献速递牙体牙髓病

羟基磷灰石基脱敏剂对通用型粘接剂粘接性能的影响

[Effect of hydroxyapatite based agents on the bonding properties of universal adhesives].
PubMed 文献 · Zhonghua Kou Qiang Yi Xue Za Zhi · 2022-01-01

研究选取60颗因阻生拔除的第三磨牙,建立牙本质敏感模型后分别用含羟基磷灰石脱敏牙膏Biorepair、Dontodent Sensitive及羟基磷灰石糊剂处理,再以酸蚀-冲洗或自酸蚀模式应用中强酸型通用型粘接剂G-Premio Bond。结果显示酸蚀-冲洗模式下各脱敏组粘接强度均显著高于对照组,自酸蚀模式下四组无显著差异;含羟基磷灰石脱敏剂对粘接性能无不利影响,搭配自酸蚀模式可获得良好粘接效果。

要点

  • 脱敏牙膏和糊剂可部分或完全封闭多数牙本质小管。
  • 酸蚀-冲洗模式下,脱敏牙膏A、B组和糊剂组粘接强度均显著大于对照组。
  • 自酸蚀模式四组粘接强度无显著差异,且各组自酸蚀均显著大于同组酸蚀-冲洗。

核心结论

  • 含羟基磷灰石的脱敏剂对中强酸型通用型粘接剂粘接性能无不利影响,搭配自酸蚀粘接模式可获得良好粘接效果。

研究设计与样本

  • 选取因阻生而拔除的第三磨牙60颗,由西安交通大学口腔医院口腔颌面外科提供。
  • 4颗牙制备1 mm厚牙本质片,1%柠檬酸处理建立牙本质敏感模型,分对照组、脱敏牙膏A组、脱敏牙膏B组和脱敏糊剂组(每组2片)。
  • 剩余牙暴露冠中部牙本质建立敏感模型后分入上述4组,每组再分酸蚀-冲洗和自酸蚀2个亚组,应用中强酸型通用型粘接剂G-Premio Bond粘接。
  • 制备树脂-牙本质片状试件(每亚组4个)、微拉伸试件(每亚组20个)和片状试件(每亚组6个),行扫描电镜、微拉伸强度测试和激光扫描共聚焦显微镜观察。

主要发现

  • 扫描电镜显示脱敏牙膏和脱敏糊剂处理均可部分或完全封闭多数牙本质小管。
  • 酸蚀-冲洗模式下,脱敏牙膏A组粘接强度(40.98±4.60)MPa、脱敏牙膏B组(40.89±4.64)MPa、脱敏糊剂组(41.48±3.65)MPa均显著大于对照组(38.58±4.28)MPa(F=3.89,P<0.05)。
  • 自酸蚀模式下4组粘接强度差异无统计学意义(F=0.48,P>0.05)。
  • 各组自酸蚀粘接模式粘接强度均显著大于同组酸蚀-冲洗粘接模式(P<0.05)。
  • 4组总体断裂模式主要为混合破坏和界面破坏;酸蚀-冲洗模式粘接界面银染颗粒沿混合层底部呈斑点状分布,自酸蚀模式几乎不存在银染颗粒沉积;激光扫描共聚焦显微镜显示酸蚀-冲洗模式混合层内存在连续线状渗透,自酸蚀模式呈不连续线状渗透。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

Objective: To study the effect of hydroxyapatite (HA) based agents on the bonding properties of universal adhesive with different application modes, and to provide evidence for the use of adhesives after desensitization treatment. Methods: Sixty impacted third molars were extracted and selected (acquired from Department of Oral and Maxillofacial Surgery, College of Stomatology, Xi'an Jiaotong University). Four third molars were used to prepare 1 mm thick dentin disks and treated with 1% citric acid to simulate sensitive tooth models. The dentin surfaces were observed by scanning electron microscope (SEM) after treating with no desensitization (control group), desensitized by HA based toothpaste Biorepair and Dontodent Sensitive respectively (desensitizing toothpaste A group and B group), or HA paste treatment (desensitizing paste group ) (n=2 per group). The remaining teeth were selected to expose the mid-coronal dentin and establish dentin sensitivity models. Then, the specimens were divided into 4 former groups and received corresponding treatment. Each group was randomly divided into 2 subgroups, and intermediately strong universal adhesive (G-Premio Bond) was applied on the desensitized dentin by either etch-and-rinse mode or self-etch mode. Resin-dentin slice specimens (n=4 per subgroup), microtensile specimens (n=20 per subgroup) and slice specimens (n=6 per subgroup) were prepared. The microstructure and nanoleakage of the adhesive interfaces were observed by scanning electron microscopy (SEM). The microtensile strength (bond strength) and fracture mode were tested and recorded. The water permeability of the adhesive interface was observed by laser scanning confocal microscopy (LSCM). Results: SEM showed that desensitizing toothpaste and desensitizing paste could partially or entirely occlude most of the dentin tubules. For the etch-and-rinse mode, the bond strength of specimens treated with toothpaste A [(40.98±4.60) MPa], toothpaste B [(40.89±4.64) MPa] and HA paste [(41.48±3.65) MPa] was significantly higher than that of the control group [(38.58±4.28) MPa] (F=3.89,P<0.05). There was no statistically significant difference in bond strength among the 4 subgroups for self-etch modes (F=0.48,P>0.05). After desensitization, the bond strength of the control group and desensitizing groups in the self-etch mode was significantly higher than that in the etch-and-rinse mode (P<0.05). The overall fracture modes were mixed failure and interfacial failure in the control group and desensitizing groups. SEM showed speckled silver-stained particles deposited along the bottom of the hybrid layer on the bond interface of etch-and-rinse mode, and there were few silver-stained particles deposited on the bond interface of self-etch mode. LSCM showed continuous linear penetration in the hybrid layer of etch-and-rinse mode subgroups and discontinuous linear penetration in the hybrid layer of self-etch mode subgroups. Conclusions: HA based desensitizers have no adverse effect on the bond strength of intermediately strong universal adhesive and show good bonding performance accompanied with the self-etch mode. 目的: 探讨含羟基磷灰石(hydroxyapatite,HA)的脱敏剂对不同粘接模式下通用型粘接剂粘接性能的影响,为脱敏处理后粘接剂的使用提供依据。 方法: 选取因阻生而拔除的第三磨牙60颗(西安交通大学口腔医院口腔颌面外科提供)。将4颗牙制备为1 mm厚牙本质片,1%柠檬酸处理建立牙本质敏感模型,分为对照组(无任何处理)、脱敏牙膏A和B组(分别用含HA的脱敏牙膏Biorepair和Dontodent Sensitive处理)、脱敏糊剂组(HA糊剂处理)(每组2片),扫描电镜观察各组牙本质表面形貌。剩余牙暴露冠中部牙本质并建立牙本质敏感模型,分入上述4组进行相应处理。每组再分为2个亚组,使用中强酸型通用型粘接剂(G-Premio Bond)分别在酸蚀-冲洗模式或自酸蚀模式下进行粘接,堆塑树脂,制备树脂-牙本质片状试件(每亚组4个)、微拉伸试件(每亚组20个)和片状试件(每亚组6个),分别进行粘接界面微观结构和纳米渗漏情况扫描电镜观察、微拉伸强度(粘接强度)测试及断裂模式记录、粘接界面水渗透情况激光扫描共聚焦显微镜观察。 结果: 扫描电镜显示,脱敏牙膏和脱敏糊剂处理均可部分或完全封闭多数牙本质小管。对于酸蚀-冲洗模式,脱敏牙膏A、B组和脱敏糊剂组粘接强度[分别为(40.98±4.60)、(40.89±4.64)和(41.48±3.65)MPa]均显著大于对照组[(38.58±4.28)MPa](F=3.89,P<0.05);对于自酸蚀模式,4组粘接强度差异均无统计学意义(F=0.48,P>0.05);各组自酸蚀粘接模式粘接强度均显著大于同组酸蚀-冲洗粘接模式(P<0.05)。4组总体断裂模式主要为混合破坏和界面破坏。扫描电镜观察显示,酸蚀-冲洗模式下粘接界面银染颗粒沿混合层底部呈斑点状分布,自酸蚀模式几乎不存在银染颗粒沉积。激光扫描共聚焦显微镜显示酸蚀-冲洗模式混合层内存在连续线状渗透,自酸蚀模式混合层内呈不连续线状渗透。 结论: 含HA的脱敏剂处理对中强酸型通用型粘接剂的粘接性能无不利影响,搭配自酸蚀粘接模式可获得良好的粘接效果。.

来源:Zhonghua Kou Qiang Yi Xue Za Zhi,查看原文。版权归原作者所有。

引用

  1. Meng YC, Huang F, Wang SL, et al. [Effect of hydroxyapatite based agents on the bonding properties of universal adhesives]. Zhonghua Kou Qiang Yi Xue Za Zhi. 2022. PMID: 35152654. doi:10.3760/cma.j.cn112144-20210516-00250

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。