文献速递牙体牙髓病口腔修复与种植

短期降解的树脂基牙科材料中双酚A的释放

Bisphenol A release from short-term degraded resin-based dental materials.
PubMed 文献 · J Dent · 2021-11-17

本研究量化了八种未聚合树脂基材料中的双酚A(BPA)杂质,并评估聚合后样本在唾液、变形链球菌、酸性和碱性介质中的短期降解释放。结果显示仅复合树脂含可定量BPA(301±32至1534±62 pg/mg),唾液和细菌降解下释放量过低无法准确定量,碱性介质中两种复合树脂释放显著减少而一种粘接剂显著增加。结论认为未聚合材料中已存在的BPA可解释聚合后的释放,短期降解未明确增加BPA释放。

要点

  • 仅复合树脂含可定量BPA杂质(301±32至1534±62 pg/mg),其他材料未检出。
  • 唾液和变形链球菌降解下BPA释放量过低,无法准确定量。
  • 碱性介质中两种复合树脂BPA释放显著减少,一种粘接剂显著增加。

核心结论

  • 未聚合树脂基材料中已存在的BPA可解释聚合后的BPA释放。
  • 无明确迹象表明短期材料降解导致BPA释放增加。

研究设计与样本

  • 体外研究:测定八种未聚合树脂基材料(四种复合树脂、一种窝沟封闭剂、两种粘接剂、一种根管封闭剂)中BPA含量。
  • 聚合样本(n=5)分别浸入1 mL成人混合全唾液、变形链球菌(2×10^7 CFU/mL)、0.1 M HCl、0.1 M NaOH及对照介质中。
  • 采用UPLC-MS/MS法(吡啶-3-磺酰氯衍生化)定量BPA。

主要发现

  • 仅复合树脂含高于定量限的痕量BPA(301±32至1534±62 pg/mg),可能为单体合成杂质。
  • 唾液和细菌降解下BPA释放量过低,无法准确定量;水中所有材料均可定量释放BPA。
  • 碱性介质中两种复合树脂BPA释放较水显著减少,一种粘接剂较水显著增加。

临床怎么用

  • 原文未据此给出推荐。

局限性

  • 原文未报告局限性。

以上解读依据论文摘要(全文未开放获取或许可不允许翻译转载)。

原文

OBJECTIVES: There is still much debate about the release of bisphenol A (BPA) from resin-based dental materials. Therefore, this study aimed to quantify BPA present as an impurity and to evaluate whether their degradation by salivary, bacterial, and chemical challenges could increase its release. METHODS: BPA was determined in three different amounts (300, 400, and 500 µg) of eight unpolymerized resin-based materials (four composites, one fissure sealant, two adhesives and one root canal sealer). Next, polymerized samples (n = 5) of each material were immersed in 1 mL of whole human pooled saliva collected from adults, Streptococcus mutans (2 × 107 CFU/mL), and acidic (0.1 M HCl), alkaline (0.1 M NaOH), and control media, respectively. The amount of BPA was quantified using an UPLC-MS/MS method including derivatization of BPA by pyridine-3-sulfonyl chloride. RESULTS: Only the composites contained trace amounts of BPA above the limit of quantification (ranging from 301±32 pg PBA/mg to 1534±62 pg BPA/mg), most likely as impurity from the synthesis of the monomers. The amounts of BPA released from polymerized materials upon salivary and bacterial degradation were too low for accurate quantification, but in water, quantifiable amounts of BPA were released from all materials. In alkaline media, the BPA release from two composites was significantly decreased, while the release from one adhesive was significantly increased, compared to water. CONCLUSIONS: BPA already present in unpolymerized resin-based materials may account for the release of BPA after polymerization. There was no clear indication that short-term material degradation leads to increased release of BPA.

来源:J Dent,查看原文。版权归原作者所有。

引用

  1. De Nys S, Duca RC, Vervliet P, et al. Bisphenol A release from short-term degraded resin-based dental materials. J Dent. 2021. PMID: 34798152. doi:10.1016/j.jdent.2021.103894

供执业医师工作参考,不替代临床判断;数值与分级以指南原文为准。